					引用本文:
						|  |  
    					|  |  
    					| 直接包套轧制铸态Ti-46Al-8Nb合金的组织特征及热变形机制 |  
						| 李天瑞1, 刘国怀1(  ), 于少霞2, 王文娟2, 张风奕2, 彭全义2, 王昭东1 |  
					| 1 东北大学轧制技术与连轧自动化国家重点实验室 沈阳 110819 2 东北大学材料科学与工程学院 沈阳 110819
 |  
						|  |  
    					| Microstructure Evolution and Deformation Mechanisms by Direct Hot-Pack Rolling for As-Cast Ti-46Al-8Nb Alloys |  
						| LI Tianrui1, LIU Guohuai1(  ), YU Shaoxia2, WANG Wenjuan2, ZHANG Fengyi2, PENG Quanyi2, WANG Zhaodong1 |  
						| 1 State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819, China 2 School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China
 |  
								李天瑞, 刘国怀, 于少霞, 王文娟, 张风奕, 彭全义, 王昭东. 直接包套轧制铸态Ti-46Al-8Nb合金的组织特征及热变形机制[J]. 金属学报, 2020, 56(8): 1091-1102.	
																												Tianrui LI,
																								Guohuai LIU,
																								Shaoxia YU,
																								Wenjuan WANG,
																								Fengyi ZHANG,
																								Quanyi PENG,
																												Zhaodong WANG. 
				Microstructure Evolution and Deformation Mechanisms by Direct Hot-Pack Rolling for As-Cast Ti-46Al-8Nb Alloys[J]. Acta Metall Sin, 2020, 56(8): 1091-1102.
 
					
						| 
								
									|  
          
          
            
             
			              
            
									            
									                
																																															
