| 热处理对钛合金表面激光原位合成高铌Ti-Al金属间化合物涂层高温抗氧化行为的影响 |
刘洪喜( ),李正学,张晓伟,谭军,蒋业华 |
| 昆明理工大学材料科学与工程学院 昆明 650093 |
|
| Effect of Heat Treatment on High-Temperature Oxidation Resistance of High Niobium Ti-Al Intermetallic Coating Fabricated by Laser In Situ Synthesis on Titanium Alloy |
Hongxi LIU( ),Zhengxue LI,Xiaowei ZHANG,Jun TAN,Yehua JIANG |
| School of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093, China |
引用本文:
刘洪喜,李正学,张晓伟,谭军,蒋业华. 热处理对钛合金表面激光原位合成高铌Ti-Al金属间化合物涂层高温抗氧化行为的影响[J]. 金属学报, 2017, 53(2): 201-210.
Hongxi LIU,
Zhengxue LI,
Xiaowei ZHANG,
Jun TAN,
Yehua JIANG.
Effect of Heat Treatment on High-Temperature Oxidation Resistance of High Niobium Ti-Al Intermetallic Coating Fabricated by Laser In Situ Synthesis on Titanium Alloy[J]. Acta Metall Sin, 2017, 53(2): 201-210.
| [1] | Das B, Roy S, Rai R N, et al.Development of an in-situ synthesized multi-component reinforced Al-4.5%Cu-TiC metal matrix composite by FAS technique——Optimization of process parameters[J]. Eng. Sci. Technol., Int. J., 2016, 19: 279 | | [2] | Chen H, Zhou H M, Zou Y.Synthesis of ultrafine crystal/nanocrystalline TiAl-based alloy by in situ sintering[J]. Rare Met. Mater. Eng., 2015, 44: 2387 | | [3] | Meng J S, Ji Z S.Microstructure and technology research of in-situ synthesis TiN-TiB2/Ni composite coating by argon arc cladding[J]. Phys. Procedia, 2013, 50: 253 | | [4] | Liu K, Li Y J, Wang J, et al.Effect of high dilution on the in situ synthesis of Ni-Zr/Zr-Si(B, C) reinforced composite coating on zirconium alloy substrate by laser cladding[J]. Mater. Des., 2015, 87: 66 | | [5] | Liu H X, Zhang X W, Jiang Y H, et al.Microstructure and high temperature oxidation resistance of in-situ synthesized TiN/Ti3Al intermetallic composite coatings on Ti6Al4V alloy by laser cladding process[J]. J. Alloys Compd., 2016, 670: 268 | | [6] | Fu Y, Zhang X C, Sui J F, et al.Microstructure and wear resistance of one-step in-situ synthesized TiN/Al composite coatings on Ti6Al4V alloy by a laser nitriding process[J]. Opt. Laser Technol., 2015, 67: 78 | | [7] | Weng F, Chen C Z, Yu H J, et al.Research status of laser cladding on titanium and its alloys: A review[J]. Mater. Des., 2014, 58: 412 | | [8] | Wang Y, Yu H J, Chen C Z, et al.Review of the biocompatibility of micro-arc oxidation coated titanium alloys[J]. Mater. Des., 2015, 85: 640 | | [9] | Zhang Q, Chen J, Tan H, et al.Influence of solution treatment on microstructure evolution of TC21 titanium alloy with near equiaxed β grains fabricated by laser additive manufacture[J]. J. Alloys Compd., 2016, 666: 380 | | [10] | Hounkpati V, Fréour S, Gloaguen D, et al.In situ neutron measurements and modelling of the intergranular strains in the near-β titanium alloy Ti-β21S[J]. Acta Mater., 2016, 109: 341 | | [11] | Riedl H, Koller C M, Munnik F, et al.Influence of oxygen impurities on growth morphology, structure and mechanical properties of Ti-Al-N thin films[J]. Thin Solid Films, 2016, 603: 39 | | [12] | Cui H Z, Ma L, Cao L L, et al.Effect of NiAl content on phases and microstructures of TiC-TiB2-NiAl composites fabricated