| Re和Ru对镍基单晶高温合金组织偏析的影响 |
| 刘刚, 刘林, 张胜霞, 杨初斌, 张军, 傅恒志 |
| 西北工业大学凝固技术国家重点实验室, 西安 710072 |
|
| EFFECTS OF Re AND Ru ON MICROSTRUCTURE AND SEGREGATION OF Ni-BASED SINGLE-CRYSTAL SUPERALLOYS |
| LIU Gang, LIU Lin, ZHANG Shengxia, YANG Chubin, ZHANG Jun, FU Hengzhi |
| State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072 |
引用本文:
刘刚 刘林 张胜霞 杨初斌 张军 傅恒志. Re和Ru对镍基单晶高温合金组织偏析的影响[J]. 金属学报, 2012, 48(7): 845-852.
,
,
,
,
,
.
EFFECTS OF Re AND Ru ON MICROSTRUCTURE AND SEGREGATION OF Ni-BASED SINGLE-CRYSTAL SUPERALLOYS[J]. Acta Metall Sin, 2012, 48(7): 845-852.
| [1] Hu Z Q, Liu L R, Jin T, Sun X F. Aeroengine, 2005; 31: 1(胡壮麒, 刘丽荣, 金涛, 孙晓峰. 航空发动机, 2005; 31: 1)[2] Pollock T M, Tin S. J Propul Power, 2006; 22: 361[3] Guo J T. Acta Metall Sin, 2010; 46: 513(郭建亭. 金属学报, 2010; 46: 513)[4] Yang C B, Liu L, Zhao X B, Liu G, Zhang J, Fu H Z. Acta Metall Sin, 2011; 47: 1246(杨初斌, 刘林, 赵新宝, 刘 刚, 张军, 傅恒志. 金属学报, 2011; 47: 1246)[5] Walston WS, Schaeffer J C, MurphyWH. In: Kissinger R D, Deye D J, Anton D L, Cetel A D, Nathal M V, Pollock T M, Woodford D A, eds., Superalloys 1996, Warrendale: TMS, 1996: 9[6] Guan X R, Liu E Z, Zheng Z, Yu Y S, Tong J, Zhai Y C. J Mater Sci Technol, 2011; 27: 113[7] Rae C M F, Reed R C. Acta Mater, 2001; 49: 4113[8] Retting R, Singer R F. Acta Mater, 2011; 59: 317[9] Walston S, Cetel A, Mackay R, O’Hara K, Duhl D, Dresfield R. In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S, eds., Superalloys 2004, Warrendale: TMS, 2004: 15[10] Hobbs R A, Zhang L, Rae C M F, Tin S. Metall Mater Trans, 2008; 39A: 1014[11] Hedge S R, Kearsey R M, Beddoes J C. Mater Sci Eng, 2010; A527: 5528[12] Yu J J, Sun X F, Zhao N R, Jin T, Guan H R, Hu Z Q. Mater Sci Eng, 2007; A460–461: 420[13] Feng Q, Carroll L J, Pollock T M. Metall Mater Trans, 2006; 37A: 1949[14] Liu G, Liu L, Zhao X B, Ge B M, Zhang J, Fu H Z. Metall Mater Trans, 2011; 42A: 2733[15] Hu H Q. Solidification Principle of Metals. Beijing: China Machine Press, 2000: 130(胡汉起. 金属凝固原理. 北京: 机械工业出版社, 2000: 130)[16] Kablov E N, Petrushin N V. In: Reed R C, Green K A, Caron P, Gabb T P, Fahrmann M G, Huron E S, Woodard S A, eds., Superalloys 2008, Warrendale: TMS, 2008: 901[17] Karunaratne M S A, Cox D C, Reed R C. In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S, eds., Superalloys 2004, Warrendale: TMS, 2004: 263[18] Volek A, Singer R F. In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S, eds., Superalloys 2004, Warrendale: TMS, 2004: 713[19] Lifshitz L M, Slyozov V V. J Phys Chem, 1961; 19: 35[20] F¨ahrmann M, F¨ahrmann E, Pollock T M, Johnson W C. Metall Mater Trans, 1997; 28A: 1943[21] Neumeier S, Pyczak F, G¨oken M. In: Reed R C, Green K A, Caron P, Gabb T P, Fahrmann M G, Huron E S, Woodard S A, eds., Superalloys 2008, Warrendale: TMS, 2008: 109[22] Tian S G, Zhou H H, Zhang J H, Yang H C, Xu Y B, Hu Z Q. Acta Metall Sin, 1998; 6: 591(田素贵, 周惠华, 张静华, 杨洪才, 徐永波, 胡壮麒. 金属学报, 1998; 6: 591)[23] Zhang J X, Wang J C, Harada H, Koizumi Y. Acta Mater, 2005; 53: 4623[24] Caron P, Khan T. Mater Sci Eng, 1983; A61: 173[25] Ofori A P, Humphreys C J, Jones C N. In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S, eds., Superalloys 2004, Warrendale: TMS, 2004: 787[26] Carroll L J, Feng Q, Mansfield J F, Pollock T M. Mater Sci Eng, 2007; A457: 292[27] Volek A, Pyczak F, Singer R F, Mughrabi H. Scr Mater, 2005; 52: 141[28] Reed R C, Yeh A C, Tin S, Babu S S, Miller M K. Scr Mater, 2004; 51: 327[29] Yokokawa T, Osawa M, Nishida K, Kobayashi T, Koizumi Y, Harada H. Scr Mater, 2003; 49: 1041[30] Chen J Y, Zhao B, Feng Q, Cao L M, Sun Z Q. Acta Metall Sin, 2010; 46: 897(陈晶阳, 赵宾, 冯强, 曹腊梅, 孙祖庆. 金属学报, 2010; 46: 897) |
|