大型铸锭均质化问题及其新解 |
李军1,2, 夏明许1, 胡侨丹1, 李建国1,2( ) |
1 上海交通大学材料科学与工程学院 上海 200240 2 上海交通大学高新船舶与深海开发装备协同创新中心 上海 200240 |
|
Solutions in Improving Homogeneities of Heavy Ingots |
Jun LI1,2, Mingxu XIA1, Qiaodan HU1, Jianguo LI1,2( ) |
1 School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China 2 Collaborative Innovation Center for Advanced Ship and Deep-Sea Exploration, Shanghai Jiao Tong University, Shanghai 200240, China |
引用本文:
李军, 夏明许, 胡侨丹, 李建国. 大型铸锭均质化问题及其新解[J]. 金属学报, 2018, 54(5): 773-788.
Jun LI,
Mingxu XIA,
Qiaodan HU,
Jianguo LI.
Solutions in Improving Homogeneities of Heavy Ingots[J]. Acta Metall Sin, 2018, 54(5): 773-788.
[1] | Zhao J W, Chen X W, Shi Y L, et al.The current stage and development trend of forging technology and defect control for heavy forging[J]. China Metalform. Equip. Manuf. Technol., 2009, 44(4): 23(赵俊伟, 陈学文, 史宇麟等. 大型锻件锻造工艺及缺陷控制技术的研究现状及发展趋势[J]. 锻压装备与制造技术, 2009, 44(4): 23) | [2] | Kurz W, Fisher D, translated by Li J G, Hu Q D. Fundamentals of solidification [M]. Beijing: Higher Education Press, 2010: 1(Kurz W, Fisher D J著, 李建国, 胡侨丹译. 凝固原理 [M]. 北京: 高等教育出版社, 2010: 1) | [3] | Zhang Y.Urgency of domestic production of heavy casting and forging in China[J]. Heavy Mach., 2009, (4): 1(张扬. 我国大型铸锻件应坚持国产化之路[J]. 重型机械, 2009, (4): 1) | [4] | Li D Z, Chen X Q, Fu P X, et al.Inclusion flotation-driven channel segregation in solidifying steels[J]. Nat. Commun., 2015, 5: 5572 | [5] | Ding Z Y, Hu Q D, Zeng L, et al.Hot deformation characteristics of as-cast high-Cr ultra-super-critical rotor steel with columnar grains[J]. Int. J. Miner. Metall. Mater., 2016, 23: 1275 | [6] | Bitterlin M, Loucif A, Charbonnier N, et al.Cracking mechanisms in large size ingots of high nickel content low alloyed steel[J]. Eng. Fail. Anal., 2016, 68: 122 | [7] | Zhang X X, Cui Z S, Chen W, et al.A criterion for void closure in large ingots during hot forging[J]. J. Mater. Proc. Technol., 2009, 209: 1950 | [8] | Iron Steel Institute.Report on the heterogeneity of steel ingots[J]. J. Iron. Steel. I., 1926, 113: 39 | [9] | Olsson A, West R, Fredriksson H.Macrosegregation in ingots[J]. Scand. J. Metall., 1986, 15: 104 | [10] | Chvorinov N.Theory of the solidification of castings[J]. Giesserei, 1940, 27: 177 | [11] | Zhu Y X.Low segregation superalloys[J]. Trans. Met. Heat Treat., 1997, 18(3): 16(朱耀霄. 低偏析高温合金[J]. 金属热处理学报, 1997, 18(3): 16) | [12] | Zeng L, Zhang W, Ji Y L, et al.Improving cooling rate during solidification by eliminating the metal-mold interfacial gap[J]. Metall. Mater. Trans., 2015, 46A: 2819 | [13] | Ling Y F, Hu C J.Application of inner chilling on heavy thick wall steel castings[J]. China Found. Mach. Technol., 2010, (2): 36(凌云飞, 胡昌军. 内冷铁在厚大铸钢件上的应用[J]. 中国铸造装备与技术, 2010, (2): 36) | [14] | Sang B G, Kang X H, Li D Z.A novel technique for reducing macrosegregation in heavy steel ingots[J]. J. Mater. Process. Technol., 2010, 210: 703 | [15] | Zhao J, Yu J H, Li Q J, et al.Structure of slowly solidified 30Cr2Ni4MoV casting with surface pulsed magneto-oscillation[J]. Mater. Sci. Technol., 2015, 31: 1589 | [16] | Zeng L, Xu M Q, Ma X R, et al.Grain refinement and delta ferrite reduction of high Cr steel ingots by thermal control[J]. ISIJ Int., 2014, 54: 2302 | [17] | Wang C H, Zhang J, Liu L, et