| 高温合金单晶铸件中共晶组织分布的表面效应 |
马德新1,2, 赵运兴1,2( ), 徐维台1, 皮立波1, 李重行1 |
1.深圳万泽中南研究院 深圳 518045 2.中南大学 粉末冶金研究院 长沙 410083 |
|
| Surface Effect on Eutectic Structure Distribution in Single Crystal Superalloy Castings |
MA Dexin1,2, ZHAO Yunxing1,2( ), XU Weitai1, PI Libo1, LI Zhongxing1 |
1.Wedge Central South Research Institute, Shenzhen 518045, China 2.Powder Metallurgy Research Institute, Central South University, Changsha 410083, China |
引用本文:
马德新, 赵运兴, 徐维台, 皮立波, 李重行. 高温合金单晶铸件中共晶组织分布的表面效应[J]. 金属学报, 2021, 57(12): 1539-1548.
Dexin MA,
Yunxing ZHAO,
Weitai XU,
Libo PI,
Zhongxing LI.
Surface Effect on Eutectic Structure Distribution in Single Crystal Superalloy Castings[J]. Acta Metall Sin, 2021, 57(12): 1539-1548.
| 1 |
Seo S M, Lee J H, Yoo Y S, et al. A comparative study of the γ/γ′ eutectic evolution during the solidification of Ni-base superalloys [J]. Metall. Mater. Trans., 2011, 42A: 3150
|
| 2 |
Brewster G, Dong H B, Green N R, et al. Surface Segregation during directional solidification of Ni-base superalloys [J]. Metall. Mater. Trans., 2008, 39B: 87
|
| 3 |
Cao L. Research on the formation of surface eutectic of Ni-base single crystal superalloys [D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2015
|
| 3 |
曹 亮. 镍基单晶高温合金中表面共晶形成行为研究 [D]. 沈阳: 中国科学院金属研究所, 2015
|
| 4 |
Cao L, Yao L, Zhou Y Z, et al. Formation of the surface eutectic of a Ni-based single crystal superalloy [J]. J. Mater. Sci. Technol., 2017, 33: 347
|
| 5 |
Cao L, Zhou Y Z, Jin T, et al. Effects of Re on surface eutectic formation for Ni-base single crystal superalloys during directional solidification [J]. J. Mater. Sci. Technol., 2017, 33: 1308
|
| 6 |
Sidhu R K, Ojo O A, Chaturvedi M C. Sub-solidus melting of directionally solidified Rene 80 superalloy during solution heat treatment [J]. J. Mater. Sci., 2008, 43: 3612
|
| 7 |
Hegde S R, Kearsey R M, Beddoes J C. Designing homogenization-solution heat treatments for single crystal superalloys [J]. Mater. Sci. Eng., 2010, A527: 5528
|
| 8 |
Chen R Z. A problem in manufacturing and using of cast turbine blades—Surface recrystallization [J]. Aviat. Eng. Maint., 1990, (4): 22
|
| 8 |
陈荣章. 铸造涡轮叶片制造和使用中的一个问题——表面再结晶 [J]. 航空制造工程, 1990, (4): 22
|
| 9 |
Xiong J C, Li J R, Liu S Z, et al. Microstructure of surface recrystallization of single crystal superalloy DD6 [J]. J. Mater. Eng., 2009, (): 110
|
| 9 |
熊继春, 李嘉荣, 刘世忠等. 单晶高温合金DD6表面再结晶组织 [J]. 材料工程, 2009, (): 110
|
| 10 |
Ma D X, Bührig-Polaczek A. Application of heat-conductor technique to production of single crystal turbine blade [J]. Metall. Mater. Trans., 2009, 40B: 738
|
| 11 |
Ma D X, Wu Q, Bührig-Polaczek A. Some new observations on freckle formation in directionally solidified superalloy components [J]. Metall. Mater. Trans., 2012, 43B: 344
|
| 12 |
Ma D X. Development of single crystal solidification technology for production of superalloy turbine blades [J]. Acta Metall. Sin., 2015, 51: 1179
|
| 12 |
马德新. 高温合金叶片单晶凝固技术的新发展 [J]. 金属学报, 2015, 51: 1179
|
| 13 |
Ma D X, Wang F X, Wu Q, et al. Innovations in casting techniques for single crystal turbine blades of superalloys [A]. Superalloys 2016: Proceedings of the 13th Intenational Symposium of Superalloys [C]. Warrendale, PA: TMS, 2016: 237
|
| 14 |
Ma D X, Wang F, Wu Q, et al. Temperature evolution and grain defect formation during single crystal solidification of a blade cluster [J]. Chin. Foundr., 2017, 14: 456
|
| 15 |
Ma D X. Novel casting processes for single-crystal turbine blades of superalloys [J]. Front. Mech. Eng., 2018, 13: 3
|
| 16 |
Giamei A F, Kear B H. On the nature of freckles in nickel base superalloys [J]. Metall. Trans., 1970, 1: 2185
|
| 17 |
Copley S M, Giamei A F, Johnson S M, et al. The origin of freckles in unidirectionally solidified castings [J]. Metall. Trans., 1970, 1: 2193
|
| 18 |
Auburtin P, Cockcroft S L, Mitchell A, et al. Liquid density inversions during the solidification of superalloys and their relationship to freckle formation in castings [A]. Superalloy 1996 [C]. Warrendale, PA: TMS, 1996: 443
|
| 19 |
Beckmann C, Gu J P, Boettinger W J. Development of a freckle predictor via Rayleigh number method for single-crystal nickel-base superalloy castings [J]. Metall. Mater. Trans., 2000, 31A: 2545
|
| 20 |
Ma D X, Bührig-Polaczek A. The geometrical effect on freckle formation in the directionally solidified superalloy CMSX-4 [J]. Metall. Mater. Trans., 2014, 45A: 1435
|
| 21 |
Ma D X. Freckle formation during directional solidification of complex castings of superalloys [J]. Acta Metall. Sin., 2016, 52: 426
|
| 21 |
马德新. 定向凝固的复杂形状高温合金铸件中的雀斑形成 [J]. 金属学报, 2016, 52: 426
|
| 22 |
Hong J P, Ma D X, Wang J, et al. Freckle defect formation near the casting interfaces of directionally solidified superalloys [J]. Materials, 2016, 9: 929
|
| 23 |
Hong J P, Ma D X, Wang J, et al. Geometrical effect of freckle formation on directionally solidified superalloy CM247 LC components [J]. J. Alloys Compd., 2015, 648: 1076
|
| 24 |
Ma D X, Zhou B, Bührig-Polaczek A. Investigation of freckle formation under various solidification conditions [J]. Adv. Mater. Res., 2011, 278: 428
|
| 25 |
Wilson B C, Cutler E R, Fuchs G E. Effect of solidification parameters on the microstructures and properties of CMSX-10 [J]. Mater. Sci. Eng., 2008, A479: 356
|
| 26 |
Khan T. Heat-resistant materials/superalloys [J]. Adv. Mater. Process, 1990, 137: 19
|
| 27 |
General Editorial Board of Aviation Manufacturing Engineering Manual. Aviation Manufacturing Engineering Manual, Heat Treatment Division [M]. Beijing: Aviation Industry Press, 1993: 325
|
| 27 |
《航空制造工程手册》总编委会. 航空制造工程手册——热处理 [M]. 北京: 航空工业出版社, 1993: 325
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|