Please wait a minute...
金属学报  2013, Vol. 49 Issue (7): 845-852    DOI: 10.3724/SP.J.1037.2012.00712
  论文 本期目录 | 过刊浏览 |
GH4169G合金热处理期间的相转变特征与机理分析
田素贵1),王欣1),谢君1),刘臣1),郭忠革),刘姣2),孙文儒2)
1)沈阳工业大学材料科学与工程学院, 沈阳 110870
2)中国科学院金属研究所高温合金研究部, 沈阳 110016
 
CHARACTERISTIC AND MECHANISM OF PHASE TRANSFORMATION OF GH4169G ALLOY DURING HEAT TREATMENT
TIAN Sugui1), WANG Xin1), XIE Jun1), LIU Chen1), GUO Zhongge1),LIU Jiao2), SUN Wenru2)
1)School of Materials Science and Engineering, Shenyang University of Technology, Shenyang 110870
2)Superalloys Division, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
引用本文:

田素贵,王欣,谢君,刘臣,郭忠革,刘姣,孙文儒. GH4169G合金热处理期间的相转变特征与机理分析[J]. 金属学报, 2013, 49(7): 845-852.
TIAN Sugui, WANG Xin, XIE Jun, LIU Chen, GUO Zhongge, LIU Jiao, SUN Wenru. CHARACTERISTIC AND MECHANISM OF PHASE TRANSFORMATION OF GH4169G ALLOY DURING HEAT TREATMENT[J]. Acta Metall Sin, 2013, 49(7): 845-852.

全文: PDF(2881 KB)  
摘要: 

通过组织形态观察和XRD分析, 研究了热处理对GH4169G合金相组成和分布规律的影响.结果表明, 在实验条件下, 合金的组织结构由γ基体、粒状γ′相、圆盘状γ〞相和δ相组成, 且各相之间保持共格界面, 其中,直接时效处理ITF-DA-GH4169G合金由少量γ′相、大量γ〞相和γ基体组成, 而长期时效处理ITF-DA-LTA-GH4169G合金由少量γ′相、大量γ〞相和γ相及针状δ相组成. 时效期间,随着合金中Nb原子扩散进入γ′相, 使γ′相(001)面的Nb和Ni原子沿1/2<110>方向迁移, L12结构的γ′-Ni3Al相可转变成DO22结构的γ〞-Ni3Nb相. 随时效时间延长, γ〞相长大,γ〞相单胞中的平行六面体沿特定晶面发生1/6<112>位移,促使γ〞相转变成DOa结构的δ-Ni3Nb. 其中,γ〞相中的a, b轴与γ基体和γ′相保持共格界面,可使其沿c轴生长成为圆盘状形态; 而δ-Ni3Nb相的{200}δ晶面与γ基体的{111}γ晶面保持共格界面, 是促使δ相沿(100)晶面生长成为针状的主要原因.

关键词 : GH4169G合金,  热处理,  组织结构,  晶格常数,  相转变    
Abstract:

By means of heat treatment at different regimes, microstructure observation and XRD analysis, an investigation has been made into the influence of heat treatment on the phases constitution and distribution regularity of GH4169G alloy. The results show that under the experimental conditions, microstructure of GH4169G alloy consists of γ matrix, particle-like γ′,disc-like γ〞and δ phases, and the coherent interfaces are kept between the phases. Thereinto, microstructure of directional aging treatment ITF-DA-GH4169G alloy consists of a few γ′phase, lots of γ〞 and γ phases, however, long-time aging treatment ITF-DA-LTA-GH4169G consists of a few γ′,lots of γ〞, γ and needle-like δ phases. As the Nb atom diffuses into the lattice of γ′  phase during the aging treatment,γ′ -Ni3Al phase with L12 structure is transformed intoγ〞-Ni3Nb phase with DO22 structure when the Nb and Ni atoms on (001) plane of γ′ phase migrate along 1/2<110> direction. With the growth of γ〞 phase during the long term aging, the given crystal plane in the new parallelepiped migrates along the 1/6<112> direction, which makes the γ〞 phase transform into δ-Ni3Nb phase with DOa structure. Moreover, the γ〞 phase may grow up into the disc-like configuration along the c-axis direction due to the restriction of the a- and b-axis coherent interfaces. And it is a main reason that the δ-Ni3Nb phase grows into needle-like configuration along the (100) plane due to the {200}δ plane ofδ phase keeps coherent interface with {111}γ plane of γ matrix phase.

