| TA1/X65复合板焊接工艺及焊缝组织和性能研究* |
毕宗岳1,2( ),杨军1,2,刘海璋1,2,张万鹏1,2,杨耀彬1,2,田磊1,2,黄晓江1,2 |
1 国家石油天然气管材工程技术研究中心, 宝鸡 721008。 2 宝鸡石油钢管有限责任公司钢管研究院, 宝鸡 721008 |
|
| INVESTIGATION ON THE WELDING PROCESS AND MICROSTRUCTURE AND MECHANICAL PROPERTY OF BUTT JOINTS OF TA1/X65 CLAD PLATES |
Zongyue BI1,2( ),Jun YANG1,2,Haizhang LIU1,2,Wanpeng ZHANG1,2,Yaobin YANG1,2,Lei TIAN1,2,Xiaojiang HUANG1,2 |
1 National Engineering Technology Research Center for Petroleum and Natural Gas Tubular Goods, Baoji 721008, China. 2 Steel Pipe Research Institute of Baoji Petroleum Steel Pipe Co., Ltd., Baoji 721008, China |
引用本文:
毕宗岳,杨军,刘海璋,张万鹏,杨耀彬,田磊,黄晓江. TA1/X65复合板焊接工艺及焊缝组织和性能研究*[J]. 金属学报, 2016, 52(8): 1017-1024.
Zongyue BI,
Jun YANG,
Haizhang LIU,
Wanpeng ZHANG,
Yaobin YANG,
Lei TIAN,
Xiaojiang HUANG.
INVESTIGATION ON THE WELDING PROCESS AND MICROSTRUCTURE AND MECHANICAL PROPERTY OF BUTT JOINTS OF TA1/X65 CLAD PLATES[J]. Acta Metall Sin, 2016, 52(8): 1017-1024.
| [1] | Zhang X Y, Zhao Y Q, Bai C G.Titanium Alloys and Their Applications .Beijing: Chemical Industry Press, 2005: 287 | | [1] | (张喜燕, 赵永庆, 白晨光. 钛合金及应用. 北京: 化学工业出版社, 2005: 287) | | [2] | Yuan X J, Sheng G M, Qin B.Mater Charact, 2008; 59: 930 | | [3] | Li G Q.Welded Pipe Tube, 2011; 34(11): 39 | | [3] | (李国庆. 焊管, 2011; 34(11): 39) | | [4] | Xu G Z.Welded Pipe Tube, 2009; 32(11): 70 | | [4] | (许贵芝. 焊管, 2009; 32(11): 70) | | [5] | Yang K, Wang Y J, Yun H T, Bai Y, Fu L.Welded Pipe Tube, 2015; 38(7): 6 | | [5] | (杨凯, 王永军, 云海涛, 白颖, 傅莉. 焊管, 2015; 38(7): 6 ) | | [6] | Sheng C C, Master Thesis Jiangsu University of Science and Technology, Zhenjiang, 2008 | | [6] | (盛长城. 江苏科技大学硕士学位论文, 镇江, 2008) | | [7] | Li P, Li J L, Xiong J T, Zhang F S.J Aeronaut Mater, 2010; 30(5): 25 | | [7] | (李鹏, 李京龙, 熊江涛, 张赋升. 航空材料学报, 2010; 30(5): 25) | | [8] | Liu P, Lu M, Ji X W, Huang Q, Dai R X.Ordnance Mater Sci Eng, 2011; 34(3): 14 | | [8] | (刘鹏, 陆明, 冀鑫炜, 黄钦, 戴汝迅. 兵器材料科学与工程, 2011; 34(3): 14) | | [9] | Yan W, Master Thesis Northeastern University Shenyang, 2006 | | [9] | (闫伟. 东北大学硕士学位论文, 沈阳, 2006) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|