al.Microstructure evolution of directionally solidified DZ125 superalloy with melt superheating treatment[J]. J. Alloys Compd., 2010, 508: 440 | [18] | Liao X L, Zhao Q J, Luo J, et al.Refining mechanism of the electric current pulse on the solidification structure of pure aluminum[J]. Acta Mater., 2007, 55: 3103 | [19] | Cui J Z, Zhang Z Q, Le Q Z.DC casting of light alloys under magnetic fields[J]. Trans. Nonferrous Met. Soc. China, 2010, 20: 2046 | [20] | Liu Q M, Zhai Q J, Qi F P, et al.Effects of power ultrasonic treatment on microstructure and mechanical properties of T10 steel[J]. Mater. Lett., 2007, 61: 2422 | [21] | Fu H, Zhou Q, Tan S L.Influence of mechanical vibration on solidification structures of ignition-proof magnesium alloy AZ91D-3Ca[J]. Spec. Cast. Nonferrous Alloys, 2013, 33: 565(付浩, 周全, 谭水淋. 机械振动对AZ91D-3Ca镁合金凝固组织的影响[J]. 特种铸造及有色合金, 2013, 33: 565) | [22] | Jiang X L.Research and application of extreme manufacturing technology for 600 tonner low segregation and high purity heavy alloy ingot[J]. Heavy Cast. Forg., 2013, (5): 15(蒋新亮. 600吨级低偏析高纯净特大合金钢锭极限制造技术研究与应用[J]. 大型铸锻件, 2013, (5): 15) | [23] | Doub V S, Romashkin A N, Malginov A N.Main trends in the development of technology for casting steel into ingots[J]. Metallurgist, 2013, 57: 487 | [24] | Gao J J, Ba J T.Research on manufacturing technology of super large steel ingot[J]. Heavy Cast. Forg., 2013, (2): 7(高建军, 巴钧涛. 超大型钢锭制造技术研究[J]. 大型铸锻件, 2013, (2): 7) | [25] | Tanaka Y, Sato I.Development of high purity large forgings for nuclear power plants[J]. J. Nucl. Mater., 2011, 417: 854 | [26] | Tu W T, Zhang X, Shen H F, et al.Numerical simulation on multiple pouring process for a 292 t steel ingot[J]. China Found., 2014, 11: 52 | [27] | Tu W T, Shen H F, Liu B C.Modelling of macrosegregation in a 231-ton steel ingot with multi-pouring process[J]. Mater. Res. Innov., 2015, 19(Suppl.4): S59 | [28] | Li J, Liu D R, Kang X H, et al.Numerical simulation of delayed pouring technique for a 360t heavy steel ingot[J]. IOP Conf. Ser.: Mater. Sci. Eng., 2012, 33: 012092 | [29] | Tateno M.Development of large size high quality steels and their future prospects as "Near Net Shape" material[J]. Trans. Iron Steel Inst. Jpn., 1985, 25: 97 | [30] | Lesoult G. Macrosegregation in steel strands and ingots: Characterisation, formation and consequences [J]. Mater. Sci. Eng., 2005, A413-414: 19 | [31] | Flemings M C.Principles of control of soundness and homogeneity of large ingots[J]. Scand. J. Metall., 1976, 5: 1 | [32] | Pickering E J, Chesman C, Al-Bermani S, et al.A comprehensive case study of macrosegregation in a steel ingot[J]. Metall. Mater. Trans., 2015, 46B: 1860 | [33] | Duan Z H, Tu W T, Shen B Z, et al.Experimental measurements for numerical simulation of macrosegregation in a 36-ton steel ingot[J]. Metall. Mater. Trans., 2016, 47A: 3597 | [34] | Kawai M.On the Λ segregated zone of large carbon steel ingot (II): Mechanism of formation of the Λ segregated line (Part 2)[J]. ISIJ Int., 1956, 42: 19 | [35] | Li J, Wu M H, Ludwig A, et al.Simulation of macrosegregation in a 2.45-ton steel ingot using a three-phase mixed columnar-equiaxed model[J]. Int. J. Heat Mass Tran., 2014, 72: 668 | [36] | Flemings M C.Solidification processing[M]. New York: McGraw-Hill Book Company, 1974 | [37] | Shen H F, Chen K X, Liu B C.Numerical simulation of macrosegregation in steel ingot casting[J]. Acta Metall. Sin., 2018, 54: 151(沈厚发, 陈康欣, 柳百成. 