富Fe红壤中管线钢的硫酸盐还原菌腐蚀行为 |
于利宝1,2, 闫茂成1(), 马健3, 吴明浩3, 舒韵1,4, 孙成1, 许进1, 于长坤1, 卿永长1,2 |
1 中国科学院金属研究所 沈阳 110016 2 中国科学院大学 北京100049 3 中国石油新疆油田油气储运分公司 克拉玛依 834002 4 中国科学技术大学材料科学与工程学院 沈阳 110016 |
|
Sulfate Reducing Bacteria Corrosion of Pipeline Steel inFe-Rich Red Soil |
Libao YU1,2, Maocheng YAN1(), Jian MA3, Minghao WU3, Yun SHU1,4, Cheng SUN1, Jin XU1, Changkun YU1, Yongchang QING1,2 |
1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2 University of Chinese Academy of Sciences, Beijing 100049, China 3 Xinjiang Oilfield Branch Company, China National Petroleum Corporation, Karamay 834002, China 4 School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China |
引用本文:
于利宝, 闫茂成, 马健, 吴明浩, 舒韵, 孙成, 许进, 于长坤, 卿永长. 富Fe红壤中管线钢的硫酸盐还原菌腐蚀行为[J]. 金属学报, 2017, 53(12): 1568-1578.
Libao YU,
Maocheng YAN,
Jian MA,
Minghao WU,
Yun SHU,
Cheng SUN,
Jin XU,
Changkun YU,
Yongchang QING.
Sulfate Reducing Bacteria Corrosion of Pipeline Steel inFe-Rich Red Soil[J]. Acta Metall Sin, 2017, 53(12): 1568-1578.
[1] | Hamilton W A.Sulphate-reducing bacteria and anaerobic corrosion[J]. Annu. Rev. Microbiol., 1985, 9: 195 | [2] | Usher K M, Kaksonen A H, Cole I, et al.Critical review: Microbially influenced corrosion of buried carbon steel pipes[J]. Int. Biodeter. Biodegr., 2014, 93: 84 | [3] | Shi X B, Xu D K, Yan M C, et al.Study on microbiologically influenced corrosion behavior of novel Cu-bearing pipeline steels[J]. Acta Metall. Sin., 2017, 53: 153(史显波, 徐大可, 闫茂成等. 新型含Cu管线钢的微生物腐蚀行为研究[J]. 金属学报, 2017, 53: 153) | [4] | Kuang F, Wang J, Yan L, et al.Effects of sulfate-reducing bacteria on the corrosion behavior of carbon steel[J]. Electrochim. Acta, 2007, 52: 6084 | [5] | von Wolzogen Kuhr C A H. Unity of anaerobic and aerobic iron corrosion process in the soil[J]. Corrosion, 1961, 17: 293t | [6] | Iversen A.Microbially influenced corrosion on stainless steel in waste water treatment plants: Part 2[J]. Br. Corros. J., 2001, 36: 284 | [7] | Dinh H T, Kuever J, Mu?mann M, et al.Iron corrosion by novel anaerobic microorganisms[J]. Nature, 2004, 427: 829 | [8] | Reguera G, McCarthy K D, Mehta T, et al. Extracellular electron transfer via microbial nanowires[J]. Nature, 2005, 435: 1098 | [9] | Xu D K, Gu T Y.Carbon source starvation triggered more aggressive corrosion against carbon steel by the Desulfovibrio vulgaris biofilm[J]. Int. Biodeter. Biodegr., 2014, 91: 74 | [10] | Enning D, Garrelfs J.Corrosion of iron by sulfate-reducing bacteria: New views of an old problem[J]. Appl. Environ. Microbiol., 2014, 80: 1226 | [11] | Lovley D R.Dissimilatory metal reduction[J]. Annu. Rev. Microbiol., 1993, 47: 263 | [12] | Lovley D R. Dissimilatory Fe(III) and Mn(IV) reduction[J]. Microbiol. Rev., 1991, 55: 259 | [13] | Lovley D R. Organic matter mineralization with the reduction of ferric iron: A review[J]. Geomicrobiol. J., 1987, 5: 375 | [14] | Liu D, Dong H, Bishop M E, et al.Microbial reduction of structural iron in interstratified illite-smectite minerals by a sulfate-reducing bacterium[J]. Geobiology, 2012, 10: 150 | [15] | Gorby Y A, Yanina S, McLean J S, et al. Electrically conductive bacterial nanowires produced by Shewanella oneidensis strain MR-1 and other microorganisms[J]. Proc. Natl. Acad. Sci. USA, 2006, 103: 11358 | [16] | Li Y L, Vali H, Sears S K, et al.Iron reduction and alteration of nontronite NAu-2 by a sulfate-reducing bacterium[J]. Geochim. Cosmochim. Acta, 2004, 68: 3251 | [17] | Cao C N.Material Natural Environment Corrosion in China [M]. Beijing: Chemical Industry Press, 2005: 87(曹楚南. 中国材料的自然环境腐蚀 [M]. 