| 低碳钢Q235、管线钢L415和压力容器钢16MnNi在湛江高湿高辐照海洋工业大气环境下的初期腐蚀行为 |
李小涵1,2, 曹公望2( ), 郭明晓1,2, 彭云超3, 马凯军3, 王振尧2( ) |
1中国科学技术大学 材料科学与工程学院 沈阳 110016 2中国科学院金属研究所 沈阳 110016 3国家管网集团东部原油储运有限公司 徐州 221008 |
|
| Initial Corrosion Behavior of Carbon Steel Q235, Pipeline Steel L415, and Pressure Vessel Steel 16MnNi Under High Humidity and High Irradiation Coastal-Industrial Atmosphere in Zhanjiang |
LI Xiaohan1,2, CAO Gongwang2( ), GUO Mingxiao1,2, PENG Yunchao3, MA Kaijun3, WANG Zhenyao2( ) |
1School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China 2Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 3PipeChina Network Corporation Eastern Oil Storage and Transportation Co., Ltd., Xuzhou 221008, China |
引用本文:
李小涵, 曹公望, 郭明晓, 彭云超, 马凯军, 王振尧. 低碳钢Q235、管线钢L415和压力容器钢16MnNi在湛江高湿高辐照海洋工业大气环境下的初期腐蚀行为[J]. 金属学报, 2023, 59(7): 884-892.
Xiaohan LI,
Gongwang CAO,
Mingxiao GUO,
Yunchao PENG,
Kaijun MA,
Zhenyao WANG.
Initial Corrosion Behavior of Carbon Steel Q235, Pipeline Steel L415, and Pressure Vessel Steel 16MnNi Under High Humidity and High Irradiation Coastal-Industrial Atmosphere in Zhanjiang[J]. Acta Metall Sin, 2023, 59(7): 884-892.
| 1 |
Han W, Yu G C, Wang Z Y, et al. Characterisation of initial atmospheric corrosion carbon steels by field exposure and laboratory simulation [J]. Corros. Sci., 2007, 49: 2920
doi: 10.1016/j.corsci.2007.01.009
|
| 2 |
Song Q Q, Wang X D, Pan B Y, et al. Effect of relative humidity on corrosion of Q235 carbon steel under thin electrolyte layer in simulated marine atmosphere [J]. Anti-Corros. Methods Mater., 2020, 67: 187
doi: 10.1108/ACMM-07-2019-2157
|
| 3 |
Zheng L Y, Cao F H, Liu W J, et al. Corrosion behavior of Q235 in simulated natural environment by electrochemical technology [J]. Equip. Environ. Eng., 2011, 8(4): 8
|
| 3 |
郑利云, 曹发和, 刘文娟 等. Q235钢在模拟自然环境下失效行为的电化学研究 [J]. 装备环境工程, 2011, 8(4): 8
|
| 4 |
Stratmann M, Bohnenkamp K, Engell H J. An electrochemical study of phase-transitions in rust layers [J]. Corros. Sci., 1983, 23: 969
doi: 10.1016/0010-938X(83)90024-0
|
| 5 |
Castaño J G, Botero C A, Restrepo A H, et al. Atmospheric corrosion of carbon steel in Colombia [J]. Corros. Sci., 2010, 52: 216
doi: 10.1016/j.corsci.2009.09.006
|
| 6 |
Cai Y K, Zhao Y, Ma X B, et al. Influence of environmental factors on atmospheric corrosion in dynamic environment [J]. Corros. Sci., 2018, 137: 163
doi: 10.1016/j.corsci.2018.03.042
|
| 7 |
He J X, Qin X Z, Yi P, et al. Corrosion exposure study on Q235 steel in marine atmospheric [J]. Surf. Technol., 2006, 35(4): 21
|
| 7 |
何建新, 秦晓洲, 易 平 等. Q235钢海洋大气腐蚀暴露试验研究 [J]. 表面技术, 2006, 35(4): 21
|
| 8 |
Song L Y, Chen Z Y. The role of UV illumination on the NaCl-induced atmospheric corrosion of Q235 carbon steel [J]. Corros. Sci., 2014, 86: 318
doi: 10.1016/j.corsci.2014.06.013
|
| 9 |
Mao X, Liu X, Revie R W. Pitting corrosion of pipeline steel in dilute bicarbonate solution with chloride ions [J]. Corrosion, 1994, 50: 651
doi: 10.5006/1.3293540
|
| 10 |
Chen H L, Wei Y. Mechanism of industrial atmospheric corrosion for carbon steel [J]. Corros. Prot., 2006, 27: 284
