| 金属材料在三亚海水中的腐蚀电位序及合金成分对耐蚀性的影响 |
陈闽东1, 张帆1, 刘智勇1, 杨朝晖2, 丁国清2, 李晓刚1,3( ) |
1 北京科技大学腐蚀与防护中心教育部腐蚀与防护重点实验室 北京 100083 2 钢铁研究总院青岛海洋腐蚀研究所 青岛 266071 3 中国科学院宁波材料技术与工程研究所 宁波 315201 |
|
| Galvanic Series of Metals and Effect of Alloy Compositions on Corrosion Resistance in Sanya Seawater |
Mindong CHEN1, Fan ZHANG1, Zhiyong LIU1, Chaohui YANG2, Guoqing DING2, Xiaogang LI1,3( ) |
1 Key Laboratory for Corrosion and Protection, Ministry of Education, Corrosion and Protection Center, University of Science and Technology Beijing, Beijing 100083, China 2 Qingdao Marine Corrosion Research Institute, Central Iron & Steel Research Insititute, Qingdao 266071, China; 3 Ningbo Institute of Material Technology & Engineering, Chinese Academy of Sciences, Ningbo 315201, China; |
引用本文:
陈闽东, 张帆, 刘智勇, 杨朝晖, 丁国清, 李晓刚. 金属材料在三亚海水中的腐蚀电位序及合金成分对耐蚀性的影响[J]. 金属学报, 2018, 54(9): 1311-1321.
Mindong CHEN,
Fan ZHANG,
Zhiyong LIU,
Chaohui YANG,
Guoqing DING,
Xiaogang LI.
Galvanic Series of Metals and Effect of Alloy Compositions on Corrosion Resistance in Sanya Seawater[J]. Acta Metall Sin, 2018, 54(9): 1311-1321.
| [1] | Hou B R, Li X G, Ma X M, et al.The cost of corrosion in China[J]. npj Mater. Degrad., 2017, 1: 4 | | [2] | Sun F L, Ren S, Li Z, et al.Comparative study on the stress corrosion cracking of X70 pipeline steel in simulated shallow and deep sea environments[J]. Mater. Sci. Eng., 2017, A685: 145 | | [3] | Li T, Li X G, Dong C F, et al.Characterization of atmospheric corrosion of 2A12 aluminum alloy in tropical marine environment[J]. J. Mater. Eng. Perform., 2010, 19: 591 | | [4] | Ma Y T, Li Y, Wang F H.The effect of β-FeOOH on the corrosion behavior of low carbon steel exposed in tropic marine environment[J]. Mater. Chem. Phys., 2008, 112: 844 | | [5] | Wu J J, Zhang D, Wang P, et al.The influence of Desulfovibrio sp. and Pseudoalteromonas sp. on the corrosion of Q235 carbon steel in natural seawater[J]. Corros. Sci., 2016, 112: 552 | | [6] | Matsukawa Y, Chuta H, Miyashita M, et al.Galvanic series of metals conventionally used in tap water with and without flow and its comparison to that in seawater[J]. Corrosion, 2011, 67: 1389 | | [7] | Tewary N K, Kundu A, Nandi R, et al.Microstructural characterisation and corrosion performance of old railway girder bridge steel and modern weathering structural steel[J]. Corros. Sci., 2016, 113: 57 | | [8] | Liu M, Cheng X Q, Li X G, et al.Corrosion behavior and durability of low-alloy steel rebars in marine environment[J]. J. Mater. Eng. Perform., 2016, 25: 4967 | | [9] | Mu X, Wei J, Dong J H, et al.In situ corrosion monitoring of mild steel in a simulated tidal zone without marine fouling attachment by electrochemical impedance spectroscopy[J]. J. Mater. Sci. Technol., 2014, 30: 1043 | | [10] | Gao L F, Du M.Pitting corrosion behavior of 304 stainless steel in desalination seawater[J]. Corros. Sci. Prot. Technol., 2017, 29: 8(高丽飞, 杜敏. 304不锈钢在淡化海水中的点蚀行为[J]. 