| 一步电沉积法制备超疏水Cu网及其耐腐蚀和油水分离性能 |
赵婷婷, 康志新( ), 马夏雨 |
| 华南理工大学机械与汽车工程学院 国家金属材料近净成形工程技术研究中心 广东省金属新材料制备与成形重点实验室 广州 510640 |
|
| Fabricating Superhydrophobic Copper Meshes by One-Step Electrodeposition Method and Its Anti-Corrosion and Oil-Water Separation Abilities |
Tingting ZHAO, Zhixin KANG( ), Xiayu MA |
| Guangdong Key Laboratory for Advanced Metallic Materials Processing, National Engineering Research Center of Near-Net-Shape Forming for Metallic Materials, School of Mechanical and Automotive Engineering, South China University of Technology, Guangzhou 510640, China |
引用本文:
赵婷婷, 康志新, 马夏雨. 一步电沉积法制备超疏水Cu网及其耐腐蚀和油水分离性能[J]. 金属学报, 2018, 54(1): 109-117.
Tingting ZHAO,
Zhixin KANG,
Xiayu MA.
Fabricating Superhydrophobic Copper Meshes by One-Step Electrodeposition Method and Its Anti-Corrosion and Oil-Water Separation Abilities[J]. Acta Metall Sin, 2018, 54(1): 109-117.
| [1] | Liu Y, Zhang K T, Yao W G, et al.A facile electrodeposition process for the fabrication of superhydrophobic and superoleophilic copper mesh for efficient oil-water separation[J]. Ind. Eng. Chem. Res., 2016, 55: 2704 | | [2] | Neinhuis C, Barthlott W.Characterization and distribution of water-repellent, self-cleaning plant surfaces[J]. Ann. Bot., 1997, 79: 667 | | [3] | Barthlott W, Neinhuis C.Purity of the sacred lotus, or escape from contamination in biological surfaces[J]. Planta, 1997, 202: 1 | | [4] | Liu Q, Chen D X, Kang Z X.One-step electrodeposition process to fabricate corrosion-resistant superhydrophobic surface on magnesium alloy[J]. ACS Appl. Mater. Interfaces, 2015, 7: 1859 | | [5] | Kang Z X, Guo M J.Fabrication of superhydrophobic Ti surface by thermal oxidation and its anticorrosion property[J]. Acta Metall. Sin., 2013, 49: 629(康志新, 郭明杰. 热氧化法制备超疏水Ti表面及其耐腐蚀性[J]. 金属学报, 2013, 49: 629) | | [6] | Liu C S, Su F H, Liang J Z, et al.Facile fabrication of superhydrophobic cerium coating with micro-nano flower-like structure and excellent corrosion resistance[J]. Surf. Coat. Technol., 2014, 258: 580 | | [7] | Wenzel R N.Resistance of solid surfaces to wetting by water[J]. Ind. Eng. Chem., 1936, 28: 988 | | [8] | Yan L, Li J, Li W J, et al.A photo-induced ZnO coated mesh for on-demand oil/water separation based on switchable wettability[J]. Mater. Lett., 2016, 163: 247 | | [9] | Luo Z Y, Chen K X, Wang J H, et al.Hierarchical nanoparticle-induced superhydrophilic and under-water superoleophobic Cu foam with ultrahigh water permeability for effective oil/water separation[J]. J. Mater. Chem., 2016, 4A: 10566 | | [10] | Wang F J, Lei S, Xu Y, et al.Green approach to the fabrication of superhydrophobic mesh surface for oil/water separation[J]. ChemPhysChem, 2015, 16: 2237 | | [11] | Kong L H, Chen X H, Yu L G, et al.Superhydrophobic cuprous oxide nanostructures on phosphor-copper meshes and their oil-water separation and oil spill cleanup[J]. ACS Appl. Mater. Interfaces, 2015, 7: 2616 | | [12] | Shinde S L, Nanda K K.Facile synthesis of large area porous Cu2O as super hydrophobic yellow-red phosphors[J]. RSC Adv., 2012, 2: 3647 | | [13] | Yin S H, Wu D X, Yang J, et al.Fabrication and surface characterization of biomimic superhydrophobic copper surface by solution-immersion and self-assembly[J]. Appl. Surf. Sci., 2011, 257: 8481 | | [14] | Fan Y H, Chen Z J, Liang J, et al.Preparation of superhydrophobic films on copper substrate for corrosion protection[J]. Surf. Coat. Technol., 2014, 244: 1 | | [15] | Ou J F, Hu W H, Liu S, et al.Superoleophobic textured copper surfaces fabricated by chemical etching/oxidation and surface fluorination[J]. ACS Appl. Mater. Interfaces, 2013, 5: 10035 | | [16] | Qing Y Q, Yang C N, Zhao Q Q, et al.Simple fabrication of superhydrophobic/superoleophobic surfaces on copper substrate by two-step method[J]. J. Alloys Compd., 2017, 695: 1878 | | [17] | Lv Y.Electrodeposited patterning organic luminescent films and their applications for display devices [D]. Changchun: Jilin University, 2013(吕营. 电沉积图案化有机发光薄膜及其在显示器件中的应用 [D]. 长春: 吉林大学, 2013) | | [18] | Hong B.Study on texture and internal stress of electrodeposited copper film [D]. Shanghai: Shanghai Jiao Tong University, 2008(洪波. 电沉积铜薄膜中织构与内应力的研究 [D]. 上海: 上海交通大学, 2008) | | [19] | She Z X, Li Q, Wang Z W, et al.Highly anticorrosion, selfcleaning superhydrophobic Ni- Co surface fabricated on AZ91D magnesium alloy[J]. Surf. Coat. Technol., 2014, 251: 7 | | [20] | Zhang X F, Chen R J, Hu J M.Superhydrophobic surface constructed on electrodeposited silica films by two-step method for corrosion protection of mild steel[J]. Corros. Sci., 2016, 104: 336 | | [21] | Chen Z, Hao L M, Chen C L.A fast electrodeposition method for fabrication of lanthanum superhydrophobic surface with hierarchical micro-nanostructures[J]. Colloids Surf., 2012, 401A: 1 | | [22] | Xi J M, Feng L, Jiang L.A general approach for fabrication of superhydrophobic and superamphiphobic surfaces[J]. Appl. Phys. Lett., 2008, 92: 053102 | | [23] | Cassie A B D, Baxter S. Wettability of porous surfaces[J]. Trans. Faraday. Soc., 1944, 40: 546 | | [24] | Chen Z, Hao L M, Chen C L.Simultaneous fabrication of superhydrophobic coatings on cathodic and anodic copper surfaces with Micro/nano- structures[J]. ECS Electrochem. Lett., 2012, 1: D21 | | [25] | Wang S, Feng L, Jiang L.One-step solution-immersion process for the fabrication of stable bionic superhydrophobic surfaces[J]. Adv. Mater., 2006, 18: 767 | | [26] | Zhao T T, Kang Z X.Simultaneously fabricating multifunctional superhydrophobic/superoleophilic coatings by one-step electrodeposition method on cathodic and anodic magnesium surfaces[J]. J. Electrochem. Soc., 2016, 163: D628 | | [27] | Chen Z, Hao L M, Chen A Q, et al.A rapid one-step process for fabrication of superhydrophobic surface by electrodeposition method[J]. Electrochim. Acta, 2012, 59: 168 | | [28] | Crick C R, Gibbins J A, Parkin I P.Superhydrophobic polymer-coated copper-mesh; membranes for highly efficient oil-water separation[J]. J. Mater. Chem., 2013, 1A: 5943 |
|
|