| TiAl预合金粉末热等静压致密化机理及热处理对微观组织的影响* |
王刚1,徐磊2,崔玉友2( ),杨锐2 |
1 营口理工学院机电系, 营口 115003 2 中国科学院金属研究所, 沈阳 110016 |
|
| DENSIFICATION MECHANISM OF TiAl PRE-ALLOY POWDERS CONSOLIDATED BY HOT ISOSTATIC PRESSING AND EFFECTS OF HEAT TREATMENTON THE MICROSTRUCTURE OF TiAl POWDER COMPACTS |
Gang WANG1,Lei XU2,Yuyou CUI2( ),Rui YANG2 |
1 Yingkou Institute of Technology, Yingkou 115003, China 2 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |
引用本文:
王刚,徐磊,崔玉友,杨锐. TiAl预合金粉末热等静压致密化机理及热处理对微观组织的影响*[J]. 金属学报, 2016, 52(9): 1079-1088.
Gang WANG,
Lei XU,
Yuyou CUI,
Rui YANG.
DENSIFICATION MECHANISM OF TiAl PRE-ALLOY POWDERS CONSOLIDATED BY HOT ISOSTATIC PRESSING AND EFFECTS OF HEAT TREATMENTON THE MICROSTRUCTURE OF TiAl POWDER COMPACTS[J]. Acta Metall Sin, 2016, 52(9): 1079-1088.
| [1] | Schmoelzer T, Liss K D, Kirchlechner C, Mayer S, Stark A, Peel M, Clemens H.Intermetallics, 2013; 39: 25 | | [2] | Gupta R K, Pant B, Sinha P P.Trans Indian Inst Met, 2014; 67: 143 | | [3] | Wang H, Zhou M X, Wu B H, Li X Q.Aeronaut Manuf Tech, 2015; (22): 47 | | [3] | (王辉, 周明星, 吴宝海, 李小强. 航空制造技术, 2015; (22): 47) | | [4] | Gussone J, Hagedorn Y C, Gherekhloo H, Kasperovich G, Merzouk T, Hausmann J.Intermetallics, 2015; 66: 133 | | [5] | Wang J W, Wang Y, Liu Y, Li J B, He L Z, Zhang C.Intermetallics, 2015; 64: 70 | | [6] | Wang S R, Guo P Q, Yang L Y.J Mater Process Technol, 2008; 204: 492 | | [7] | Imayev V, Oleneva T, Imayev R, Christ H J, Fecht H J.Intermetallics, 2012; 26: 91 | | [8] | Kong F T, Xiao S L, Chen Y Y, Li B H.Rare Met Mater Eng, 2009; 38: 25 | | [8] | (孔凡涛, 肖树龙, 陈玉勇, 李宝辉. 稀有金属材料与工程, 2009; 38: 25) | | [9] | Schwaighofer E, Clemens H, Mayer S, Lindemann J, Klose J, Smarsly W, Güther V.Intermetallics, 2014; 44: 128 | | [10] | Wang G, Zheng Z, Chang L T, Xu L, Cui Y Y, Yang R.Acta Metall Sin, 2011; 47: 1263 | | [10] | (王刚, 郑卓, 常立涛, 徐磊, 崔玉友, 杨锐. 金属学报, 2011; 47: 1263) | | [11] | Jabbar H, Couret A, Durand L, Monchoux J P. J Alloys Compd, 2011; 509: 9826 | | [12] | Guyon J, Hazotte A, Monchoux J P, Bouzy E.Intermetallics, 2013; 34: 94 | | [13] | Nishida M, Morizono Y, Kai T, Sugimoto J, Chiba A, Kumagae R.Mater Trans JIM, 1997; 38: 334 | | [14] | Choi B W, Deng Y G, McCullough C, Paden B, Mehrabian R.Acta Metall Mater, 1990; 38: 2225 | | [15] | Chai L H.PhD Dissertation,Harbin Institute of Technology, 2010 | | [15] | (柴丽华. 哈尔滨工业大学博士学位论文, 2010) | | [16] | Habel U, McTiernan B J.Intermetallics, 2004; 12: 63 | | [17] | Hao Y L, Yang R, Cui Y Y, Li D.Acta Mater, 2000; 48: 1313 | | [18] | Schlesinger M E, Okamoto H, Gokhale A B, Abbaschian R.J Phase Equilib, 1993; 14: 502 | | [19] | Dong L M, Cui Y Y, Yang R, Wang F H.Acta Metall Sin, 2004; 40: 383 | | [19] | (董利民, 崔玉友, 杨锐, 王福会. 金属学报, 2004; 40: 383) | | [20] | Zhou L Z, Guo J T, Xiao X, Lupinc V, Maldini M.Acta Metall Sin, 2002; 38: 1175 | | [20] | (周兰章, 郭建亭, 肖旋, Lupinc V, Maldini M. 金属学报, 2002; 38: 1175) | | [21] | Adams A G, Rahaman M N, Dutton R E.Mater Sci Eng, 2008; A477: 137 | | [22] | Zhang X D, Dean T A, Loretto M H.Acta Metall Mater, 1994; 42: 2035 | | [23] | Dey S R, Hazotte A, Bouzy E.Intermetallics, 2009; 17: 1052 | | [24] | Denquin A, Naka S.Acta Mater, 1996; 44: 343 | | [25] | Schaeffer R J, Janowski G M.Acta Metall Mater, 1992; 40: 1645 | | [26] | Huang P Y. Powder Metallurgy.Beijing: Metallurgy Industry Press, 1997: 287 | | [26] | (黄培云. 粉末冶金原理. 北京: 冶金工业出版社, 1997: 287) | | [27] | Berteaux O, Popoff F, Thomas M.Metall Mater Trans, 2008; 39A: 2281 | | [28] | Ramanujan R V.Int Mater Rev, 2000; 45: 217 |
|
|