一种细晶铸造镍基高温合金的组织与力学性能* |
杨金侠( ), 孙元, 金涛, 孙晓峰, 胡壮麒 |
中国科学院金属研究所, 沈阳 110016 |
|
MICROSTRUCTURE AND MECHANICAL PROPERTIES OF A Ni-BASED SUPERALLOY WITH REFINED GRAINS |
YANG Jinxia( ), SUN Yuan, JIN Tao, SUN Xiaofeng, HU Zhuangqi |
Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
杨金侠, 孙元, 金涛, 孙晓峰, 胡壮麒. 一种细晶铸造镍基高温合金的组织与力学性能*[J]. 金属学报, 2014, 50(7): 839-844.
Jinxia YANG,
Yuan SUN,
Tao JIN,
Xiaofeng SUN,
Zhuangqi HU.
MICROSTRUCTURE AND MECHANICAL PROPERTIES OF A Ni-BASED SUPERALLOY WITH REFINED GRAINS[J]. Acta Metall Sin, 2014, 50(7): 839-844.
[1] |
Ewing B A, Green K A. In: Gell M, Kortovin C S, Bricknell R H, Kent W B, Radavich J F eds., Superalloys, Champion: The Metallergical Society of AIME, 1984: 33
|
[2] |
McClean M. Mater Sci Technol, 1988; 4: 205
|
[3] |
Bouse G K, Behrend M R. In: Loria E ed., Mechanical Properties of Microcast-X Alloy 718 Fine Grain Investment Castings, Superalloy 718-Metallurgy and Applications, Warrendale, PA: The Metallurgical Society, 1989: 319
|
[4] |
Prichard P D, Dalal R P. In: Antolovich S D, Stusrud R W, Mackay R A, Anton D L, Khan T, Kissinger R D, Klarstrom D L eds., Superalloys, Champion: The Metallurgical Society of AIME, 1992: 205
|
[5] |
Liu L, Zhen B L, Banerlly A, Relf W. Scr Metall Mater, 1994; 30: 593
|
[6] |
Liu L, Huang T, Xiong Y, Yang A, Zhao Z, Zhang R, Li J. Mater Sci Eng, 2005; A394: 1
|
[7] |
Xiong Y, Yang A, Guo Y, Liu W, Liu L. Sci Technol Adv Mater, 2001; 2: 13
|
[8] |
Xiong Y H, Liu W, Yang A M, Zhang R, Liu L. Acta Metall Sin, 1999; 35: 689
|
[8] |
(熊玉华, 柳 伟, 杨爱民, 张 蓉, 刘 林. 金属学报, 1999; 35: 689)
|
[9] |
Ma Y, Sun J, Xie X, Hu Y, Zhao J, Yan P. J Mater Sci Technol, 2003; 137: 35
|
[10] |
Zhang B, Cui J, Liu G. Mater Sci Eng, 2003; A355: 325
|
[11] |
Paul P C, Nasar S A. Introduction of Electromagnetic Fields. New York: McGraw-Hill, 1987: 306
|
[12] |
Li T G, Cao Z Q, Jin J Z, Zhang Z F. Mater Trans, 2001; 42: 281
|
[13] |
Cao Z Q, Jia F, Zhang X G, Hao H, Jin J Z. Mater Sci Eng, 2002; A327: 133
|
[14] |
Zhou J, Xie F X, Wu X Q, Zhang J. Foundry, 2009; 58: 678
|
[14] |
(周俊, 谢发勤, 吴向清, 张军. 铸造, 2009; 58: 678)
|
[15] |
Zheng J B, Ding J, Guo Y P, Liu L, Liu W, Li X J. Acta Metall Sin, 1998; 34: 362
|
[15] |
(郑建邦, 丁 洁, 郭益平, 刘 林, 柳 伟, 李行建. 金属学报, 1998; 34: 362)
|
[16] |
Zhao H T, Shi C X. Acta Metall Sin, 1981; 17: 118
|
[16] |
(赵慧田, 师昌绪. 金属学报, 1981; 17: 118)
|
[17] |
EI-Bagoury N, Nofal A. Mater Sci Eng, 2010; A527: 7793
|
[18] |
Hu H Q. Principles of Metal Solidification. Beijing: Machinery Industry Press, 1991: 48
|
[18] |
(胡汉起. 金属凝固原理. 北京: 机械工业出版社, 1991: 48)
|
[19] |
Herlach D M. Mater Sci Eng, 1994; R12: 177
|
[20] |
Peng Z F. Acta Metall Sin, 2002; 23: 135
|
[20] |
(彭志方. 金属学报, 2002; 23: 135)
|
[21] |
Yin F S. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2003
|
[21] |
(殷凤仕. 中国科学院金属研究所博士学位论文, 沈阳, 2003)
|
[22] |
Jin W Z, Li J, Li T J, Yin G M. Rare Met Mater Eng, 2008; 37: 1012
|
[22] |
(金文中, 李 军, 李廷举, 殷国茂. 稀有金属材料与工程, 2008; 37: 1012)
|
[23] |
Qiu H, Qian H C, Samir H A, Wu S M. Foundry Technol, 2004; 25: 265
|
[23] |
(邱 华, 钱翰城, Samir H A, 吴仕明. 铸造技术, 2004; 25: 265)
|
[24] |
Nilsson J O, Thorvaldsson T. Fatigue Fract Eng Mater Struct, 1985; 8: 4
|
[25] |
Leverant G R. Trans Metall Soc AIME, 1969: 245
|
[26] |
Liu F X, Yuan W M, Tang X, Yang A D. Acta Metall Sin, 1995; 31(Suppl): S739
|
[26] |
(刘发信, 袁文明, 汤 鑫, 杨爱德. 金属学报, 1995; 31(增刊): S739)
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|