| X80管线钢表面SRB生物膜特征及腐蚀行为 |
舒韵1,2, 闫茂成1( ), 魏英华1, 刘福春1, 韩恩厚1, 柯伟1 |
1 中国科学院金属研究所 沈阳 110016 2 中国科学技术大学材料科学与工程学院 沈阳 110016 |
|
| Characteristics of SRB Biofilm and Microbial Corrosionof X80 Pipeline Steel |
Yun SHU1,2, Maocheng YAN1( ), Yinghua WEI1, Fuchun LIU1, En-Hou HAN1, Wei KE1 |
1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2 School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China |
引用本文:
舒韵, 闫茂成, 魏英华, 刘福春, 韩恩厚, 柯伟. X80管线钢表面SRB生物膜特征及腐蚀行为[J]. 金属学报, 2018, 54(10): 1408-1416.
Yun SHU,
Maocheng YAN,
Yinghua WEI,
Fuchun LIU,
En-Hou HAN,
Wei KE.
Characteristics of SRB Biofilm and Microbial Corrosionof X80 Pipeline Steel[J]. Acta Metall Sin, 2018, 54(10): 1408-1416.
| [1] | Hamilton W A.Sulphate-reducing bacteria and anaerobic corrosion[J]. Annu. Rev. Microbiol., 1985, 39: 195 | | [2] | Usher K M, Kaksonen A H, Cole I, et al.Critical review: Microbially influenced corrosion of buried carbon steel pipes[J]. Int. Biodeterior. Biodegrad., 2014, 93: 84 | | [3] | Kuang F, Wang J, Yan L, et al.Effects of sulfate-reducing bacteria on the corrosion behavior of carbon steel[J]. Electrochim. Acta, 2007, 52: 6084 | | [4] | Wolfram J H, Rogers R D, Gazsó L G.Microbial Degradation Processes in Radioactive Waste Repository and in Nuclear Fuel Storage Areas[M]. Netherlands: Springer, 1997: 37 | | [5] | Gaines R H.Bacterial activity as a corrosive influence in the soil[J]. Ind. Eng. Chem., 1910, 2: 128 | | [6] | Li F S, An M Z, Liu G Z, et al.Effects of sulfidation of passive film in the presence of SRB on the pitting corrosion behaviors of stainless steels[J]. Mater. Chem. Phys., 2009, 113: 971 | | [7] | Yu L, Duan J Z, Zhao W, et al.Characteristics of hydrogen evolution and oxidation catalyzed by Desulfovibrio caledoniensis biofilm on pyrolytic graphite electrode[J]. Electrochim. Acta, 2011, 56: 9041 | | [8] | Chen S Q, Wang P, Zhang D.The influence of sulphate-reducing bacteria on heterogeneous electrochemical corrosion behavior of Q235 carbon steel in seawater[J]. Mater. Corros., 2016, 67: 340 | | [9] | Xu F L, Duan J Z, Hou B R.Electron transfer process from marine biofilms to graphite electrodes in seawater[J]. Bioelectrochemistry, 2010, 78: 92 | | [10] | Xu D K, Li Y C, Gu T Y.Mechanistic modeling of biocorrosion caused by biofilms of sulfate reducing bacteria and acid producing bacteria[J]. Bioelectrochemistry, 2016, 110: 52 | | [11] | Zhang P Y, Xu D K, Li Y C, et al.Electron mediators accelerate the microbiologically influenced corrosion of 304 stainless steel by the Desulfovibrio vulgaris biofilm[J]. Bioelectrochemistry, 2015, 101: 14 | | [12] | Von Wolzogen Kuhr C A H. Unity of anaerobic and aerobic iron corrosion process in the soil[J]. Corrosion, 1961, 17: 293t | | [13] | Starkey R L.Interrelations between microorganisms and plant roots in the rhizosphere[J]. Bacteriol. Rev., 1958, 22: 154 | | [14] | King R A, Miller J D A. Corrosion by the sulphate-reducing bacteria[J]. Nature, 1971, 233: 491 | | [15] | Iverson W P.Corrosion of iron and formation of iron phosphide by Desulfovibrio desulfuricans[J]. Nature, 1968, 217: 1265 | | [16] | Pope D H, Morris E A.Some experiences with microbiologically-influenced corrosion of pipelines[J]. Mater. Performance, 1995, 34: 23 | | [17] | Evans T E, Hart A C, Skedgell A N.The nature of the film on coloured stainless steel[J]. Trans. IMF, 1973, 51: 108 | | [18] | Dinh H T, Kuever J, Mu?mann M, et al.Iron corrosion by novel anaerobic microorganisms[J]. Nature, 2004, 427: 829 | | [19] | Yu L, Duan J Z, Du X Q, et al.Accelerated anaerobic corrosion of electroactive sulfate-reducing bacteria by electrochemical impedance spectroscopy and chronoamperometry[J]. Electrochem. Commun., 2013, 26: 101 | | [20] | Xu D K, Gu T Y.Carbon source starvation triggered more aggressive corrosion against carbon steel by the Desulfovibrio vulgaris biofilm[J]. Int. Biodeterior. Biodegrad., 2014, 91: 74 | | [21] | Xu D K, Li Y C, Song F M, et al.Laboratory investigation of microbiologically influenced corrosion of C1018 carbon steel by nitrate reducing bacterium Bacillus licheniformis[J]. Corros. Sci., 2013, 77: 385 | | [22] | Li Y C, Xu D K, Chen C F, et al.Anaerobic microbiologically influenced corrosion mechanisms interpreted using bioenergetics and bioelectrochemistry: A review[J]. J. Mater. Sci. Technol., 2018, 34: 1713 | | [23] | Jia R, Tan J L, Jin P, et al.Effects of biogenic H2S on the microbiologically influenced corrosion of C1018 carbon steel by sulfate reducing Desulfovibrio vulgaris biofilm[J]. Corros. Sci., 2018, 130: 1 | | [24] | Yu L B, Yan M C, Ma J, et al.Sulfate reducing bacteria corrosion of pipeline steel in Fe-rich red soil[J]. Acta Metall. Sin., 2017, 53: 1568(于利宝, 闫茂成, 马健等. 