| 样品取向对AZ31镁合金静态再结晶行为的影响 |
| 黄洪涛1,Godfrey Andrew1,刘伟1,唐瑞鹤1,刘庆2 |
1.清华大学材料科学与工程系, 北京 100084
2.重庆大学材料科学与工程学院, 重庆 400044 |
|
| EFFECT OF SAMPLE ORIENTATION ON STATIC RECRYSTALLIZATION OF AZ31 MAGNESIUM ALLOY |
| HUANG Hongtao1, Godfrey Andrew1, LIU Wei1, TANG Ruihe1, LIU Qing2 |
1.Department of Materials Science and Engineering, Tsinghua University, Beijing 100084
2.School of Materials Science and Engineering, Chongqing University, Chongqing 400044 |
引用本文:
黄洪涛 Godfrey Andrew 刘伟 唐瑞鹤 刘庆. 样品取向对AZ31镁合金静态再结晶行为的影响[J]. 金属学报, 2012, 48(8): 915-921.
,
,
,
,
.
EFFECT OF SAMPLE ORIENTATION ON STATIC RECRYSTALLIZATION OF AZ31 MAGNESIUM ALLOY[J]. Acta Metall Sin, 2012, 48(8): 915-921.
| [1] Beer A G, Barnett M R. Mater Sci Eng, 2008; A485: 318[2] Robson J D, Henry D T, Davis B. Acta Mater, 2009; 57: 2739[3] Li X, Yang P, Wang L N, Meng L, Cui F. Mater Sci Eng, 2009; A517: 160[4] Yi S B, Schestakow I, Zaefferer S. Mater Sci Eng, 2009; A516: 58[5] Jager A, Lukac P V. Gartnerova V, Haloda J, Dopita M. Mater Sci Eng, 2006; A432: 20[6] Huang X S, Suzuki K, Chino Y. J Alloys Compd, 2011; 509: 4854[7] Mackenzie L W F, Pekguleryuz M. Mater Sci Eng, 2008; A480: 189[8] Liu Q. Acta Metall Sin, 2010; 46: 1458(刘庆. 金属学报, 2010; 46: 1458)[9] Perez–Prado M T, Ruano O A. Scr Mater, 2002; 46: 149[10] Perez–Prado M T, Ruano O A. Scr Mater, 2003; 48: 59[11] Jiang J, Godfrey A, Liu W, Liu Q. Mater Sci Eng, 2008; A483: 576[12] Humphreys F J, Hatherly M. Recrystallization and Related Annealing Phenomena. 2Ed., Oxford: Pergamon Press, 2004: 222[13] Huang H T, Liu W, Godfrey A, Tang R H, Liu Q. Acta Metall Sin, 2012; 48: 357(黄洪涛, 刘伟, Godfrey A, 唐瑞鹤, 刘庆. 金属学报, 2012; 48: 357)[14] Yang X Y, Zhang L. Acta Metall Sin, 2009; 45: 1303(杨续跃, 张雷. 金属学报, 2009; 45: 1303)[15] Wang M Y, Xin R L, Wang B S, Liu Q. Mater Sci Eng, 2011; A528: 2941[16] Brown D W, Agnew S R, Bourke M A M, Holden T M, Vogel S C, Tome C N. Mater Sci Eng, 2005; A399: 1[17] Clausen B , Tom´e C N, Brown D W, Agnew S R. Acta Mater, 2008; 56: 2456[18] Li X, Yang P, Meng L, Cui F E. Acta Metall Sin, 2010;46: 147(李萧, 杨平, 孟利, 崔凤娥. 金属学报, 2010; 46: 147)[19] Al–Samman T, Molodov K D, Molodov D A, Gottstein G, Suwas S. Acta Mater, 2012; 60: 537[20] Galiyev A, Kaibyshev R, Gottstein G. Acta Mater, 2001; 49: 1199[21] Jin Q L, Shim S Y, Lim S G. Scr Mater, 2006; 55: 843[22] Stanford N, Geng J, Chun Y B, Davies C H J, Nie J F, Barnett M R. Acta Mater, 2012; 60: 218[23] Barnett M R, Keshavarz Z, Ma X. Metall Mater Trans, 2006; 37A: 2283[24] Al–Samman T, Gottstein G. Mater Sci Eng, 2008; A490: 411 |
|