| DD9单晶高温合金拉伸性能各向异性 |
王效光,李嘉荣( ),喻健,刘世忠,史振学,岳晓岱 |
|
| TENSILE ANISOTROPY OF SINGLE CRYSTAL SUPERALLOY DD9 |
Xiaoguang WANG,Jiarong LI( ),Jian YU,Shizhong LIU,Zhenxue SHI,Xiaodai YUE |
| Science and Technology on Advanced High Temperature Structural Materials Laboratory, Beijing Institute of Aeronautical Materials, Beijing 100095 |
引用本文:
王效光,李嘉荣,喻健,刘世忠,史振学,岳晓岱. DD9单晶高温合金拉伸性能各向异性[J]. 金属学报, 2015, 51(10): 1253-1260.
Xiaoguang WANG,
Jiarong LI,
Jian YU,
Shizhong LIU,
Zhenxue SHI,
Xiaodai YUE.
TENSILE ANISOTROPY OF SINGLE CRYSTAL SUPERALLOY DD9[J]. Acta Metall Sin, 2015, 51(10): 1253-1260.
| [1] | Sato A, Harada H. Scr Mater, 2006; 54: 1679 | | [2] | Cetel A D, Duhl D N. In: Recichman S, Duhl D N, Maurer G, Antolovich S, Lund C eds., Superalloys 1988, Seven Springs, PA: TMS, 1988: 235 | | [3] | Harris K, Erickson G L, Sikkenga S L, Brentnall W D, Aurrecoechea J M, Kubarych K G. In: Antolovich S D, Stusrud R W, MacKay R A, Anton D L, Khan T, Kissinger R D, Klarstrom D L eds., Superalloys 1992, Pennsylvania, PA: TMS, 1992: 567 | | [4] | Ross E W, O'hara K S. In: Kissinger R D, Deye D J, Anton D L, Cetel A D, Nathal M V, Pollock T M, Woodford D A eds., Superalloys 1996, Seven Springs, PA: TMS, 1996: 19 | | [5] | Walston W S, O'hara K S, Ross E W, Pollock T M, Murphy W H. In: Kissinger R D, Deye D J, Anton D L, Cetel A D, Nathal M V, Pollock T M, Woodford D A eds., Superalloys 1996, Seven Springs, PA: TMS, 1996: 27 | | [6] | Seth B B. In: Pollock T M, Kissinger R D, Bowman R R, Green K A, McLean M, Olson S, Schirra J J eds., Superalloys 2000, Seven Springs, PA: TMS, 2000: 3 | | [7] | Shah D M, Duhl D N. In: Gell M, Kortovich C S, Bricknell R H eds., Superalloys 1984, Seven Springs, PA: TMS, 1984: 105 | | [8] | Dalal R P, Thomasc R, Dardi L E. In: Gell M, Kortovich C S, Bricknell R H eds., Superalloys 1984, Seven Springs, PA: TMS, 1984: 185 | | [9] | Liu J L, Jin T, Zhang J H, Hu Z Q. Acta Metall Sin, 2001; 37: 1233 (刘金来, 金 涛, 张静华, 胡壮麒. 金属学报, 2001; 37: 1233) | | [10] | MacKay R A, Maier R D. Metall Mater Trans, 1982; 13A: 1747 | | [11] | Li J R, Shi Z X, Yuan H L, Liu S Z, Zhao J Q, Han M, Liu W W. J Mater Eng, 2008; (12): 6 (李嘉荣, 史振学, 袁海龙, 刘世忠, 赵金乾, 韩 梅, 刘维维. 材料工程, 2008; (12): 6) | | [12] | Li J R, Liu S Z, Shi Z X, Luo Y S, Wang X G. J Iron Steel Res, 2011; 23(suppl 2): 337 (李嘉荣, 刘世忠, 史振学, 骆宇时, 王效光. 钢铁研究学报, 2011; 23(增刊2): 337) | | [13] | Miner R V, Voigt R C, Gayda J, Gabb T P. Metall Mater Trans, 1986; 17A: 491 | | [14] | Wang L N, Liu Y, Yu J J, Xu Y, Sun X F, Guan H R, Hu Z Q. Mater Sci Eng, 2009; A505: 144 | | [15] | Ardakani M G, McLean M, Shollock B A. Acta Mater, 1999; 47: 2593 | | [16] | Milligan W W, Antolovich S D. Metall Mater Trans, 1991; 22A: 2309 | | [17] | Shi Z X, Li J R, Liu S Z, Zhao J Q. J Iron Steel Res Int, 2011; 18: 66 | | [18] | Kakehi K. Metall Mater Trans, 1999; 30A: 1249 | | [19] | Hu H Q. Fundamentals of Metal Solidification. 2nd Ed.,Beijing: China Machine Press, 2000: 142 (胡汉起. 金属凝固原理. 第2版, 北京: 机械工业出版社, 2000: 142) | | [20] | Zhang L F, Yan P, Zhao J C, Zeng Q, Han F K. J Mater Eng, 2011; (6): 67 (张龙飞, 燕 平, 赵京晨, 曾 强, 韩凤奎. 材料工程, 2011; (6): 67) | | [21] | Feng D. Physics of Metals. Beijing: Science Press, 1999: 326 (冯 端. 金属物理学. 北京: 科学出版社, 1999: 326) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|