腐蚀科学与防护技术, 2017, 29: 8) | | [11] | Thierry D, Leballeur C, Larché N.Galvanic series in seawater as a function of temperature, oxygen content and chlorination[J]. Corrosion, 2018, 74: 147 | | [12] | Sun F L, Li X G, Lu L, et al.Corrosion behavior of copper alloys in deep ocean environment of South China Sea[J]. Acta Metall. Sin., 2013, 49: 1211(孙飞龙, 李晓刚, 卢琳等. 铜合金在中国南海深海环境下的腐蚀行为研究[J]. 金属学报, 2013, 49: 1211) | | [13] | Basumatary J, Wood R J K. Synergistic effects of cavitation erosion and corrosion for nickel aluminium bronze with oxide film in 3.5% NaCl solution [J]. Wear, 2017, 376-377: 1286 | | [14] | Mameng S H, Pettersson R, Leygraf C.Effect of stainless steel composition on atmospheric corrosion resistance at a marine site in Dubai[J]. Corrosion, 2017, 73: 880 | | [15] | Sun F L, Li X G, Lu L, et al.Corrosion behavior of 5052 and 6061 aluminum alloys in deep ocean environment of South China Sea[J]. Acta Metall. Sin., 2013, 49: 1219(孙飞龙, 李晓刚, 卢琳等. 5052和6061铝合金在中国南海深海环境下的腐蚀行为研究[J]. 金属学报, 2013, 49: 1219) | | [16] | Fin?gar M.Galvanic series of different stainless steels and copper-and aluminium-based materials in acid solutions[J]. Corros. Sci., 2013, 68: 51 | | [17] | Song W X.Metallography [M]. 2nd Ed., Beijing: Metallurgical Industry Press, 1989: 421(宋维锡. 金属学[M]. 第二版. 北京: 冶金工业出版社, 1989: 421) | | [18] | Hernandez-Sandoval J, Gonzalez-Lopez R, Hernandez-Rodriguez M A L, et al. Localized corrosion in an electrical submergible pump (ESP)[J]. Eng. Fail. Anal., 2015, 53: 124 | | [19] | Bokati K S, Dehghanian C, Yari S.Corrosion inhibition of copper, mild steel and galvanically coupled copper-mild steel in artificial sea water in presence of 1H-benzotriazole, sodium molybdate and sodium phosphate[J]. Corros. Sci., 2017, 126: 272 | | [20] | Li X G, Zhang D W, Liu Z Y, et al.Materials science: Share corrosion data[J]. Nature, 2015, 527: 441 | | [21] | Morcillo M, Díaz I, Chico B, et al.Weathering steels: From empirical development to scientific design. A review[J]. Corros. Sci., 2014, 83: 6 | | [22] | Zhou Y L, Chen J, Xu Y, et al.Effects of Cr, Ni and Cu on the corrosion behavior of low carbon microalloying steel in a Cl- containing environment[J]. J. Mater. Sci. Technol., 2013, 29: 168 | | [23] | Huang G Q.Study of the corrosion potential of metals in seawater[J]. Corros. Prot., 2000, 21(1): 8(黄桂桥. 金属在海水中的腐蚀电位研究[J]. 腐蚀与防护, 2000, 21(1): 8) | | [24] | Liu D Y, Wei K J.Corrosion potentials of metals in natural sea water of South China Sea[J]. Corros. Sci. Prot. Technol., 1991, 11: 330(刘大扬, 魏开金. 金属在南海海域腐蚀电位研究[J]. 腐蚀科学与防护技术, 1999, 11: 330) | | [25] | Mu X, Wei J, Dong J H, et al.The effect of sacrificial anode on corrosion protection of Q235B steel in simulated tidal zone[J]. Acta Metall. Sin., 2014, 50: 1294(穆鑫, 魏洁, 董建华等. 牺牲阳极保护对Q235B钢在模拟海洋潮差区间腐蚀行为的影响[J]. 金属学报, 2014, 50: 1294) | | [26] | Ding G Q, Yang C H, Huang G Q, et al.Corrosion potential of metals in natural river water[J]. Equip. Environ. Eng., 2017, 14(2): 31(丁国清, 杨朝晖, 黄桂桥等. 金属材料在天然河水中的腐蚀电位研究[J]. 