Ti-6Al-4V激光冲击强化及其微结构响应分析 |
罗新民1), 赵广志1), 张永康2), 陈康敏1, 3), 罗开玉2), 任旭东2) |
1) 江苏大学材料科学与工程学院, 镇江 212013
2) 江苏大学机械工程学院, 镇江 212013
3) 江苏大学分析测试中心, 镇江 212013 |
|
LASER SHOCK PROCESSING OF Ti-6Al-4V AND ANALYSIS OF ITS MICROSTRUCTURE RESPONSE |
LUO Xinmin1), ZHAO Guangzhi1), ZHANG Yongkang2), CHEN Kangmin1, 3), LUO Kaiyu2), REN Xudong2) |
1) School of Material Science and Engineering, Jiangsu University, Zhenjiang 212013
2) School of Mechanical Engineering, Jiangsu University, Zhenjiang 212013
3) Analysis and Test Center, Jiangsu University, Zhenjiang 212013 |
引用本文:
罗新民 赵广志 张永康 陈康敏 罗开玉 任旭东. Ti-6Al-4V激光冲击强化及其微结构响应分析[J]. 金属学报, 2012, 48(9): 1116-1122.
,
,
,
,
,
,
,
.
LASER SHOCK PROCESSING OF Ti-6Al-4V AND ANALYSIS OF ITS MICROSTRUCTURE RESPONSE[J]. Acta Metall Sin, 2012, 48(9): 1116-1122.
[1] Zhong M L, Fan P X. Chin J Lasers, 2011; 38: 0601001–1
(钟敏霖, 范培迅. 中国激光, 2011; 38: 0601001-1)
[2] Zhong M L, Liu W J. Chin J Lasers, 2008; 35: 1653
(钟敏霖, 刘文今. 中国激光, 2008; 35: 1653)
[3] Zhou J Z, Fan Y J, Huang S, Ruan H Y, Zhu W, Wei D H, Wang C D, Chen H S. Chin J Lasers, 2011; 38: 0601003–1
(周建忠, 樊玉杰, 黄 舒, 阮鸿雁, 朱 伟, 卫登辉, 王呈栋, 陈寒松. 中国激光, 2011; 38: 0601003-1)
[4] Huang Y G, Liu S B. Chin J Lasers, 2009; 36: 3133
(黄永光, 刘世炳. 中国激光, 2009; 36: 3133)
[5] Luo X M, Zhang J W, Ma H, Zhang Y K, Chen K M, Ren X D, Luo K Y. Acta Optica Sin, 2011; 31: 714002–1
(罗新民, 张静文, 马辉, 张永康, 陈康敏, 任旭东, 罗开玉. 光学学报, 2011; 31: 714002-1)
[6] Xu H Y, Zou S K, Che Z G, Cao Z W. Chin J Lasers, 2011; 38: 0303002–1
(许海鹰, 邹世坤, 车志刚, 曹子文. 中国激光, 2011; 38: 0303002--)
[7] Zhang Y K, Zhou L C, Ren X D. J Jiangsu Univ (Nat Sci Ed), 2009; 30(1): 10
(张永康, 周立春, 任旭东. 江苏大学学报(自然科学版), 2009; 30(1): 10)
[8] Trdan U, Grum J, Hill M R. Mater Sci Forum, 2011; 681: 480
[9] Zou S K, Gong S L, Guo E M, Li B. Chin J Lasers, 2011; 38: 0601009–1
(邹世坤, 巩水利, 郭恩明, 李斌. 中国激光, 2011; 38: 0601009-1)
[10] Ren X D, Zhang Y K, Zhou J Z, Ma Z. J Huazhong Univ Sci Technol (Nat Sci Ed), 2007; 35(3): 150
(任旭东, 张永康, 周建忠, 马壮. 华中科技大学学报(自然科学版), 2007; 35(3): 150)
[11] Hu Y X, Yao Z Q. Acta Metall Sin (Engl Lett), 2008; 21: 125
[12] Li P, Li S X, Wang Z G. Prog Mater Sci, 2011; 56: 328
[13] Zhang Y K, Pei X, Chen J F, Gu Y Y, Ren A G, You J. Acta Optica Sin, 2010; 30: 2613
(张永康, 裴旭, 陈菊芳, 顾永玉, 任爱国, 尤建. 光学学报, 2010; 30: 2613)
[14] Guo N G, Luo X M, Hua Y Q. Mater Rev, 2006; 20(6): 10