by reaction synthesis[J]. Trans. Nonferrous Met. Soc. China, 2014, 24: 346 | | [13] | Sina H, Surreddi K B, Iyengar S.Phase evolution during the reactive sintering of ternary Al-Ni-Ti powder compacts[J]. J. Alloys Compd., 2016, 661: 294 | | [14] | Chen L, Yang Y, Wu M J, et al.Correlation between arc evaporation of Ti-Al-N coatings and corresponding Ti0.50Al0.50 target types[J]. Surf. Coat. Technol., 2015, 275: 309 | | [15] | Wang T T, Wang C S, Sun W, et al.Microstructure evolution and mechanical properties of GH984G alloy with different Ti/Al ratios during long-term thermal exposure[J]. Mater. Des., 2014, 62: 225 | | [16] | Sun Y B, Vajpai S K, Ameyama K, et al.Fabrication of multilayered Ti-Al intermetallics by spark plasma sintering[J]. J. Alloys Compd., 2014, 585: 734 | | [17] | Shi Z W, Wei H, Zhang H Y, et al.Nanotwinned Ti(O, C) induced by oriented attachment in a hot-pressed Nb-Ti-Al alloy[J]. Acta Mater., 2016, 105: 114 | | [18] | Shi Z W, Wei H, Zhang H Y, et al.Investigation of a hot-pressed Nb-Ti-Al alloy: Mechanical alloying, microstructure and mechanical property[J]. Mater. Sci. Eng., 2016, A651: 869 | | [19] | Farooq M U, Khalid F A, Zaigham H, et al.Superelastic behaviour of Ti-Nb-Al ternary shape memory alloys for biomedical applications[J]. Mater. Lett., 2014, 121: 58 | | [20] | Kenel C, Leinenbach C.Influence of Nb and Mo on microstructure formation of rapidly solidified ternary Ti-Al-(Nb, Mo) alloys[J]. Intermetallics, 2016, 69: 82 | | [21] | Ding X F.Effect of microstructures on mechanical properties for Ti-Al-Nb ternary alloys [D].[D] Dalian: Dalian University of Technology, 2005 | | [21] | (丁晓菲. Ti-Al-Nb三元系中的合金组织对性能的影响 [D][D]. 大连: 大连理工大学, 2005) | | [22] | Witusiewicz V T, Bondar A A, Hecht U, et al.The Al-B-Nb-Ti system: IV. Experimental study and thermodynamic re-evaluation of the binary Al-Nb and ternary Al-Nb-Ti systems[J]. J. Alloys Compd., 2009, 472: 133 | | [23] | Shen Y, Ding X F, Wang F G, et al.High-temperature oxidation resistance of high-Nb TiAl-based alloy[J]. J. Chin. Soc. Corros. Protec., 2004, 24: 203 | | [23] | (沈勇, 丁晓非, 王富岗等. 高铌TiAl基合金高温抗氧化性能研究[J]. 中国腐蚀与防护学报, 2004, 24: 203) | | [24] | Wang X J, Chang H W, Lei M K.Thermodynamic aspects of oxidation for Nb alloying γ-TiAl intermetallic compounds[J]. Acta Metall. Sin., 2001, 37: 810 | | [24] | (王兴军, 常海威, 雷明凯. Nb合金化γ-TiAl的氧化热力学理论分析[J]. 金属学报, 2001, 37: 810) | | [25] | Burks N,Meyer G H, translated by Zhao G T, Zhao K Q. Introduction to High Temperature Oxidation of Metals [M]. Beijing: Metallurgical Industry Press, 1989: 45 | | [25] | (Burks N, Meyer G H 著, 赵公台, 赵克清译. 金属高温氧化导论 [M]. 北京: 冶金工业出版社, 1989: 45) | | [26] | Stroosnijder M F, Zheng N, Quadakkers W J, et al.The effect of niobium ion implantation on the oxidation behavior of a γ-TiAl-based intermetallic[J]. Oxid. Met., 1996, 46: 19 | | [27] | Liang Y J, Che Y C.Handbook of Thermodynamic Data of Inorganic Materials [M]. Shenyang: Northeastern University Press, 1993: 17 | | [27] | (梁英教, 车荫昌. 无机物热力学数据手册 [M]. 沈阳: 东北大学出版社, 1993: 17) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|