富Fe红壤中管线钢的硫酸盐还原菌腐蚀行为[J]. 金属学报, 2017, 53: 1568) | | [25] | Lovley D R.Dissimilatory metal reduction[J]. Annu. Rev. Microbiol., 1993, 47: 263 | | [26] | Féron D.Nuclear Corrosion Science and Engineering [M]. Cambridge: Woodhead Publishing, 2012: 231 | | [27] | Sun C, Xu J, Wang F H, et al.Interaction of sulfate-reducing bacteria and carbon steel Q235 in biofilm[J]. Ind. Eng. Chem. Res., 2011, 50: 12797 | | [28] | Liu H F, Liu L W, Xu L M, et al.Effects of biofilm on corrosion of carbon steel[J]. J. Chin. Soc. Corros. Pro., 1999, 19: 291(刘宏芳, 刘烈炜, 许立铭等. 生物膜对碳钢腐蚀的影响[J]. 中国腐蚀与防护学报, 1999, 19: 291) | | [29] | Chen L P.Biofilms and biofouling[J]. Corros. Prot., 1996, 17: 3(陈六平. 生物膜与生物污损[J]. 腐蚀与防护, 1996, 17: 3) | | [30] | Lee W, Characklis W G.Corrosion of mild steel under anaerobic biofilm[J]. Corrosion, 1993, 49: 186 | | [31] | Yuan W S.Corrosion behavior under biofilm of metal material in the circulation cooling water system [D]. Beijing: Beijing Jiaotong University, 2008(苑维双. 循环冷却水中微生物膜下金属材料腐蚀行为研究 [D]. 北京: 北京交通大学, 2008) | | [32] | Awad A M, Ghazy E A, Abo El-Enin S A, et al. Electropolishing of AISI-304 stainless steel for protection against SRB biofilm[J]. Surf. Coat. Technol., 2012, 206: 3165 | | [33] | Sherar B W A, Power I M, Keech P G, et al. Characterizing the effect of carbon steel exposure in sulfide containing solutions to microbially induced corrosion[J]. Corros. Sci., 2011, 53: 955 | | [34] | Wu T Q, Yang P, Zhang M D, et al.Microbiologically induced corrosion of X80 pipeline steel in an acid soil solution: (II) Corrosion morphology and corrosion product analysis[J]. J. Chin. Soc. Corros. Prot., 2014, 34: 353(吴堂清, 杨圃, 张明德等. 酸性土壤浸出液中X80钢微生物腐蚀研究: (II)腐蚀形貌和产物分析[J]. 中国腐蚀与防护学报, 2014, 34: 353) | | [35] | AlAbbas F M, Williamson C, Bhola S M, et al. Influence of sulfate reducing bacterial biofilm on corrosion behavior of low-alloy, high-strength steel (API-5L X80)[J]. Int. Biodeterior. Biodegrad., 2013, 78: 34 | | [36] | Yuan S J, Liang B, Zhao Y, et al.Surface chemistry and corrosion behaviour of 304 stainless steel in simulated seawater containing inorganic sulphide and sulphate-reducing bacteria[J]. Corros. Sci., 2013, 74: 353 | | [37] | Siriwardane R V, Cook J M.Interactions of SO2 with sodium deposited on CaO[J]. J. Colloid Interf. Sci., 1986, 114: 525 | | [38] | Abraham K M, Chaudhri S M.The lithium surface film in the Li/SO2 cell[J]. J. Electrochem. Soc., 1986, 133: 1307 | | [39] | Peisert H, Chassé T, Streubel P, et al.Relaxation energies in XPS and XAES of solid sulfur-compounds[J]. J. Electron. Spectrosc. Relat. Phenom., 1994, 68: 321 | | [40] | Wu T Q, Xu J, Yan M C, et al.Synergistic effect of sulfate-reducing bacteria and elastic stress on corrosion of X80 steel in soil solution[J]. Corros. Sci., 2014, 83: 38 | | [41] | Yu X R, Liu F, Wang Z Y, et al.Auger parameters for sulfur-containing compounds using a mixed aluminum-silver excitation source[J]. J. Electron. Spectrosc. Relat. Phenom., 1990, 50: 159 | | [42] | Jin J T, Wu G X, Zhang Z H, et al.Effect of extracellular polymeric substances on corrosion of cast iron in the reclaimed wastewater[J]. Bioresour. Technol., 2014, 165: 162 | | [43] | Dong Z H, Liu T, Liu H F.Influence of EPS isolated from thermophilic sulphate-reducing bacteria on carbon steel corrosion[J]. Biofouling, 2011, 27: 487 | | [44] | Huang Y, Liu S J, Jiang C Y.Microbiologically influenced corrosion and mechanisms[J]. Microbiol. China, 2017, 44: 1699(黄烨, 刘双江, 姜成英. 微生物腐蚀及腐蚀机理研究进展[J]. 微生物学通报, 2017, 44: 1699) | | [45] | Yan M C, Sun C, Xu J, et al.Electrochemical behavior of API X80 steel in acidic soils from Southeast China[J]. Int. J. Electrochem. Sci., 2015, 10: 1762 | | [46] | Feliu V, González J A, Andrade C, et al.Equivalent circuit for modelling the steel-concrete interface. I. Experimental evidence and theoretical predictions[J]. Corros. Sci., 1998, 40: 975 |
|
|