| TiCu/Zn界面反应周期层片结构形成的热力学和动力学研究* |
吴长军1,2, 朱晨露1, 苏旭平1,2( ), 刘亚1,2, 彭浩平3, 王建华1,2 |
1 常州大学材料科学与工程学院, 常州213164 2 江苏省材料表面技术重点实验室, 常州213164 3 常州大学石油工程学院, 常州213164 |
|
| THERMODYNAMICAL AND KINETIC INVESTIGA-TION OF FORMATION OF PERIODIC LAYERED STRUCTURE IN TiCu/Zn INTERFACE REACTION |
WU Changjun1,2, ZHU Chenlu1, SU Xuping1,2( ), LIU Ya1,2, PENG Haoping3, WANG Jianhua1,2 |
1 School of Materials Science and Engineering, Changzhou University, Changzhou 213164 2 Jiangsu Key Laboratory of Materials Surface Technology, Changzhou 213164 3 School of Petroleum Engineering, Changzhou University, Changzhou 213164 |
引用本文:
吴长军, 朱晨露, 苏旭平, 刘亚, 彭浩平, 王建华. TiCu/Zn界面反应周期层片结构形成的热力学和动力学研究*[J]. 金属学报, 2014, 50(8): 930-936.
Changjun WU,
Chenlu ZHU,
Xuping SU,
Ya LIU,
Haoping PENG,
Jianhua WANG.
THERMODYNAMICAL AND KINETIC INVESTIGA-TION OF FORMATION OF PERIODIC LAYERED STRUCTURE IN TiCu/Zn INTERFACE REACTION[J]. Acta Metall Sin, 2014, 50(8): 930-936.
| [1] |
He M, Su X P, Yin F C, Wang J H, Li Z. Scr Mater, 2008; 59: 411
|
| [2] |
Osinski K, Vriend A W, Bastin F, Loo F. Z Metallkd, 1982; 73: 258
|
| [3] |
Su X P, Liu C, Yin F C, Wang J H. Scr Mater, 2010; 62: 485
|
| [4] |
Andersson J,Höglund L,Jönsson B,Agren J,Purdy G. Fundamentals and Applications of Ternary Diffusion. New York: Pergamon Press, 1990: 153
|
| [5] |
Dunaev S F, Zverkov S A. J Less Common Met, 1989; 153: 143
|
| [6] |
Schiepers R C J, Van Beek J A, Van Loo F J J, De With G. J Eur Ceram Soc, 1993; 11: 211
|
| [7] |
Rijnders M R, Kodentsov A A, Van Beek J A, Van Den Akker J, Van Loo F J J. Solid State Ionics, 1997; 95: 51
|
| [8] |
Gutman I, Klinger L, Gotman I, Shapiro M. Scr Mater, 2001; 45: 363
|
| [9] |
Rijnders M R, Van Beek J A, Kodentsov A A, Van Loo F J J. Z Metallkd, 1996; 87: 732
|
| [10] |
Effenberg G, Ilyenko S. Non-Ferrous Metal Systems. Berlin: Springer Berlin Heidelberg, 2007: 451
|
| [11] |
Chen Y C, Zhang X F, Han L, Du Z W. Mater Lett, 2012; 76: 151
|
| [12] |
Kodentsov A A, Rijnders M R, Van Loo F J J. Acta Mater, 1998; 46: 6521
|
| [13] |
Osinski K. PhD Dissertation, Eindhoven University of Technology, 1983
|
| [14] |
Kao C R, Chang Y A. Acta Metall Mater, 1993; 41: 3463
|
| [15] |
Kirkaldy J S, Young D J. Diffusion in the Condensed State. London: Institute of Metals London, 1987: 387
|
| [16] |
Kumar K C H, Ansara I, Wollants P, Delaey L. Z Metallkd, 1996; 87: 666
|
| [17] |
Gierlotka W, Chen S W. J Mater Res, 2008; 23: 258
|
| [18] |
Chen X A, Jeitschko W, Danebrock M E, Evers C B H, Wagner K. J Solid State Chem, 1995; 118: 219
|
| [19] |
Soares D, Vilarinho C, Castro F. Scand J Metall, 2001; 30: 254
|
| [20] |
Heine W, Zweicker U. Z Metallkd, 1962; 53: 386
|
| [21] |
Chen Y C, Zhang X F, Ren Y K, Han L, Lin D Y, Wang Q P. Intermetallics, 2013; 36: 8
|
| [22] |
Zhang X, Chena Y, Fan X, Hao G. Procedia Eng, 2012; 27: 1707
|
| [23] |
Zhang X F. Master Thesis, Shandong University of Science and Technology, Jinan, 2011
|
| [23] |
(张喜凤. 山东科技大学硕士学位论文, 济南, 2011)
|
| [24] |
Chen Y C, Xu J, Fan X H, Zhang X F, Han L, Lin D Y, Li Q H, Uher C. Intermetallics, 2009; 17: 920
|
| [25] |
Chen Y C, Qi L, Zhang Y G, Chen C Q. J Beijing Univ (Nat Sci), 2006; 42: 168
|
| [25] |
(陈永翀, 其 鲁, 张永刚, 陈昌麒. 北京大学学报(自然科学版), 2006; 42: 168)
|
| [26] |
Chen Y C, Li Z H, Qi L, Zhang Y G, Chen C Q. Acta Metall Sin, 2006; 42: 225
|
| [26] |
(陈永翀, 黎振华, 其 鲁, 张永刚, 陈昌麒. 金属学报, 2006; 42: 225)
|
| [27] |
Chen Y C, Qi L, Zhang Y G, Chen C Q. Acta Metall Sin, 2005; 41: 235
|
| [27] |
(陈永翀, 其 鲁, 张永刚, 陈昌麒. 金属学报, 2005; 41: 235)
|
| [28] |
Chen Y C, Zhang Y G, Chen C Q. Mater Sci Eng, 2003; A362: 135
|
| [29] |
Su X P, Li Z, Yin F C, He Y H, Pan S W. Acta Metall Sin, 2008; 44: 718
|
| [29] |
(苏旭平, 李 智, 尹付成, 贺跃辉, 潘世文. 金属学报, 2008; 44: 718)
|
| [30] |
Doi K, Ono S, Ohtani H, Hasebe M. J Phase Equilib Diff, 2006; 27: 63
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|