| 镁合金焊缝液化裂纹敏感性及预测方法探究 |
陈树君, 王宣, 袁涛( ), 李晓旭 |
| 北京工业大学机电学院汽车结构部件先进制造技术教育部工程研究中心 北京 100124 |
|
| Research on Prediction Method of Liquation Cracking Susceptibility to Magnesium Alloy Welds |
Shujun CHEN, Xuan WANG, Tao YUAN( ), Xiaoxu LI |
| Engineering Research Center of Advanced Manufacturing Technology for Automotive Components, Ministry of Education, Beijing University of Technology, Beijing 100124, China |
引用本文:
陈树君, 王宣, 袁涛, 李晓旭. 镁合金焊缝液化裂纹敏感性及预测方法探究[J]. 金属学报, 2018, 54(12): 1735-1744.
Shujun CHEN,
Xuan WANG,
Tao YUAN,
Xiaoxu LI.
Research on Prediction Method of Liquation Cracking Susceptibility to Magnesium Alloy Welds[J]. Acta Metall Sin, 2018, 54(12): 1735-1744.
| [1] | Froes F H, Eliezer D, Aghion E.The science, technology, and applications of magnesium[J]. JOM, 1998, 50(9): 30 | | [2] | Ishihara S, Nan Z Y, Goshima T. Effect of microstructure on fatigue behavior of AZ31 magnesium alloy [J]. Mater. Sci. Eng., 2007, A468-470: 214 | | [3] | Li W, Zhou H, Zhou W, et al.Effect of cooling rate on ignition point of AZ91D-0.98 wt.% Ce magnesium alloy[J]. Mater. Lett., 2007, 61: 2772 | | [4] | Montemor M F, Sim?es A M, Carmezim M J.Characterization of rare-earth conversion films formed on the AZ31 magnesium alloy and its relation with corrosion protection[J]. Appl. Surf. Sci., 2007, 253: 6922 | | [5] | Munitz A, Cotler C, Stern A, et al.Mechanical properties and microstructure of gas tungsten arc welded magnesium AZ91D plates[J]. Mater. Sci. Eng., 2001, A302: 68 | | [6] | Rethmeier M, Kleinpeter B, Wohlfahrt H.MIG welding of magnesium alloys metallographic aspects[J]. Weld. World, 2004, 48: 28 | | [7] | Yu Z H, Yan H G, Yin X Y, et al.Liquation cracking in laser beam welded joint of ZK60 magnesium alloy[J]. Trans. Nonferrous Met. Soc. China, 2012, 22: 2891 | | [8] | Ma B X, Zhao J X, Wang L P, et al.Research progress of welding hot crack of magnesium alloys[J]. Mater. Rev., 2016, 30(3): 81(马宝霞, 赵建勋, 王丽萍等. 镁合金焊接热裂纹的研究进展[J]. 材料导报, 2016, 30(3): 81) | | [9] | Zhou W, Long T Z, Mark C K.Hot cracking in tungsten inert gas welding of magnesium alloy AZ91D[J]. Mater. Sci. Technol., 2007, 23: 1294 | | [10] | Zhao X X.Liquefaction crack of welding[J]. Machinery, 1981,(11): 19(赵晓星. 焊接液化裂纹 [J]. 机械, 1981, (11): 19) | | [11] | Lippold J C, translated by Qu Z X, Zhang H Q, Wang D P. Welding Metallurgy and Weldability [M]. Beijing: Machinery Industry Press, 2017: 34(Lippold J C著, 屈朝霞, 张汉谦, 王东坡译. 焊接冶金与焊接性 [M]. 北京: 机械工业出版社, 2017: 34) | | [12] | Huang C, Kou S. Partially melted zone in aluminum welds—Liquation mechanism and directional solidification [J]. Weld. J., 2000, 79: 113-s | | [13] | Huang C, Kou S. Liquation cracking in full-penetration Al-Cu welds [J]. Weld. J., 2004, 83: 50-s | | [14] | Huang C, Kou S. Liquation cracking in full-penetration Al-Mg-Si welds [J]. Weld. J., 2004, 83: 111-s | | [15] | Cao G, Kou S. Predicting and reducing liquation-cracking susceptibility based on temperature vs. fraction solid [J]. Weld. J., 2006, 85: 9-s | | [16] | Sun D X.Study on weldability of magnesium alloys (AZ91D and AZ31B) [D]. Changchun: Jilin University, 2008(孙德新. 镁合金(AZ91D、AZ31B)焊接性的研究 [D]. 长春: 吉林大学, 2008) | | [17] | Yuan T.Study on welding metallurgy process and microstructure of magnesium welds with the external energy field [D]. Tianjin: Tianjin University, 2016(袁涛. 基于外加能量场的镁合金焊接冶金过程及微观组织研究 [D]. 天津: 天津大学, 2016) | | [18] | Yuan T, Chai X, Luo Z, et al.Predicting susceptibility of magnesium alloys to weld-edge cracking[J]. Acta Mater., 2015, 90: 242 | | [19] | Chai X, Yuan T, Kou S. Liquation and liquation cracking in partially melted zones of magnesium welds [J]. Weld. J., 2016, 95: 57-s | | [20] | Yuan T, Luo Z, Liu Y Y.Study on sensitivity of magnesium alloy weld to liquefaction crack[J]. Weld. Technol., 2016, 45(12): 14(袁涛, 罗震, 刘亚云. 镁合金焊缝液化裂纹敏感性研究[J]. 焊接技术, 2016, 45(12): 14) | | [21] | Kou S.Welding Metallurgy[M]. 2nd Ed., Hoboken, NJ: John Wiley & Sons, 2003: 301 | | [22] | Flemings M C.Solidification Processing[M]. New York: McGraw-Hill, 1974: 15 | | [23] | Kou S, Sun D K.Fluid flow and weld penetration in stationary arc welds[J]. Metall. Trans., 1985, 16A: 203 | | [24] | Kou S, Wang Y H.Computer simulation of convection in moving arc weld pools[J]. Metall. Trans., 1986, 17A: 2271 | | [25] | Tsai M C, Kou S.Marangoni convection in weld pools with a free surface[J]. Int. J. Numer. Methods Fluids, 1989, 9: 1503 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|