| Al-Mg-Si合金时效早期显微组织演变及其对强化的影响* |
汪波, 王晓姣, 宋辉, 严菊杰, 邱涛, 刘文庆, 李慧( ) |
| 上海大学微结构重点实验室, 上海 200444 |
|
| STRENGTHENING EFFECTS OF MICROSTRUCTURE EVOLUTION DURING EARLY AGEING PROCESS IN Al-Mg-Si ALLOY |
WANG Bo, WANG Xiaojiao, SONG Hui, YAN Jujie, QIU Tao, LIU Wenqing, LI Hui( ) |
| Key Laboratory for Microstructures, Shanghai University, Shanghai 200444 |
引用本文:
汪波, 王晓姣, 宋辉, 严菊杰, 邱涛, 刘文庆, 李慧. Al-Mg-Si合金时效早期显微组织演变及其对强化的影响*[J]. 金属学报, 2014, 50(6): 685-690.
Bo WANG,
Xiaojiao WANG,
Hui SONG,
Jujie YAN,
Tao QIU,
Wenqing LIU,
Hui LI.
STRENGTHENING EFFECTS OF MICROSTRUCTURE EVOLUTION DURING EARLY AGEING PROCESS IN Al-Mg-Si ALLOY[J]. Acta Metall Sin, 2014, 50(6): 685-690.
| [1] |
Shang B C, Yin Z M, Wang G, Liu B, Huang Z Q. Mater Des, 2011; 32: 3818
|
| [2] |
Marioara C D, Andersen S J, Jansen J, Zandbergen H W. Acta Mater, 2003; 51: 789
|
| [3] |
Jin M, Li J, Shao G J. J Alloys Compd, 2007; 437: 146
|
| [4] |
Wang H, Sun Y Z, Zhang W G, Bi A T, Kang Y L, Li W. At Energy Sci Technol, 1999; 33: 134
|
| [4] |
(王 辉, 孙源珍, 张伟国, 毕安泰, 康亚伦, 李 伟. 原子能科学与技术, 1999; 33: 134)
|
| [5] |
Yang W C, Wang M P, Sheng X F, Zhang Q, Wang Z A. Acta Metall Sin, 2010; 46: 1481
|
| [5] |
(杨文超, 汪明朴, 盛晓菲, 张 茜, 王正安. 金属学报, 2010; 46: 1481)
|
| [6] |
Yassar R S, Field D P, Weiland H. Scr Mater, 2005; 53: 299
|
| [7] |
Edwards G A, Stiller K, Dunlop G L, Couper M J. Acta Metall, 1998; 46: 3893
|
| [8] |
Starink M J, Cao L F, Rometsch P A. Acta Mater, 2012; 60: 4194
|
| [9] |
Torsæter M, Hasting H S, Lefebvre W, Marioara C D, Walmsley J C, Andersen S J, Holmestad R. J Appl Phys, 2010; 108: 1
|
| [10] |
Murayama M, Hono K, Saga M, Kikuchi M. Mater Sci Eng, 1988; A250: 127
|
| [11] |
Murayama M, Hono K. Acta Mater, 1999; 47: 1537
|
| [12] |
Zandbergen H W, Andersen S J, Jansen J. Science, 1997; 277: 1221
|
| [13] |
Marioara C D, Nordmark H, Andersen S J, Holmestad R. J Mater Sci, 2006; 41: 471
|
| [14] |
Hasting H S, Froseth A G, Andersen S J, Vissers R, Walmsley J C, Marioara C D. J Appl Phys, 2009; 106: 2
|
| [15] |
Marioara C D, Andersen S J, Zandbergen H W, Holmestad R. Metall Trans, 2005; 36A: 691
|
| [16] |
Serizawa A, Sato T, Poole W J. Philos Mag Lett, 2010; 90: 279
|
| [17] |
Buha J, Lumley R N, Crosky A G,Hono K. Acta Mater, 2007; 55: 3015
|
| [18] |
Esmaeili S, Lloyd D J, Poole W J. Acta Mater, 2003; 51: 3467
|
| [19] |
Pogatscher S, Antrekowitsch H, Leitner H, Ebner T, Uggowitzer P J. Acta Mater, 2011; 59: 3352
|
| [20] |
Sha G, Ringer S P. Ultramicroscopy, 2009; 109: 508
|
| [21] |
Abid T, Boubertakh A, Hamamda S. J Alloys Compd, 2010; 490: 166
|
| [22] |
Rometsch P A, Cao L F, Xiong X F, Muddle B C. Ultramicroscopy, 2011; 111: 690
|
| [23] |
Pogatscher S, Antrekowitsch H, Leitner H, Poschmann D, Zhang Z L, Uggowitzer P J. Acta Mater, 2012; 60: 4496
|
| [24] |
Sha G, Mller H, Stumpf W E, Xia J H, Govender G, Ringer S P. Acta Mater, 2012; 60: 692
|
| [25] |
Rinderer B, Couper M, Xiong X, Gao S, Nie J F. Mater Sci Forum, 2010; 654-656: 590
|
| [26] |
Chang C S T, Wieler I, Wanderka N, Banhart J. Ultramicroscopy, 2009; 109: 585
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|