装备环境工程, 2017, 14(2): 31) | | [27] | Hao W K, Liu Z Y, Wu W, et al.Electrochemical characterization and stress corrosion cracking of E690 high strength steel in wet-dry cyclic marine environments[J]. Mater. Sci. Eng., 2018, A710: 318 | | [28] | Dexter S C, Gao G Y.Effect of seawater biofilms on corrosion potential and oxygen reduction of stainless steel[J]. Corrosion, 1988, 44: 717 | | [29] | Liu B, Duan J Z, Hou B R.Microbiologically influenced corrosion of 316L SS by marine biofilms in seawater[J]. J. Chin. Soc. Corros. Protect., 2012, 32: 48(刘彬, 段继周, 侯保荣. 天然海水中微生物膜对316L不锈钢腐蚀行为研究[J]. 中国腐蚀与防护学报, 2012, 32: 48) | | [30] | Fischer D A, Daille L, Aguirre J, et al.Corrosion of stainless steel in simulated tide of fresh natural seawater of South East Pacific[J]. Int. J. Electrochem. Sci., 2016, 11: 6873 | | [31] | Katkar V A, Gunasekaran G.Galvanic corrosion of AA6061 with other ship building materials in seawater[J]. Corrosion, 2015, 72: 400 | | [32] | Ju H, Duan J Z, Yang Y, et al.Mapping the galvanic corrosion of three coupled metal alloys using coupled multielectrode array: Influence of chloride ion concentration[J]. Materials, 2018, 11: 634 | | [33] | Guo J, Yang S W, Shang C J, et al.Influence of carbon content and microstructure on corrosion behaviour of low alloy steels in a Cl- containing environment[J]. Corros. Sci., 2009, 51: 242 | | [34] | Wang Z F, Liu J R, Wu L X, et al.Study of the corrosion behavior of weathering steels in atmospheric environments[J]. Corros. Sci., 2013, 67: 1 | | [35] | Sedriks A J.Plenary lecture—1986: Effects of alloy composition and microstructure on the passivity of stainless steels[J]. Corrosion, 1986, 42: 376 | | [36] | Wu J S, Pang K, Peng D D, et al.Corrosion behaviors of carbon steels in artificially simulated and accelerated marine environment[J]. Int. J. Electrochem. Sci., 2017, 12: 1216 | | [37] | Melchers R E.Effect of small compositional changes on marine immersion corrosion of low alloy steels[J]. Corros. Sci., 2004, 46: 1669 | | [38] | Cheng X Q, Jin Z, Liu M, et al.Optimizing the nickel content in weathering steels to enhance their corrosion resistance in acidic atmospheres[J]. Corros. Sci., 2017, 115: 135 | | [39] | Xing P, Lu L, Li X G.Oxygen-concentration cell induced corrosion of E690 steel for ocean platform[J]. Chin. J. Mater. Res., 2016, 30: 241(邢佩, 卢琳, 李晓刚. 海洋用高强钢E690氧浓差腐蚀行为研究[J]. 材料研究学报, 2016, 30: 241) | | [40] | Ghahari M, Krouse D, Laycock N, et al.Synchrotron X-ray radiography studies of pitting corrosion of stainless steel: Extraction of pit propagation parameters[J]. Corros. Sci., 2015, 100: 23 | | [41] | Le Bozec N, Compère C, L'Her M, et al. Influence of stainless steel surface treatment on the oxygen reduction reaction in seawater[J]. Corros. Sci., 2001, 43: 765 | | [42] | Zhang T, Yang Y G, Shao Y W, et al.Advances of the analysis methodology for electrochemical noise[J]. J. Chin. Soc. Corros. Protect., 2014, 34: 1(张涛, 杨延格, 邵亚薇等. 电化学噪声分析方法的研究进展[J]. 中国腐蚀与防护学报, 2014, 34: 1) | | [43] | Li X G, Dong C F, Xiao K, et al.Corrosion behavior and mechanism of typical materials in Xisha ocean atmosphere environment [M]. Beijing: Science Press, 2014: 123(李晓刚, 董超芳, 肖葵等. 西沙海洋大气环境下典型材料腐蚀/老化行为与机理 [M]. 北京: 科学出版社, 2014: 123) | | [44] | Li J, Mayer J W, Colgan E G.Oxidation and protection in copper and copper alloy thin films[J]. J. Appl. Phys., 1991, 70: 2820 |
|
|