| 不同热加工工艺对Al-Mg-Si-Cu合金板材力学性能和组织的影响* |
张艳,郭明星( ),邢辉,王斐,汪小锋,张济山,庄林忠 |
| 北京科技大学新金属材料国家重点实验室, 北京 100083 |
|
| INFLUENCE OF DIFFERENT THERMOMECHANICAL PROCESSES ON THE MECHANICAL PROPERTIES AND MICROSTRUCTURE OF Al-Mg-Si-Cu ALLOY SHEETS |
| Yan ZHANG,Mingxing GUO,Hui XING,Fei WANG,Xiaofeng WANG,Jishan ZHANG,Linzhong ZHUANG |
| State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing,Beijing 100083 |
引用本文:
张艳,郭明星,邢辉,王斐,汪小锋,张济山,庄林忠. 不同热加工工艺对Al-Mg-Si-Cu合金板材力学性能和组织的影响*[J]. 金属学报, 2015, 51(12): 1425-1434.
Yan ZHANG,
Mingxing GUO,
Hui XING,
Fei WANG,
Xiaofeng WANG,
Jishan ZHANG,
Linzhong ZHUANG.
INFLUENCE OF DIFFERENT THERMOMECHANICAL PROCESSES ON THE MECHANICAL PROPERTIES AND MICROSTRUCTURE OF Al-Mg-Si-Cu ALLOY SHEETS[J]. Acta Metall Sin, 2015, 51(12): 1425-1434.
| [1] | Yu Z Q, Lin Z Q, Zhao Y X. Mater Des, 2007; 28: 203 | | [2] | Gao Q M, Cao L S, Yu X D. Light Alloy Fabr Technol, 2009; 37: 30 | | [2] | (高琪妹, 曹力生, 于晓丹. 轻合金加工技术, 2009; 37: 30) | | [3] | Engler O, Hirsch J. Mater Sci Forum, 1996; 217: 479 | | [4] | Bennett T A, Petrov R H, Kestens L A I. Scr Mater, 2010; 63: 461 | | [5] | Troeger L P, Starke Jr E A. Mater Sci Eng, 2000; A293: 19 | | [6] | Peng X Y, Guo M X, Wang X F, Cui L, Zhang J S, Zhuang L Z. Acta Metall Sin, 2015; 51: 169 | | [6] | (彭祥阳, 郭明星, 汪小峰, 崔 莉, 张济山, 庄林忠. 金属学报, 2015; 51: 169) | | [7] | Lievers W B, Pilkey A K, Lloyd D J. Mater Sci Eng, 2003; A361: 312 | | [8] | Lankford W T, Snyder S C, Bauscher J A. Trans Am Soc Met, 1950; 42: 1197 | | [9] | Hirofumi I, Takayuki T. Mater Trans, 2007; 48: 2014 | | [10] | Leu D K. Int J Mach Tools Manuf, 1997; 37: 201 | | [11] | Humphreys F J. Acta Metall, 1977; 25: 1323 | | [12] | Orsund R, Nes E. Scr Mater, 1988; 22: 665 | | [13] | Davies R K, Randle V, Marshall G J. Acta Mater, 1998; 46: 6021 | | [14] | Bennett T A, Petrov R H, Kestensv L A I. Scr Mater, 2010; 62: 78 | | [15] | Higginson R L, Aindow M, Bate P S. Mater Sci Eng, 1997; A225: 9 | | [16] | Ito K, Musick R, Lucke K. Acta Metall, 1983; 31: 2137 | | [17] | Jensen D J, Hansen N, Humphreys E J. Acta Metall, 1985; 33: 2155 | | [18] | Hansen N, Jensen D J. Metall Trans, 1986; 17A: 253 | | [19] | Hirsch J, Nes E, Lucke K. Acta Metall, 1987; 35: 427 | | [20] | Kashihara K, Inagaki H. Metall Trans, 2009; 50A: 528 | | [21] | Humphreys F J. Acta Metall, 1977; 25: 1323 | | [22] | Engler O. Mater Sci Technol, 1996; 12: 859 |
|
|