| NZ30K镁合金时效析出动力学与强化模型的研究* |
王小娜1, 韩利战1,2, 顾剑锋1,2( ) |
1 上海交通大学材料科学与工程学院, 上海 200240 2 上海市激光制造与材料改性重点实验室, 上海 200240 |
|
| PRECIPITATION KINETICS AND YIELD STRENGTH MODEL FOR NZ30K-Mg ALLOY |
WANG Xiaona1, HAN Lizhan1,2, GU Jianfeng1,2( ) |
1 School of Materials Science and Engineering, Shanghai Jiaotong University, Shanghai 200240 2 Shanghai Key Laboratory of Materials Laser Processing and Modification, Shanghai 200240 |
引用本文:
王小娜, 韩利战, 顾剑锋. NZ30K镁合金时效析出动力学与强化模型的研究*[J]. 金属学报, 2014, 50(3): 355-360.
Xiaona WANG,
Lizhan HAN,
Jianfeng GU.
PRECIPITATION KINETICS AND YIELD STRENGTH MODEL FOR NZ30K-Mg ALLOY[J]. Acta Metall Sin, 2014, 50(3): 355-360.
| [1] |
Li J H, Jie W Q, Yang G Y. Trans Nonferrous Met Soc China, 2008; 18: S27
|
| [2] |
Li J H, Sha G, Jie W Q, Ringer S P. Mater Sci Eng, 2012; A538: 272
|
| [3] |
Antion C, Donnadieu P, Perrard F, Deschamps A, Tassin C, Pisch A. Acta Mater, 2003; 51: 5335
|
| [4] |
Hantzsche K, Bohlen J, Wendt J, Kainer K U, Yi S B, Letzig D. Scr Mater, 2010; 63: 725
|
| [5] |
Mishra R K, Gupta A K, Rao P R, Sachdev A K, Kumar A M, Luo A A. Scr Mater, 2008; 59: 562
|
| [6] |
Nuttall P A, Pike T J, Noble B. Metallography, 1980; 13: 3
|
| [7] |
Fu P H, Peng L M, Jiang H Y, Chang J W, Zhai C Q. Mater Sci Eng, 2008; A486: 183
|
| [8] |
Gill L R, Lorimer G W, Lyon P. Adv Eng Mater, 2007; 9: 784
|
| [9] |
Ma L, Mishra R K, Balogh M P, Peng L M, Luo A A, Sachdev A K, Ding W J. Mater Sci Eng, 2012; A543: 12
|
| [10] |
Nie J F, Muddle B C. Acta Mater, 2000; 48: 1691
|
| [11] |
Nie J F, Ohishi K, Gao X, Hono K. Acta Mater, 2008; 56: 6061
|
| [12] |
Pike T J, Noble B. J Less-common Met, 1973; 30: 63
|
| [13] |
Esmaeili S, Lloyd D J. Acta Mater, 2005; 53: 5257
|
| [14] |
Esmaeili S, Lloyd D J, Poole W J. Acta Mater, 2003; 51: 2243
|
| [15] |
Esmaeili S, Lloyd D J, Poole W J. Acta Mater, 2003; 51: 3467
|
| [16] |
Liu G, Ding X D, Sun J, Chen K H. Chin J Nonferrous Met, 2001; 11: 337
|
| [16] |
(刘 刚, 丁向东, 孙 军, 陈康华. 中国有色金属学报, 2001; 11: 337)
|
| [17] |
Liu G, Zhang G J, Ding X D, Sun J, Chen K H. Rare Met Mater Eng, 2003; 32: 971
|
| [17] |
(刘 刚, 张国君, 丁向东, 孙 军, 陈康华. 稀有金属材料与工程, 2003; 32: 971)
|
| [18] |
Deschamps A, Brechet Y. Acta Mater, 1999; 47: 293
|
| [19] |
Deschamps A, Livet F, Bréchet Y. Acta Mater, 1998; 47: 281
|
| [20] |
Esmaeili S, Vaumousse D, Zandbergen M W, Poole W J, Cerezo A, Lloyd D J. Philos Mag, 2007; 87: 3797
|
| [21] |
Vyazovkin S, Burnham A K, Criado J M, Pérez-Maqueda L A, Popescu C, Sbirrazzuoli N. Thermochim Acta, 2011; 520: 1
|
| [22] |
Burnham A, Dinh L. J Therm Anal Calorim, 2007; 89: 479
|
| [23] |
Friedman H L. J Polym Sci, 1964; 6C: 183
|
| [24] |
Ardell A J. Metall Trans, 1985; 16A: 2131
|
| [25] |
Hutchinson C R, Nie J F, Gorsse S. Metall Mater Trans, 2005; 36A: 2093
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|