    					| 低温挤压Mg-4Zn-2Al-2Sn合金的组织与力学性能研究* | 
  					 
  					  										
						赵东清1,2, 周吉学2, 刘运腾2, 董旭光1, 王晶1, 杨院生1,2( ) | 
					 
															
					1 中国科学院金属研究所, 沈阳110016 2 山东省科学院新材料研究所, 济南250014 | 
					 
										
						 | 
					 
   										
    					| MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Mg-4Zn-2Al-2Sn ALLOYS EXTRUDED AT LOW TEMPERATURES | 
  					 
  					  					  					
						ZHAO Dongqing1,2, ZHOU Jixue2, LIU Yunteng2, DONG Xuguang1, WANG Jing1, YANG Yuansheng1,2( ) | 
					 
															
						1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 2 Institute of New Materials Research, Shandong Academy of Sciences, Jinan 250014 | 
					   
									 
				
				引用本文: 
				
								赵东清, 周吉学, 刘运腾, 董旭光, 王晶, 杨院生. 低温挤压Mg-4Zn-2Al-2Sn合金的组织与力学性能研究*[J]. 金属学报, 2014, 50(1): 41-48.	
																												 																				Dongqing ZHAO,
																								Jixue ZHOU,
																								Yunteng LIU,
																								Xuguang DONG,
																								Jing WANG,
																												Yuansheng YANG. 
				MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Mg-4Zn-2Al-2Sn ALLOYS EXTRUDED AT LOW TEMPERATURES[J]. Acta Metall Sin, 2014, 50(1): 41-48.	                                                        				  
				
				
					
						
							
								
									
									
									
									
									 
          
          
            
             
			              
            
									            
									                
																																															
																| [1] | 
																 
															     Kashefi N, Mahmudi R.Mater Des, 2012; 39: 200
															     																 | 
																	  
																																
																| [2] | 
																 
															     Song D H, Lee S W, Park Y D, Park Y H, Cho K M, Park I M. Mater Sci Forum, 2007; 539-543: 1790
															     																 | 
																	  
																																
																| [3] | 
																 
															     Chen Z H,Yan H G,Chen J H,Quan Y J,Wang H M,Chen D. Magnesium Alloys. Beijing: Chemical Industry Press, 2004: 202
															     																 | 
																	  
																																
																| [3] | 
																 
															     (陈振华,严红革,陈吉华,全亚杰,王慧敏,陈 鼎. 镁合金. 北京: 化学工业出版社, 2004: 202)
															     																 | 
																	  
																																
																| [4] | 
																 
															     Sasaki T T, Yamamoto K, Honma T, Kamado S, Hono K. Scr Mater, 2008; 59: 1111
															     																 | 
																	  
																																
																| [5] | 
																 
															     Liu C M,Zhu X R,Zhou H T. Magnesium Alloy Phase Diagrams. Nanjing: Southeast University Press, 2006: 49
															     																 | 
																	  
																																
																| [5] | 
																 
															     (刘楚明,朱秀荣,周海涛. 镁合金相图集. 南京: 东南大学出版社, 2006: 49)
															     																 | 
																	  
																																
																| [6] | 
																 
															     Bronfin B, Aghion E, Buch F V, Schumann S, Katzir M. US Pat,7041179B2, 2006
															     																 | 
																	  
																																
																| [7] | 
																 
															     Dong X G, Fu J W, Yang Y S. Acta Metall Sin, 2013; 49: 621
															     																 | 
																	  
																																
																| [7] | 
																 
															     (董旭光, 付俊伟, 杨院生. 金属学报, 2013; 49: 621)
															     																 | 
																	  
																																
																| [8] | 
																 
															     Lim H K, Kim D H, Lee J Y, Kim W T, Kim D H.J Alloys Compd, 2009; 468: 308
															     																 | 
																	  
																																
																| [9] | 
																 
															     Chen J H, Chen Z H, Yan H G, Zhang F Q, Kun L.J Alloys Compd, 2008; 461: 209
															     																 | 
																	  
																																
																| [10] | 
																 
															     Zhao D Q, Dong X G, Zhang X E, Gao A J, Zhou J X, Yang Y S. Mater Sci Forum, 2013; 747-748: 398
															     																 | 
																	  
																																
																| [11] | 
																 
															     Kang D H, Park S S, Kim N J. Mater Sci Eng, 2005; A413-414: 555
															     																 | 
																	  
																																
																| [12] | 
																 
															     Henes S, Gerold V. ZMetallk, 1962; 53: 743
															     																 | 
																	  
																																
																| [13] | 
																 
															     Rabkin E.Scr Mater, 1998; 39: 1631
															     																 | 
																	  
																																
																| [14] | 
																 
															     Li W B, Easterling K E.Acta Metall Mater, 1990; 38: 1045
															     																 | 
																	  
																																
																| [15] | 
																 
															     Mendis C L, Ohishi K, Kawamura Y, Honma T, Kamado S, Hono K.Acta Mater, 2009; 57: 749
															     																 | 
																	  
																																
																| [16] | 
																 
															     Park S S, You B S, Yoon D J.J Mater Process Technol, 2009; 209: 5940
															     																 | 
																	  
																																
																| [17] | 
																 
															     Shahzad M, Wagner L.Mater Sci Eng, 2009; A506: 141
															     																 | 
																	  
																																
																| [18] | 
																 
															     Yang P, Hu Y S, Cui F E. ChinJ Mater Res, 2004; 18: 52
															     																 | 
																	  
																																
																| [18] | 
																 
															     (杨 平, 胡轶嵩, 崔凤娥. 材料研究学报, 2004; 18: 52)
															     																 | 
																	  
																																
																| [19] | 
																 
															     Park S S, Tang W N, You B S. Mater Lett, 2010; 64: 31
															     																 | 
																	  
																																
																| [20] | 
																 
															     Wang Y N, Huang J C.Acta Mater, 2007; 55: 897
															     																 | 
																	  
																																
																| [21] | 
																 
															     Barnett M R.Scr Mater, 2008; 59: 696
															     																 | 
																	  
																																
																| [22] | 
																 
															     Stanford N, Barnett M R.Mater Sci Eng, 2009; A516: 226
															     																 | 
																	  
																																
																| [23] | 
																 
															     Jain J, Poole W J, Sinclair C W, Gharghouri M A.Scr Mater, 2010; 62: 301
															     																 | 
																	  
																																													 
									             
									           
             
			            			 
			 
             
												
											    	
											        	 | 
											        	Viewed | 
											         
													
											        	 | 
											        	 | 
											         
											      	
												         | 
												        
												        	Full text 
												          	
												         | 
											        	
												        	
												        	 
												        	
												          	 
												          	
												          	
														 | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        
												        	Abstract 
												          	
														 | 
												        
															
															 
															
															
												         | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        Cited  | 
												        
												        	
												         | 
													 
													
												         | 
												         | 
												         | 
													 
													
													    |   | 
													    Shared | 
													       | 
												  	 
												  	
													     | 
													     | 
													     | 
											  		 
											  		
													    |   | 
													    Discussed | 
													       | 
												  	 
											 
											 
             
           
      
									
									
		
									
									
									
									
									
									 | 
								 
							 
						 | 
					 
				 
			
		 |