Key words: GH4169G alloy    heat treatment    microstructure    lattice parameter    phase transformation
收稿日期: 2012-11-29     
基金资助:

国家自然科学基金重点基金项目50634030和国家自然科学基金项目51271125资助

作者简介: 田素贵, 男, 1952年生, 教授

[1] Chen W, Chaturvedi M C.  Mater Sci Eng, 1994; A183: 81

[2] Wang Y, Lin L, Shao W Z, Zhen L, Zhang X M. Trans Mater Heat Treatment, 2007; 28(suppl): 176
(王岩, 林琳, 邵文柱, 甄良, 张新梅. 材料热处理学报, 2007; 28(增刊): 176
[3] Medeiros S C, Prasad Y V R K, Frazier W G, Srinivasan R. Mater Sci Eng, 2003; A193: 198
[4] Rao G A, Kymar M, Srinivas M, Sarma D S. Mater Sci Eng, 2003; A355: 114
[5] Xie X S, Dong J X, Fu S H, Zhang M C. Acta Metall Sin, 2010; 46: 1289
(谢锡善, 董建新, 付书红, 张麦仓. 金属学报, 2010; 46: 1289)
[6] Zhang M Y, Wang Y X, Chen Z, Dong W P, Lai Q B, Zhang L P. Rare Met Mater Eng, 2009; 38: 962
(张明义, 王永欣, 陈铮, 董卫平, 来庆波, 张利鹏. 稀有金属材料与工程, 2009; 38: 962)
[7] Mukherji D, Gilles R, Barbier B, Del D G. Scr Mater, 2003; 48: 333
[8] Ding R G, Rong T S, Knott J F. Mater Sci Technol, 2006; 21: 85
[9] Zhang M Y, Chen Z, Wang Y X, Lu Y L, Zhang J, Fan X L. Acta Metall Sin, 2009; 45: 930
(张明义, 陈铮, 王永欣, 卢艳丽, 张静, 范晓丽. 金属学报, 2009; 45: 930)
[10] Briant C L. Metall Trans, 1988; 19A: 137
[11] Seah M P. Acta Metall, 1980; 28: 955
[12] Liu D, Luo Z J. Rare Met, 2005; 29: 152
(刘东, 罗子健. 稀有金属, 2005; 29: 152)
[13] Xie X S, Dong J X, Fu S H, Zhang M C. Acta Metall Sin, 2010; 46: 1289
(谢锡善, 董建新, 付书红, 张麦仓. 金属学报, 2010; 46: 1289)
[14] Wang Y, Shao W Z, Zhen L. Chin J Nonferrous Met, 2011; 21: 341
(王岩, 邵文柱, 甄良. 中国有色金属学报, 2011; 21: 341)
[15] Hu Z Q, Sun W R, Guo S R, Lu D Z. Chin J Nonferrous Met, 2001; 11: 947
(胡壮麒, 孙文儒, 郭守仁, 卢德忠. 中国有色金属学报, 2001; 11: 947)
[16] Kirman I, Warrington D H. Metall Trans, 1970; 1: 2667
[17] Chaturvedi M C, Han Y F. Met Sci, 1983; 17: 145
[18] V anderschaeve G, Escaig B. Philos Mag, 1983; 48A: 265
[19] Yamakov V, Wolf D, Phillpot S R, Mukherjee A, Gleiter H. Nat Mater, 2004; 3: 43
[20] Van Swygenhoven H, Derlet P M, Froseth A. Nat Mater, 2004; 3: 399
[21] Liao X Z, Zhou F, Lavernia E J, He D W, Zhu Y T. Appl Phys Lett, 2003; 83: 5062
[22] Wang J, Huang H C. Appl Phys Lett, 2004; 85: 5983
[23] Zhen L, Xu T D, Deng Q, Si H, Dong J X. Acta Metall Sin, 2007; 43: 893
(郑磊, 徐庭栋, 邓群, 司红, 董建新. 金属学报, 2007; 43: 893)
[24] Song H W, Guo S R, Lu D Z, Xu Y, Wang Y L, Hu Z Q. Chin J Mater Res, 2000; 14: 183
(宋洪伟, 郭守仁, 卢德忠, 徐岩, 王玉兰, 胡壮麒. 材料研究学报, 2000; 14: 183)
[25] Ling B, Zhong B W, Yang Y R, Liang X F, Shen B. J Aeronaut Mater, 1994; 1: 1