(郭乃国, 罗新民, 花银群. 材料导报, 2006; 20(6): 10)
[15] Zhang W, Sui M L, Zhou Y Z, He G H, Guo J D, Li D X. Acta Metall Sin, 2003; 39: 1009
(张伟, 隋曼龄, 周亦胄, 何冠虎, 郭敬东, 李斗星. 金属学报, 2003; 39: 1009)
[16] Luo X M, Zhang Y K, Chen K M, Ren X D. In: Slabe J M ed., Proc 8th Int Conf zIndustral Tools and Material Processing Technologies{, Ljubljana: Ljubljana University, 2011: 223
[17] Luo X M, Zhao G Z, Yuan C Z, Zhang Y K, Chen K M. In: BobWed., Proc ICMTMA 2011. Los Alamitos: IEEE Computer Society, 2011: 556
[18] Rozmus G M. Acta Phys Polonica, 2010; 117A: 808
[19] Christoph L, Manfred P. Titanium and Titanium Alloys: Fundamentals and Applications. Weinheim: WILEY– VCH Verlag GmbH & Co. KGaA, 2003: 1
[20] Tao C H, Liu Q Q, Cao C X, Zhang W F. Failure and Prevention of Aeronautical Titanium Alloy. Beijing: National Defense Industry Press, 2002: 11
(陶春虎, 刘庆瑔,曹春晓, 张卫方. 航空用钛合金的失效及其预防. 北京: 国防工业出版社, 2002: 11)
[21] Zou S K, Cao ZW, Liu F J. Chin J Lasers, 2007; 34(s1): 4
(邹世坤, 曹子文, 刘方军. 中国激光, 2007; 34(s1): 4)
[22] Zhang Y K, Ye Y X. Laser Optoelectronics Prog, 2009; (9): 32
(张永康, 叶云霞. 激光与光电子学进展, 2009; (9): 32)
[23] Gu Y Y, Zhang Y K, Zhang X Q, Shi J G. Acta Phys Sin. 2006; 55: 5885
(顾永玉, 张永康, 张兴权, 史建国. 物理学报, 2006; 55: 5885)
[24] Qu H, Liu W D, Liu Z L. Acta Metall Sin, 2006; 42: 374
(屈华, 刘伟东, 刘志林. 金属学报, 2006; 42: 374)
[25] Zhou Z M. Dislocation Configuration Evolution. Shenyang: Northeastern University Press, 2003: 60
(周志敏. 位错组态演化. 沈阳: 东北大学出版社, 2003: 60)
[26] Hu G X, Qian M G. Metallurgy. Shanghai: Shanghai Science and Technology Press, 1980: 63
(胡赓祥, 钱苗根. 金属学. 上海: 上海科学技术出版社, 1980: 63)
[27] Franek A, Kalus R, Kratochvil J. Philos Mag, 1991; 64A: 497
[28] L¨utjering G, Williams J C. Titanium. 2nd Ed., Heidelberg: Springer Verlag, 2007: 97
[29] Smallman R E, Ngan A H W. Physical Metallurgy and Advanced Materials. 7th Ed., Burlington: Elsevier Ltd. 2007: 92
[30] Luo X M, Ma H, Zhang J W, Zhang Y K. Mater Rev, 2010; 20(3): 11
(罗新民, 马辉, 张静文, 张永康. 材料导报, 2010; 20(3): 11)
[31] Shao J L, Qin C S, Wang P, Zhang G C, He A M. Acta Mech Solid Sin, 2009; 30: 226
(邵建立, 秦承森, 王裴, 张广财, 何安民. 固体力学学报, 2009; 30: 226)
[32] Luo G. Master thesis, Nanjing Aeronautic and Astronautic University, 2010
(罗刚. 南京航空航天大学硕士学位论文, 2010) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|