北京: 化学工业出版社, 2005: 87) | [18] | Xu R K, Zhao A Z, Li Q M, et al.Acidity regime of the Red Soils in a subtropical region of southern China under field conditions[J]. Geoderma, 2003, 115: 75 | [19] | Yan M C, Sun C, Xu J, et al.Role of Fe oxides in corrosion of pipeline steel in a red clay soil[J]. Corros. Sci., 2014, 80: 309 | [20] | Yan M C, Sun C, Dong J H, et al.Electrochemical investigation on steel corrosion in iron-rich clay[J]. Corros. Sci., 2015, 97: 62 | [21] | Coleman M L, Hedrick D B, Lovley D R, et al.Reduction of Fe(III) in sediments by sulphate-reducing bacteria[J]. Nature, 1993, 361: 436 | [22] | Iversen A.Microbially influenced corrosion on stainless steels in waste water treatment plants: Part 1[J]. Br. Corros. J., 2001, 36: 277 | [23] | Yu L, Duan J Z, Du X Q, et al.Accelerated anaerobic corrosion of electroactive sulfate-reducing bacteria by electrochemical impedance spectroscopy and chronoamperometry[J]. Electrochem. Commun., 2013, 26: 101 | [24] | Yu L, Duan J Z, Zhao W, et al.Characteristics of hydrogen evolution and oxidation catalyzed by Desulfovibrio caledoniensis biofilm on pyrolytic graphite electrode[J]. Electrochim. Acta, 2011, 56: 9041 | [25] | Feliu V, González J A, Andrade C, et al.Equivalent circuit for modelling the steel-concrete interface. I. Experimental evidence and theoretical predictions[J]. Corros. Sci., 1998, 40: 975 | [26] | Barbalat M, Lanarde L, Caron D, et al.Electrochemical study of the corrosion rate of carbon steel in soil: Evolution with time and determination of residual corrosion rates under cathodic protection[J]. Corros. Sci., 2012, 55: 246 | [27] | Erable B, Du?eanu N M, Ghangrekar M M, et al.Application of electro-active biofilms[J]. Biofouling, 2010, 26: 57 | [28] | Yan M C, Sun C, Xu J, et al.Electrochemical behavior of API X80 steel in acidic soils from southeast China[J]. Int. J. Electrochem. Sci., 2015, 10: 1762 | [29] | Bo R, Kosec T, Kranjc A, et al.Electrochemical impedance spectroscopy of pure copper exposed in bentonite under oxic conditions[J]. Electrochim. Acta, 2011, 56: 7862 | [30] | Li C, Du C W, Liu Z Y, et al.Characteristics of electrochemical impedance spectroscopy for X100 pipeline steel in water-saturated acidic soil[J]. J. Chin. Soc. Corros. Prot., 2011, 31: 377(李超, 杜翠薇, 刘智勇等. X100管线钢在水饱和酸性土壤中的电化学阻抗谱特征[J]. 中国腐蚀与防护学报, 2011, 31: 377) | [31] | Xu R K, Zhao A Z, Li Q M, et al.Acidity regime of the Red Soils in a subtropical region of southern China under field conditions[J]. Geoderma, 2003, 115: 75 | [32] | Yan M C, Sun C, Xu J, et al.Anoxic corrosion behavior of pipeline steel in acidic soils[J]. Ind. Eng. Chem. Res., 2014, 53: 17615 | [33] | Bockheim J G, Mazhitova G, Kimble J M, et al.Controversies on the genesis and classification of permafrost-affected soils[J]. Geoderma, 2006, 137: 33 | [34] | Gotoh S, Patrick Jr W H. Transformation of iron in a waterlogged soil as influenced by redox potential and pH[J]. Soil Sci. Soc. Am. J., 1974, 38: 66 | [35] | Patrick Jr W H, Henderson R E. Reduction and reoxidation cycles of manganese and iron in flooded soil and in water solution[J]. Soil Sci. Soc. Am. J., 1981, 45: 855 | [36] | Li Y L, Vali H, Yang J, et al.Reduction of iron oxides enhanced by a sulfate-reducing bacterium and biogenic H2S[J]. Geomicrobiol. J., 2006, 23: 103 | [37] | Michel C, Brugna M, Aubert C, et al.Enzymatic reduction of chromate: Comparative studies using sulfate-reducing bacteria. Key role of polyheme cytochromes c and hydrogenases[J]. Appl. Microbiol. Biotechnol., 2001, 55: 95 | [38] | Tebo B M, Obraztsova A Y.Sulfate-reducing bacterium grows with Cr(VI), U(VI), Mn(IV), and Fe(III) as electron acceptors[J]. FEMS Microbiol. Lett., 1998, 162: 193 | [39] | Bond D R, Lovley D R.Electricity production by Geobacter sulfurreducens attached to electrodes[J]. Appl. Environ. Microbiol., 2003, 69: 1548 | [40] | Holmes D E, Bond D R, Lovley D R.Electron transfer by Desulfobulbus propionicus to Fe(III) and graphite electrodes[J]. Appl. Environ. Microbiol., 2004, 70: 1234 | [41] | Zhang J C, Xun W B, Zhu Z, et al.Influence of long-term fertilizer treatments on the fluorescence spectroscopic characterization of DOM leached by acid rain from red soil[J]. Soil Sci., 2013, 178: 639 | [42] | Luu Y S, Ramsay J A.Review: Microbial mechanisms of accessing insoluble Fe(III) as an energy source[J]. World J. Microbiol. Biotechnol., 2003, 19: 215 | [43] | Rabaey K, Rodríguez J, Blackall L L, et al.Microbial ecology meets electrochemistry: Electricity-driven and driving communities[J]. ISME J., 2007, 1: 9 | [44] | Tugel J B, Hines M E, Jones G E.Microbial iron reduction by enrichment cultures isolated from estuarine sediments[J]. Appl. Environ. Microbiol., 1986, 52: 1167 |
|
|