(凌斌, 钟炳文, 杨玉荣, 梁学锋, 沈飚. 航空材料学报, 1994; 1: 1)

[1] 王法, 江河, 董建新. 高合金化GH4151合金复杂析出相演变行为[J]. 金属学报, 2023, 59(6): 787-796.
[2] 张东阳, 张钧, 李述军, 任德春, 马英杰, 杨锐. 热处理对选区激光熔化Ti55531合金多孔材料力学性能的影响[J]. 金属学报, 2023, 59(5): 647-656.
[3] 杨累, 赵帆, 姜磊, 谢建新. 机器学习辅助2000 MPa级弹簧钢成分和热处理工艺开发[J]. 金属学报, 2023, 59(11): 1499-1512.
[4] 孙腾腾, 王洪泽, 吴一, 汪明亮, 王浩伟. 原位自生2%TiB2 颗粒对2024Al增材制造合金组织和力学性能的影响[J]. 金属学报, 2023, 59(1): 169-179.
[5] 韩林至, 牟娟, 周永康, 朱正旺, 张海峰. 热处理温度对Ti0.5Zr1.5NbTa0.5Sn0.2 高熵合金组织结构与力学性能的影响[J]. 金属学报, 2022, 58(9): 1159-1168.
[6] 李钊, 江河, 王涛, 付书红, 张勇. GH2909低膨胀高温合金热处理中的组织演变行为[J]. 金属学报, 2022, 58(9): 1179-1188.
[7] 张家榕, 李艳芬, 王光全, 包飞洋, 芮祥, 石全强, 严伟, 单以银, 杨柯. 热处理对一种双峰晶粒结构超低碳9Cr-ODS钢显微组织与力学性能的影响[J]. 金属学报, 2022, 58(5): 623-636.
[8] 曾小勤, 王杰, 应韬, 丁文江. 镁及其合金导热研究进展[J]. 金属学报, 2022, 58(4): 400-411.
[9] 袁波, 郭明星, 韩少杰, 张济山, 庄林忠. 添加3%Zn对Al-Mg-Si-Cu合金非等温时效析出行为的影响[J]. 金属学报, 2022, 58(3): 345-354.
[10] 陈润, 王帅, 安琦, 张芮, 刘文齐, 黄陆军, 耿林. 热挤压与热处理对网状TiBw/TC18复合材料组织及性能的影响[J]. 金属学报, 2022, 58(11): 1478-1488.
[11] 王迪, 黄锦辉, 谭超林, 杨永强. 激光增材制造过程中循环热输入对组织和性能的影响[J]. 金属学报, 2022, 58(10): 1221-1235.
[12] 王文权, 王苏煜, 陈飞, 张新戈, 徐宇欣. 选区激光熔化成形TiN/Inconel 718复合材料的组织和力学性能[J]. 金属学报, 2021, 57(8): 1017-1026.
[13] 王文权, 杜明, 张新戈, 耿铭章. H13钢表面电火花沉积WC-Ni基金属陶瓷涂层微观组织及摩擦磨损性能[J]. 金属学报, 2021, 57(8): 1048-1056.
[14] 王悦, 王继杰, 张昊, 赵泓博, 倪丁瑞, 肖伯律, 马宗义. 热处理对激光选区熔化AlSi10Mg合金显微组织及力学性能的影响[J]. 金属学报, 2021, 57(5): 613-622.
[15] 张少华, 谢光, 董加胜, 楼琅洪. 单晶高温合金共晶溶解行为的差热分析[J]. 金属学报, 2021, 57(12): 1559-1566.