钢锭铸造过程宏观偏析数值模拟[J]. 金属学报, 2018, 54: 151) | [38] | Shibata H, Poirier D R, Emi T.Modeling the behavior of Al2O3 inclusions during the dendritic solidification of steel[J]. ISIJ Int., 1998, 38: 339 | [39] | Qi J H, Wu J, Suo J P, et al.Discussion on the research method of fine inclusions in steel[J]. Metall. Anal., 2010, 30(10): 1(齐江华, 吴杰, 索进平等. 钢中细小夹杂物的研究方法探讨[J]. 冶金分析, 2010, 30(10): 1) | [40] | Zhang L F, Thomas B G.State of the art in the control of inclusions during steel ingot casting[J]. Metall. Mater. Trans., 2006, 37B: 733 | [41] | Liu H W, Fu P X, Kang X H, et al.Formation mechanism of shrinkage and large inclusions of a 70t 12Cr2Mo1 heavy steel ingot[J]. China Found., 2014, 11: 46 | [42] | Wang M L, Cheng G G, Zhao P, et al.Formation thermodynamics of titanium oxide during solidification of low carbon steel containing titanium[J]. J. Iron Steel Res., 2004, 16(3): 40(王明林, 成国光, 赵沛等. 含钛低碳钢凝固过程中氧化钛形成的热力学[J]. 钢铁研究学报, 2004, 16(3): 40) | [43] | Park S C, Jung I H, Oh K S, et al.Effect of Al on the evolution of non-metallic inclusions in the Mn-Si-Ti-Mg deoxidized steel during solidification: Experiments and thermodynamic calculations[J]. ISIJ Int., 2004, 44: 1016 | [44] | Gu L M, Chen Z P, Xu Y T, et al.Thermodynamic analysis of formation of inclusions in super purity ferritic stainless steel[J]. J. Chin. Rare Earth Soc., 2010, 28(Spec. Issue): 16(顾磊明, 陈兆平, 徐迎铁等. 超纯铁素体不锈钢中夹杂物形成的热力学分析[J]. 中国稀土学报, 2010, 28(专辑): 16) | [45] | Wang H P, Sun L F, Peng B, et al.Inclusions for ultra-pure ferritic stainless steels containing 21% chromium[J]. J. Iron Steel Res. Int., 2013, 20: 70 | [46] | Henschel S, Gleinig J, Lippmann T, et al.Effect of crucible material for ingot casting on detrimental non-metallic inclusions and the resulting mechanical properties of 18CrNiMo7-6 steel[J]. Adv. Eng. Mater., 2017, 19: 1700199 | [47] | Liu J H, Zhuang C L, Cui X N, et al.Inclusion distribution in ingots investigated by dissection[J]. J. Iron Steel Res. Int., 2014, 21: 660 | [48] | Zhu H C, Li H B, Zhang S C, et al.Numerical simulation of Mo macrosegregation during ingot casting of high-Mo austenitic stainless steel[J]. Ironmaking Steelmaking, 2015, 42: 748 | [49] | Hu H J, Yang M B, Luo J, et al.Application of the software ProCAST in the casting of solidification simulation[J]. Mater. Sci. Technol., 2006, 14: 293(胡红军, 杨明波, 罗静等. ProCAST软件在铸造凝固模拟中的应用[J]. 材料科学与工艺, 2006, 14: 293) | [50] | Zhou J X, Liu R X, Chen L L, et al.Application of inteCAST software to permanent mold casting[J]. Foundry, 2003, 52: 616(周建新, 刘瑞祥, 陈立亮等. 华铸CAE软件在金属型铸造中的应用[J]. 铸造, 2003, 52: 616) | [51] | Zhang Z, Yang J.Application of CASTsoft in low pressure casting[J]. Mechan. Manage. Dev., 2006, (3): 53(张诤, 杨晶. CASTsoft软件在低压铸造中的应用[J]. 