																| [1] | Yang R. Advances and challenges of TiAl base alloys [J]. Acta Metall. Sin., 2015, 51: 129 doi: 10.11900/0412.1961.2014.00396
 |  
																| [1] | (杨 锐. 钛铝金属间化合物的进展与挑战 [J]. 金属学报, 2015, 51: 129) doi: 10.11900/0412.1961.2014.00396
 |  
																| [2] | Wu X H. Review of alloy and process development of TiAl alloys [J]. Intermetallics, 2006, 14: 1114 doi: 10.1016/j.intermet.2005.10.019
 |  
																| [3] | Dimiduk D M. Gamma titanium aluminide alloys—An assessment within the competition of aerospace structural materials [J]. Mater. Sci. Eng., 1999, A263: 281 |  
																| [4] | Tetsui T, Shindo K, Kobayashi S, et al. A newly developed hot worked TiAl alloy for blades and structural components [J]. Scr. Mater., 2002, 47: 399 doi: 10.1016/S1359-6462(02)00158-6
 |  
																| [5] | Draper S L, Krause D, Lerch B, et al. Development and evaluation of TiAl sheet structures for hypersonic applications [J]. Mater. Sci. Eng., 2007, A464: 330 |  
																| [6] | Semiatin S L, Ohls M, Kerr W R. Temperature transients during hot pack rolling of high temperature alloys [J]. Scr. Metall., 1991, 25: 1851 |  
																| [7] | Schwaighofer E, Clemens H, Mayer S, et al. Microstructural design and mechanical properties of a cast and heat-treated intermetallic multi-phase γ-TiAl based alloy [J]. Intermetallics, 2014, 44: 128 doi: 10.1016/j.intermet.2013.09.010
 |  
																| [8] | Kim J S, Lee Y H, Kim Y W, et al. High temperature deformation behavior of beta-gamma TiAl alloy [J]. Mater. Sci. Forum, 2007, 539-543: 1531 doi: 10.4028/www.scientific.net/MSF.539-543
 |  
																| [9] | Kong F T, Chen Y Y, Wang W, et al. Microstructures and mechanical properties of hot-pack rolled Ti-43Al-9V-Y alloy sheet [J]. Trans. Nonferrous Met. Soc. China, 2009, 19: 1126 doi: 10.1016/S1003-6326(08)60418-5
 |  
																| [10] | Liu Z C, Lin J P, Li S J, et al. Effects of Nb and Al on the microstructures and mechanical properties of high Nb containing TiAl base alloys [J]. Intermetallics, 2002, 10: 653 doi: 10.1016/S0966-9795(02)00037-7
 |  
																| [11] | Wang X, Lin J P, Zhang L Q, et al. Hot packed-rolling process of high-Nb TiAl alloy and its microstructure evolution [J]. Chin. J. Rare Met., 2010, 34: 658 |  
																| [11] | (王 兴, 林均品, 张来启等. 高铌TiAl基合金板材制备包套热轧工艺及组织控制 [J]. 稀有金属, 2010, 34: 658) |  
																| [12] | Chen G L, Xu X J, Teng Z K, et al. Microsegregation in high Nb containing TiAl alloy ingots beyond laboratory scale [J]. Intermetallics, 2007, 15: 625 doi: 10.1016/j.intermet.2006.10.003
 |  
																| [13] | Liu G H, Li X Z, Su Y Q, et al. Microstructure, microsegregation pattern and the formation of B2 phase in directionally solidified Ti-46Al-8Nb alloy [J]. J. Alloys Compd., 2012, 541: 275 doi: 10.1016/j.jallcom.2012.07.023
 |  
																| [14] | Li T R, Liu G H, Xu M, et al. Microstructures and high temperature tensile properties of Ti-43Al-4Nb-1.5Mo alloy in the canned forging and heat treatment process [J]. Acta Metall. Sin., 2017, 53: 1055 doi: 10.11900/0412.1961.2016.00457
 |  
																| [14] | (李天瑞, 刘国怀, 徐 莽等. Ti-43Al-4Nb-1.5Mo合金包套锻造与热处理过程的微观组织及高温拉伸性能 [J]. 金属学报, 2017, 53: 1055) doi: 10.11900/0412.1961.2016.00457
 |  
																| [15] | Prasad Y V R K, Gegel H L, Doraivelu S M, et al. Modeling of dynamic material behavior in hot deformation: Forging of Ti-6242 [J]. Metall. Trans., 1984, 15A: 1883 |  
																| [16] | Zhou J, Zeng W D, Shu Y, et al. Study on globularization of lamellar a structure in TC17 titanium alloy during hot deformation using processing map [J]. Rare Met. Mater. Eng., 2006, 35: 265 |  
																| [16] | (周 军, 曾卫东, 舒 滢等. 应用热加工图研究TC17合金片状组织球化规律 [J]. 稀有金属材料与工程, 2006, 35: 265) |  
																| [17] | Wang H, Tang H P, Liu Y, et al. Hot deformation behaviors and processing maps of as-cast TiAl based alloy [J]. Mater. Sci. Eng. Powder Metall., 2012, 17: 401 |  
																| [17] | (王 辉, 汤慧萍, 刘 咏等. 铸造TiAl基合金的热变形行为及加工图 [J]. 粉末冶金材料科学与工程, 2012, 17: 401) |  
																| [18] | Niu H Z, Kong F T, Xiao S L, et al. Effect of pack rolling on microstructures and tensile properties of as-forged Ti-44Al-6V-3Nb-0.3Y alloy [J]. Intermetallics, 2012, 21: 97 doi: 10.1016/j.intermet.2011.10.003
 |  
																| [19] | Wan Z P, Sun Y, Hu L X, et al. Experimental study and numerical simulation of dynamic recrystallization behavior of TiAl-based alloy [J]. Mater. Des., 2017, 122: 11 doi: 10.1016/j.matdes.2017.02.088
 |  
																| [20] | Appel F, Wagner R. Microstructure and deformation of two-phase γ-titanium aluminides [J]. Mater. Sci. Eng., 1998, R22: 187 |  
																| [21] | Li T R, Liu G H, Xu M, et al. Flow stress prediction and hot deformation mechanisms in Ti-44Al-5Nb-(Mo, V, B) alloy [J]. Materials, 2018, 11: 2044 doi: 10.3390/ma11102044
 |  
																| [22] | Liu G H, Wang Z D, Fu T L, et al. Study on the microstructure, phase transition and hardness for the TiAl-Nb alloy design during directional solidification [J]. J. Alloys Compd., 2015, 650: 45 doi: 10.1016/j.jallcom.2015.07.259
 |  
																| [23] | Liu G H, Li T R, Fu T L, et al. Morphology and competitive growth during the development of the parallel lamellar structure by self-seeding in directionally solidified Ti-50Al-4Nb alloy [J]. J. Alloys Compd., 2016, 682: 601 doi: 10.1016/j.jallcom.2016.05.028
 |  
																| [24] | Tang B, Cheng L, Kou H C, et al. Hot forging design and microstructure evolution of a high Nb containing TiAl alloy [J]. Intermetallics, 2015, 58: 7 doi: 10.1016/j.intermet.2014.11.002
 |  
																| [25] | Wang Q, Chen R R, Gong X, et al. Microstructure, mechanical properties, and crack propagation behavior in high-Nb TiAl alloys by directional solidification [J]. Metall. Mater. Trans., 2018, 49A: 4555 |  
             
												
											    	
											        	|  | Viewed |  
											        	|  |  |  
												        |  | Full text 
 | 
 
 |  
												        |  |  |  
												        |  | Abstract 
 | 
 |  
												        |  |  |  
												        |  | Cited |  |  
												        |  |  |  |  
													    |  | Shared |  |  
													    |  |  |  |  
													    |  | Discussed |  |  |  |  |