金属学报  2013, Vol. 49 Issue (8): 959-968    DOI: 10.3724/SP.J.1037.2012.00787
  论文 本期目录 | 过刊浏览 |
添加Sn粉激光焊接钢/铝合金异种金属的显微组织与性能
周惦武,彭艳,徐少华,刘金水
湖南大学汽车车身先进设计制造国家重点实验室, 长沙 410082
MICROSTRUCTURE AND MECHANICAL PROPERTY OF STEEL/Al ALLOY LASER WELDING WITH Sn POWDER ADDITION
ZHOU Dianwu, PENG Yan, XU Shaohua, LIU Jinshui
State Key Laboratory of Advanced Design and Manufacturing for Vehicle Body,Hunan University, Changsha 410082
引用本文:

周惦武,彭艳,徐少华,刘金水. 添加Sn粉激光焊接钢/铝合金异种金属的显微组织与性能[J]. 金属学报, 2013, 49(8): 959-968.
ZHOU Dianwu, PENG Yan, XU Shaohua, LIU Jinshui. MICROSTRUCTURE AND MECHANICAL PROPERTY OF STEEL/Al ALLOY LASER WELDING WITH Sn POWDER ADDITION[J]. Acta Metall Sin, 2013, 49(8): 959-968.

全文: PDF(1313 KB)  
摘要: 

采用光纤激光器对厚度为1.4 mm的DC56D+ZF镀锌钢和厚度为1.2 mm的6016铝合金平板试件进行了添加Sn粉的激光搭接焊实验,利用卧式金相显微镜、扫描电镜、X射线衍射和微机控制电子万能试验机等研究了添加Sn粉前后焊接接头各区域的金相组织、断口形貌、界面元素分布、主要物相与接头力学性能, 采用基于密度泛函理论的第一性原理方法,计算了添加Sn后新形成物相FeSn和FeAl化合物的模量和热力学性能. 结果表明, 在激光功率为2000 W,焊接速度45 mm/s, 离焦量+2.0 mm, Ar气为保护气体且流量为15 L/min的条件下,添加Sn粉焊接试样的焊缝表面成形性良好, 焊缝区晶粒细小, 焊接接头的平均剪切强度为62.17 MPa,与没有添加Sn相比, 剪切强度提高1.46倍. 由于细晶强化, 提高熔池金属的流动性,利于钢/铝合金界面结合, 减少Fe--Al金属间化合物层厚度, 新形成的FeSn的金属间化合物具有较好延性,高温下结构稳定, 抑制或减少了Fe--Al脆性金属间化合物的生成, 因而添加Sn粉改善了焊接接头的力学性能.

关键词 : 激光焊接,  钢/铝合金异种金属,  金属间化合物,  添加Sn粉    
Abstract:

The laser welding test with Sn powder addition was carried out on DC56D+ZF galvanized steel with thickness 1.4 mm and 6016 aluminum alloy with thickness 1.2 mm. By using optical microscopy, scanning electron microscopy, X-ray diffraction and tensile test, the microstructure, fracture morphology, interface element distribution, main phase and mechanical properties of joints were studied. Elastic moduli and thermodynamic properties were calculated by using first-principles method based on density functional theory for FeAl and FeSn compounds. The results indicate that the morphology of welding surface can be improved and grain size is fine when the welding power is 2000 W, welding speed is 45 mm/s, the defocus distance is +2.0 mm, and Ar gas acts as the protection gas with flow rate 15 L/min. The average shear strength of the welding sample with Sn powder reaches 62.17 MPa. Compared to that without Sn powder addition, the average shear strength of weld joint increases by 1.46 times. Because of fine-grain strengthening and the improvement of the fluidity of the molten pool metal with Sn addition, it promotes the combination of the steel and aluminum interface and decreases the thickness of the intermetallic layer. FeSn intermetallic compounds has better ductility and is more stable than that of FeAl at high temperature that retard and reduce the generation of Fe-Al intermetallic compound, which can improve the mechanical properties of weld joint with Sn addition.

Key words: laser welding    steel/Al alloy dissimilar metal    intermetallic compounds    Sn powder addition
收稿日期: 2012-12-31     
基金资助:

