| Fe3O4颗粒对硼酸铝晶须增强铝复合材料热膨胀行为的影响 |
| 李 刚 孙 跃 费维栋 |
| 哈尔滨工业大学材料科学与工程学院; 哈尔滨 150001 |
|
| Effect of Fe3O4 Particles on Thermal Expansion Behavior of Al 18B4O33 Whisker Reinforced Aluminum Composite |
| LI Gang; SUN Yue; FEI Weidong |
| School of Materials Science and Engineering; Harbin Institute of Technology; Harbin 150001 |
引用本文:
李刚; 孙跃; 费维栋 . Fe3O4颗粒对硼酸铝晶须增强铝复合材料热膨胀行为的影响[J]. 金属学报, 2006, 42(1): 83-86 .
,
,
.
Effect of Fe3O4 Particles on Thermal Expansion Behavior of Al 18B4O33 Whisker Reinforced Aluminum Composite[J]. Acta Metall Sin, 2006, 42(1): 83-86 .
[1]Arsenault R J,Taya M.Acta Metall,1987;35:651 [2]Arsenault R J,Wu S B.Mater Sci Eng,1987;96:77 [3]Fei W D,Hu M,Yao C K.Mater Chem Phys,2003;77:882 [4]Fei W D,Chu W G,Yang W,Liu Q Y,Yao C K.MaterSci Technol,2000;16:431 [5]Fei W D,Liu Q Y,Liang N G,Yao C K.Mater Sci Technol,2001;17:912 [6]Li G,Sun Y,Fei W D.Mater Lett,2003;57:3217 [7]Levy D,Artioli G,Dapiaggi M.J Solid State Chem,2004;177:1713 [8]Wang L D,Fei W D,Jiang L S,Yao C K.J Mater Sci Lett,2002;21:737 [9]Kim C T,Lee J K,Plichta M R.Metall Trans,1990;21A:673 [10]Maeda K,Wakashima K,Ono M.Scr Mater,1997;36:335 [11]Samara G A,Giardini A A.Phys Rev,1969;186:577 [12]Govindarajan R,Carmichael C M,Schloessin H H.Phys Earth Plan Int,1982;29:108 [13]Jiang S T,Li W.Magnetic Physics of Condensed State(2nd,ed).Beijing:Science Press,2005:55(姜寿亭,李卫.凝聚态磁性物理(第二版).北京:科学出版社,2005:55) [14]Chaianni A,Yokoya T,Morimoto T,Takahashi T,Todo S.J Electron Spectros Relat Phenom,1996;78:99 [15]Li Y R,Yun Z Z.An Introduction to Electronic Materials.Beijing:Tsinghua University Press,2001:329(李言荣,恽正中.电子材料导论.北京:清华大学出版社,2001:329) [16]Fei W D,Wang L D.Mater Chem Phys,2004;85:450 |
|