|
| 10 |
陈惠玲, 魏 雨. 碳钢在含SO2环境大气中腐蚀机理的研究 [J]. 腐蚀与防护, 2006, 27: 284
|
| 11 |
Lv W Y, Wang Z Y, Yu Q C, et al. Synergic effect of NaHSO3 and NaCl on atmospheric corrosion of Q235 steel [J]. Corros. Sci. Prot. Technol., 2015, 27: 545
|
| 11 |
吕旺燕, 王振尧, 于全成 等. NaHSO3和NaCl对Q235钢大气腐蚀的协同作用 [J]. 腐蚀科学与防护技术, 2015, 27: 545
|
| 12 |
Kamimura T, Hara S, Miyuki H, et al. Composition and protective ability of rust layer formed on weathering steel exposed to various environments [J]. Corros. Sci., 2006, 48: 2799
doi: 10.1016/j.corsci.2005.10.004
|
| 13 |
Palsson N S, Wongpinkaew K, Khamsuk P, et al. Outdoor atmospheric corrosion of carbon steel and weathering steel exposed to the tropical-coastal climate of Thailand [J]. Mater. Corros., 2020, 71: 1019
|
| 14 |
Han W, Pan C, Wang Z Y, et al. Initial atmospheric corrosion of carbon steel in industrial environment [J]. J. Mater. Eng. Perform., 2015, 24: 864
doi: 10.1007/s11665-014-1329-5
|
| 15 |
Ma Y T, Li Y, Wang F H. The effect of β-FeOOH on the corrosion behavior of low carbon steel exposed in tropic marine environment [J]. Mater. Chem. Phys., 2008, 112: 844
doi: 10.1016/j.matchemphys.2008.06.066
|
| 16 |
Ma Y T, Li Y, Wang F H. Corrosion of low carbon steel in atmospheric environments of different chloride content [J]. Corros. Sci., 2009, 51: 997
doi: 10.1016/j.corsci.2009.02.009
|
| 17 |
Yu Q C, Wang Z Y, Wang C. Corrosion behaviors of low alloy steel and carbon steel deposited with NaCl and NaHSO3 under dry/humid alternative condition [J]. Acta Metall. Sin., 2010, 46: 1133
doi: 10.3724/SP.J.1037.2010.00248
|
| 17 |
于全成, 王振尧, 汪 川. 表面沉积NaCl和NaHSO3的低合金钢和碳钢在干湿交替条件下的腐蚀行为 [J]. 金属学报, 2010, 46: 1133
doi: 10.3724/SP.J.1037.2010.00248
|
| 18 |
Hao L, Zhang S X, Dong J H, et al. Evolution of corrosion of MnCuP weathering steel submitted to wet/dry cyclic tests in a simulated coastal atmosphere [J]. Corros. Sci., 2012, 58: 175
doi: 10.1016/j.corsci.2012.01.017
|
| 19 |
Hao L, Zhang S X, Dong J H, et al. Evolution of atmospheric corrosion of MnCuP weathering steel in a simulated coastal-industrial atmosphere [J]. Corros. Sci., 2012, 59: 270
doi: 10.1016/j.corsci.2012.03.010
|
| 20 |
Xiao K, Dong C F, Li X G, et al. Effect of deposition of NaCl on the initial atmospheric corrosion of Q235 [J]. J. Chin. Soc. Corros. Prot., 2006, 26: 26
|
| 20 |
肖 葵, 董超芳, 李晓刚 等. NaCl颗粒沉积对Q235钢早期大气腐蚀的影响 [J]. 中国腐蚀与防护学报, 2006, 26: 26
|
| 21 |
Hao L, Zhang S X, Dong J H, et al. Rusting evolution of MnCuP weathering steel submitted to simulated industrial atmospheric corrosion [J]. Metall. Mater. Trans., 2012, 43A: 1724
|
| 22 |
Guo M X, Pan C, Wang Z Y, et al. A study on the initial corrosion behavior of carbon steel exposed to a simulated coastal-industrial atmosphere [J]. Acta Metall. Sin., 2018, 54: 65
doi: 10.11900/0412.1961.2017.00142
|
| 22 |
郭明晓, 潘 晨, 王振尧 等. 碳钢在模拟海洋工业大气环境中初期腐蚀行为研究 [J]. 金属学报, 2018, 54: 65
doi: 10.11900/0412.1961.2017.00142
|
| 23 |