国家高技术研究发展计划重点项目2012AA111802和湖南大学汽车车身先进设计制造国家重点实验室自主课题项目71075003资助

作者简介: 周惦武, 男, 1971年生, 教授, 博士

[1] Lei Z, Wang X Y, Wang W B, Lin S Y.  Trans China Weld Inst, 2007; 28(11): 65

 (雷振, 王旭友, 王伟波, 林尚杨. 焊接学报, 2007; 28(11): 65)
[2] Torkamany M J, Tahamtan S, Sabbaghzadeh J.  Mater Des, 2010; 31: 458
[3] Zhang Q Y, Liu S Q.  Acta Metall Sin, 1981; 17: 300
 (张启运, 刘淑淇. 金属学报, 1981; 17: 300)
[4] Guo J T, Sun C, Tan M H, Li H, Lai W H.  Acta Metall Sin, 1990; 26: 20
 (郭建亭, 孙超, 谭明晖, 李辉, 赖万慧. 金属学报, 1990; 26: 20)
[5] Zhang Q X.  Rare Met Mater Eng, 1990; 20: 27
 (章桥新. 稀有金属材料与工程, 1990; 20: 27)
[6] Wang L G, Zhang B F, Guan S K, Qi X H, Geng J Y.  Rare Met Mater Eng, 2007; 36: 59
 (王利国, 张保丰, 关绍康, 齐新华, 耿家源. 稀有金属材料与工程, 2007; 36: 59)
[7] Boag A, Hughes A E, Wilson N C, Torpy A, Macrae M C, Glenn A M, Muster T H. Corros Sci, 2009; 51: 1565
[8] Akdeniz M V, Mekhrabov A O.  Acta Mater, 1998; 46: 1185
[9] Mathieu A, Pontevicci S, Viala J C, Cicala E, Matte\"{\i S, Grevey D.Mater Sci Eng, 2006; A435-436: 19
[10] Lin S B, Song J L, Yang C L, Fan C L, Zhang D W.  Mater Des, 2010; 31: 2637
[11] Braun R.  Mater Sci Eng, 2006; A426: 250
[12] Sierra G, Peyre P, Deschaux B F.  Mater Charact, 2008; 59: 1705
[13] Segall M D, Lindan P L D, Probert M J, Pickard C J, Hasnip P J, Clark S J,Payne M C.  J Phys: Condens Matter, 2002; 14: 2717
[14] Marlo M, Milman V.  Phys Rev, 2000; 62B: 2899
[15] White J A, Bird D M.  Phys Rev, 1994; 50B: 4954
[16] Lei Z, Yu N, You A Q, Lin S Y.  Trans China Weld Inst, 2008; 29(6): 21
 (雷振, 于宁, 游爱清, 林尚扬. 焊接学报, 2008; 29(6): 21)
[17] Song J L, Lin S B, Yang C L, Ma G C.  Aeronaut Manuf Technol, 2008; 12: 26
 (宋建岭, 林三宝, 杨春利, 马广超. 航空制造技术, 2008; 12: 26)
[18] Hao Y L, Xu D S, Cui Y Y, Yang R, Li D.  Acta Mater, 1999; 47: 1129
[19] Kobayashi S, Yakou T.  Mater Sci Eng, 2002; A338: 44
[20] Simmons G, Wang H.  Single Crystal Elastic Constants and Calculated Aggregate Properties. Cambridge: MIT Press, 1971: 80
[21] Fu C L, Yoo M H.  Acta Mater, 1992, 40: 703
[22] Kong Y, Hu W Y, Huang Y C, Shu X L.  Rare Met Mater Eng, 2003; 32: 87
 (孔毅, 胡望宇, 黄杨程, 舒小林. 稀有金属材料与工程, 2003; 32: 87)
[23] Mehl M J, Osburn J E, Papaconstantopoulos D A, Klein B M.  Phys Rev,1990; 41B: 10311
[24] Pugh S F.  Philos Mag, 1954; 45: 823
[25] Yu W Y, Wang N, Xiao X B, Tang B Y, Peng L M, Ding W J.  Solid State Sci,2009; 11: 1400
[1] 丁宗业, 胡侨丹, 卢温泉, 李建国. 基于同步辐射X射线成像液/固复层界面氢气泡的形核、生长演变与运动行为的原位研究[J]. 金属学报, 2022, 58(4): 567-580.
[2] 周丽君, 位松, 郭敬东, 孙方远, 王新伟, 唐大伟. 基于飞秒激光时域热反射法的微尺度Cu-Sn金属间化合物热导率研究[J]. 金属学报, 2022, 58(12): 1645-1654.
[3] 宫声凯, 尚勇, 张继, 郭喜平, 林均品, 赵希宏. 我国典型金属间化合物基高温结构材料的研究进展与应用[J]. 金属学报, 2019, 55(9): 1067-1076.
[4] 刘杨,王磊,宋秀,梁涛沙. DD407/IN718高温合金异质焊接接头的组织及高温变形行为[J]. 金属学报, 2019, 55(9): 1221-1230.
[5] 吉华,邓运来,徐红勇,郭伟强,邓建峰,范世通. 焊接线能量对5182-O/HC260YD+Z异种材料CMT搭接接头组织与性能的影响[J]. 金属学报, 2019, 55(3): 376-388.
[6] 陈丽群, 邱正琛, 于涛. Ru对NiAl[100](010)刃型位错电子结构的影响[J]. 金属学报, 2019, 55(2): 223-228.
[7] 曹丽华, 陈胤伯, 史起源, 远杰, 刘志权. 合金元素对中温Sn-Ag-Cu焊料互连组织及剪切强度的影响[J]. 金属学报, 2019, 55(12): 1606-1614.
[8] 何贤美, 童六牛, 高成, 王毅超. Nd含量对磁控溅射Si(111)/Cr/Nd-Co/Cr薄膜结构与磁性的影响[J]. 金属学报, 2019, 55(10): 1349-1358.
[9] 张敏, 慕二龙, 王晓伟, 韩挺, 罗海龙. TA1/Cu/X65复合板焊接接头微观组织及力学性能[J]. 金属学报, 2018, 54(7): 1068-1076.
[10] 康慧君, 李金玲, 王同敏, 郭景杰. 定向凝固Al-Mn-Be合金初生金属间化合物相生长行为及力学性能[J]. 金属学报, 2018, 54(5): 809-823.
[11] 耿林, 吴昊, 崔喜平, 范国华. 基于箔材反应退火合成的TiAl基复合材料板材研究进展[J]. 金属学报, 2018, 54(11): 1625-1636.
[12] 于宣, 张志豪, 谢建新. 不同Ce含量Fe-6.5%Si合金的组织、有序结构和中温拉伸塑性[J]. 金属学报, 2017, 53(8): 927-936.
[13] 赵宁,邓建峰,钟毅,殷录桥. 热迁移下Ni/Sn-xCu/Ni微焊点钎焊界面金属间化合物的演变[J]. 金属学报, 2017, 53(7): 861-868.
[14] 王大伟,修世超. 焊接温度对碳钢/奥氏体不锈钢扩散焊接头界面组织及性能的影响[J]. 金属学报, 2017, 53(5): 567-574.
[15] 张志杰,黄明亮. Cu/Sn-52In/Cu微焊点液-固电迁移行为研究[J]. 金属学报, 2017, 53(5): 592-600.