机械管理开发, 2006, (3): 53) | [52] | Yang J A, Duan Z H, Shen H F, et al.Validation of CAFE model with experimental macroscopic grain structures in a 36-ton steel ingot [A]. Proceedings of the 4th World Congress on Integrated Computational Materials Engineering (ICME 2017)[C]. Cham: Springer, 2017 | [53] | Flemings M C, Nereo G E.Macrosegregation, Part I[J]. Trans. Met. Soc. AIME, 1967, 242: 1449 | [54] | Fujii T, Poirier D R, Flemings M C.Macrosegregation in a multicomponent low alloy steel[J]. Metall. Trans., 1979, 10B: 331 | [55] | Ridder S D, Kou S, Mehrabian R.Effect of fluid flow on macrosegregation in axi-symmetric ingots[J]. Metall. Trans., 1981, 12B: 435 | [56] | Szekely J, Jassal A S.An experimental and analytical study of the solidification of a binary dendritic system[J]. Metall. Trans., 1978, 9B: 389 | [57] | Bennon W D, Incropera F P.A continuum model for momentum, heat and species transport in binary solid-liquid phase change systems—I. Model formulation[J]. Int. J. Heat Mass Transfer, 1987, 30: 2161 | [58] | Beckermann C, Viskanta R.Double-diffusive convection during dendritic solidification of a binary mixture[J]. Physicochem. Hydrodyn., 1988, 10: 195 | [59] | Ganesan S, Poirier D R.Conservation of mass and momentum for the flow of interdendritic liquid during solidification[J]. Metall. Trans., 1990, 21B: 173 | [60] | Voller V R, Brent A D, Prakash C.The modelling of heat, mass and solute transport in solidification systems[J]. Int. J. Heat Mass Transfer, 1989, 32: 1719 | [61] | Ahmad N, Rappaz J, Desbiolles J L, et al.Numerical simulation of macrosegregation: A comparison between finite volume method and finite element method predictions and a confrontation with experiments[J]. Metall. Mater. Trans., 1998, 29A: 617 | [62] | Chiang K C, Tsai H L.Interaction between shrinkage-induced fluid flow and natural convection during alloy solidification[J]. Int. J. Heat Mass Transfer, 1992, 35: 1771 | [63] | Schneider M C, Beckermann C.Formation of macrosegregation by multicomponent thermosolutal convection during the solidification of steel[J]. Metall. Mater. Trans., 1995, 26A: 2373 | [64] | Gu J P, Beckermann C.Simulation of convection and macrosegregation in a large steel ingot[J]. Metall. Mater. Trans., 1999, 30A: 1357 | [65] | Combeau H, Zalo?nik M, Hans S, et al.Prediction of macrosegregation in steel ingots: Influence of the motion and the morphology of equiaxed grains[J]. Metall. Mater. Trans., 2009, 40B: 289 | [66] | Kumar A, Zalo?nik M, Combeau H.Prediction of equiaxed grain structure and macrosegregation in an industrial steel ingot: Comparison with experiment[J]. Int. J. Adv. Eng. Sci. Appl. Mathemat., 2010, 2: 140 | [67] | Combeau H, Kumar A, Zaloznik M, et al.Macrosegregation prediction in a 65 ton steel ingot [A]. 1st International Conference on Ingot Casting, Rolling and Forging[C]. Brüssel-Saal, 2012 | [68] | Li W S, Shen H F, Liu B C.Numerical simulation of macrosegregation in steel ingots using a two-phase model[J]. Int. J. Min. Metall. Mater., 2012, 19: 787 | [69] | Kang J, Zhang C, Wang T, et al.Numerical simulation of the macrostructure evolution of a heavy steel ingot[J]. Mater. Sci. Technol., 2017, 33: 574 | [70] | Duan Z H, Shen H F, Liu B C.A numerical study of the effect of multiple pouring on macrosegregation in a 438-ton steel ingot[J]. Acta. Metall. Sin.(Engl. Lett.), 2015, 28: 1123 | [71] | Liu D R, Kang X H, Fu P X, et al.Modeling of macrosegregation in steel ingot: Influence of mold shape and melt superheat[J]. Kovove Mater., 2011, 49: 143 | [72] | Liu D R, Kang X H, Sang B G, et al.Numerical study of macrosegregation formation of ingot cast in normal sand mold and water-cooled sand mold[J]. Acta Metall. Sin.