Yamashita M, Konishi H, Kozakura T, et al. In situ observation of initial rust formation process on carbon steel under Na2SO4 and NaCl solution films with wet/dry cycles using synchrotron radiation X-rays [J]. Corros. Sci., 2005, 47: 2492
doi: 10.1016/j.corsci.2004.10.021
|
| 24 |
Ståhl K, Nielsen K, Jiang J Z, et al. On the akaganéite crystal structure, phase transformations and possible role in post-excavational corrosion of iron artifacts [J]. Corros. Sci., 2003, 45: 2563
doi: 10.1016/S0010-938X(03)00078-7
|
| 25 |
Asami K, Kikuchi M. In-depth distribution of rusts on a plain carbon steel and weathering steels exposed to coastal-industrial atmosphere for 17 years [J]. Corros. Sci., 2003, 45: 2671
doi: 10.1016/S0010-938X(03)00070-2
|
| 26 |
Asami K, Kikuchi M. Characterization of rust layers on weathering steels air-exposed for a long period [J]. Mater. Trans., 2002, 43: 2818
doi: 10.2320/matertrans.43.2818
|
| 27 |
Chen W J, Hao L, Dong J H, et al. Effect of sulphur dioxide on the corrosion of a low alloy steel in simulated coastal industrial atmosphere [J]. Corros. Sci., 2014, 83: 155
doi: 10.1016/j.corsci.2014.02.010
|
| 28 |
Antony H, Perrin S, Dillmann P, et al. Electrochemical study of indoor atmospheric corrosion layers formed on ancient iron artefacts [J]. Electrochim. Acta, 2007, 52: 7754
doi: 10.1016/j.electacta.2007.04.029
|
| 29 |
Alcántara J, Chico B, Díaz I, et al. Airborne chloride deposit and its effect on marine atmospheric corrosion of mild steel [J]. Corros. Sci., 2015, 97: 74
doi: 10.1016/j.corsci.2015.04.015
|
| 30 |
Wang Z G, Wang M, Jiang J, et al. Atmospheric corrosion analysis and rust evolution research of Q235 carbon steel at different exposure stages in Chengdu atmospheric environment of China [J]. Scanning, 2020, 2020: 9591516
|
| 31 |
Zhang X, Xiao K, Dong C F, et al. In situ Raman spectroscopy study of corrosion products on the surface of carbon steel in solution containing Cl- and S O 4 2 - [J]. Eng. Failure Anal., 2011, 18: 1981
doi: 10.1016/j.engfailanal.2011.03.007
|
| 32 |
Fajardo S, Llorente I, Jiménez J A, et al. Effect of Mn additions on the corrosion behaviour of TWIP Fe-Mn-Al-Si austenitic steel in chloride solution [J]. Corros. Sci., 2019, 154: 246
doi: 10.1016/j.corsci.2019.04.026
|
| 33 |
Li C L, Ma Y T, Li Y, et al. EIS monitoring study of atmospheric corrosion under variable relative humidity [J]. Corros. Sci., 2010, 52: 3677
doi: 10.1016/j.corsci.2010.07.018
|
| 34 |
Pan C, Guo M X, Han W, et al. Study of corrosion evolution of carbon steel exposed to an industrial atmosphere [J]. Corros. Eng. Sci. Technol., 2019, 54: 241
doi: 10.1080/1478422X.2019.1574955
|
| 35 |
Wang J H, Wei F I, Chang Y S, et al. The corrosion mechanisms of carbon steel and weathering steel in SO2 polluted atmospheres [J]. Mater. Chem. Phys., 1997, 47: 1
doi: 10.1016/S0254-0584(97)80019-3
|
| 36 |
Song L Y, Ma X M, Chen Z Y, et al. The role of UV illumination on the initial atmospheric corrosion of 09CuPCrNi weathering steel in the presence of NaCl particles [J]. Corros. Sci., 2014, 87: 427
doi: 10.1016/j.corsci.2014.07.013
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|