| 耐热铝合金:组织设计与合金制备 |
孙军( ), 刘刚, 杨冲, 张鹏, 薛航 |
| 西安交通大学 金属材料强度全国重点实验室 西安 710049 |
|
| Heat-Resistant Al Alloys: Microstructural Design and Preparation |
SUN Jun( ), LIU Gang, YANG Chong, ZHANG Peng, XUE Hang |
| State Key Laboratory for Mechanical Behavior of Materials, Xi'an Jiaotong University, Xi'an 710049, China |
引用本文:
孙军, 刘刚, 杨冲, 张鹏, 薛航. 耐热铝合金:组织设计与合金制备[J]. 金属学报, 2025, 61(4): 521-525.
Jun SUN,
Gang LIU,
Chong YANG,
Peng ZHANG,
Hang XUE.
Heat-Resistant Al Alloys: Microstructural Design and Preparation[J]. Acta Metall Sin, 2025, 61(4): 521-525.
| 1 |
Shyam A, Bahl S. Heat-resistant aluminium alloys [J]. Nat. Mater., 2023, 22: 425
|
| 2 |
Deschamps A, Hutchinson C R. Precipitation kinetics in metallic alloys: Experiments and modeling [J]. Acta Mater., 2021, 220: 117338
|
| 3 |
Polmear I J, Couper M J. Design and development of an experimental wrought aluminum alloy for use at elevated temperatures [J]. Metall. Trans., 1988, 19A: 1027
|
| 4 |
Yang C, Zhang P, Shao D, et al. The influence of Sc solute partitioning on the microalloying effect and mechanical properties of Al-Cu alloys with minor Sc addition [J]. Acta Mater., 2016, 119: 68
|
| 5 |
Xue H, Yang C, De Geuser F, et al. Highly stable coherent nanoprecipitates via diffusion-dominated solute uptake and interstitial ordering [J]. Nat. Mater., 2023, 22: 434
|
| 6 |
Rummel G, Zumkley T, Eggersmann M, et al. Diffusion of implanted 3D-transition elements in aluminum: 1. Temperature-dependence [J]. Z. Metallkd., 1995, 86:122
|
| 7 |
Du Y, Chang Y A, Huang B Y, et al. Diffusion coefficients of some solutes in fcc and liquid Al: Critical evaluation and correlation [J]. Mater. Sci. Eng., 2003, A363: 140
|
| 8 |
Calderon H A, Voorhees P W, Murray J L, et al. Ostwald ripening in concentrated alloys [J]. Acta Metall. Mater., 1994, 42: 991
|
| 9 |
Chen B A, Liu G, Wang R H, et al. Effect of interfacial solute segregation on ductile fracture of Al-Cu-Sc alloys [J]. Acta Mater., 2013, 61: 1676
|
| 10 |
Gao Y H, Guan P F, Su R, et al. Segregation-sandwiched stable interface suffocates nanoprecipitate coarsening to elevate creep resistance [J]. Mater. Res. Lett., 2020, 8: 446
|
| 11 |
Yi M, Zhang P, Yang C, et al. Improving creep resistance of Al-12 wt.% Ce alloy by microalloying with Sc [J]. Scr. Mater., 2021, 198: 113838
|
| 12 |
Yi M, Zhang P, Deng S H, et al. Atomic-scale compositional complexity ductilizes eutectic phase towards creep-resistant Al-Ce alloys with improved fracture toughness [J]. Acta Mater., 2024, 276: 120133
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|