(Engl. Lett.), 2011, 24: 54 | [73] | Cao Y F, Chen Y, Li D Z.Formation mechanism of channel segregation in carbon steels by inclusion flotation: X-ray microtomography characterization and multi-phase flow modeling[J]. Acta Mater., 2016, 107: 325 | [74] | Li J, Wu M, Hao J, et al.Simulation of channel segregation using a two-phase columnar solidification Model-Part I: Model description and verification[J]. Comput. Mater. Sci., 2012, 55: 407 | [75] | Li J, Wu M, Hao J, et al.Simulation of channel segregation using a two-phase columnar solidification model-Part II: Mechanism and parameter study[J]. Comput. Mater. Sci., 2012, 55: 419 | [76] | Wu M H, Ludwig A.A three-phase model for mixed columnar-equiaxed solidification[J]. Metall. Mater. Trans., 2006, 37A: 1613 | [77] | Ahmadein M, Wu M, Ludwig A.Analysis of macrosegregation formation and columnar-to-equiaxed transition during solidification of Al-4wt.% Cu ingot using a 5-phase model[J]. J. Cryst. Growth, 2015, 417: 65 | [78] | Wu M H, Ludwig A, Kharicha A.Simulation of as-cast steel ingots[J]. Steel Res. Int., 2017, 89: 1700037 | [79] | Wu M, Li J, Ludwig A, et al.Modeling diffusion-governed solidification of ternary alloys-Part 2: Macroscopic transport phenomena and macrosegregation[J]. Comput. Mater. Sci., 2014, 92: 267 | [80] | Wu M, Ludwig A, Kharicha A.A four phase model for the macrosegregation and shrinkage cavity during solidification of steel ingot[J]. Appl. Math. Modell., 2017, 41: 102 | [81] | Ge H H, Li J, Han X J, et al.Dendritic model for macrosegregation prediction of large scale castings[J]. J. Mater. Process. Technol., 2016, 227: 308 | [82] | Ge H H, Ren F L, Li J, et al.Modelling of ingot size effects on macrosegregation in steel castings[J]. J. Mater. Process. Technol., 2018, 252: 362 | [83] | Ge H H, Ren F L, Li J, et al.Four-phase dendritic model for the prediction of macrosegregation, shrinkage cavity, and porosity in a 55-ton ingot[J]. Metall. Mater. Trans., 2017, 48A: 1139 | [84] | Li J, Ge H H, Wu M H, et al.A columnar & non-globular equiaxed mixed three-phase model based on thermosolutal convection and grain movement[J]. Acta Metall. Sin., 2016, 52: 1096(李军, 葛鸿浩, Wu M H等. 基于热溶质对流及晶粒运动的柱状晶-非球状等轴晶混合三相模型[J]. 金属学报, 2016, 52: 1096) | [85] | Kurz W, Giovanola B, Trivedi R.Theory of microstructural development during rapid solidification[J]. Acta Metall., 1986, 34: 823 | [86] | Li W S, Shen H F, Liu B C.Application of macro segregation mathematical models to large steel ingots[J]. Heavy Cast. Forg., 2012, (6): 38(李文胜, 沈厚发, 柳百成. 宏观偏析数学模型在大型钢锭中的应用[J]. 大型铸锻件, 2012, (6): 38) | [87] | Ludwig A, Wu M H, Kharicha A.On macrosegregation[J]. Metall. Mater. Trans., 2015, 46A: 4854 | [88] | Li J, Wang J G, Ren F L, et al.Experimental and numerical simulation study on layer casting method for composition homogeneity on ingot casting[J]. Acta Metall. Sin., 2018, 54: 118(李军, 王军格, 任凤丽等. 基于成分均匀化的层状铸造方法的实验与模拟研究[J]. 金属学报, 2018, 54: 118) | [89] | Ren F L, Wang J G, Ge H H, et al.A homogeneous billet layer casting fabrication method[J]. Metall. Mater. Trans., 2017, 48A: 4453 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|