NiCrAlY/Al--Al2O3/Ti2AlNb高温抗氧化和力学性能研究 |
李海庆1,2,宫骏2,孙超2 |
1. 中国运载火箭技术研究院航天材料及工艺研究所, 北京 100076
2. 中国科学院金属研究所金属腐蚀与防护国家重点实验室, 沈阳 110016 |
|
HIGH TEMPERATURE OXIDATION RESISTANCE AND MECHANICAL PROPERTIES OF NiCrAlY/Al--Al2O3 COATINGS ON AN ORTHORHOMBIC Ti2AlNb ALLOY |
LI Haiqing1,2, GONG Jun2, SUN Chao2 |
1. Aerospace Research Institute of Materials and Processing Technology, China Academy of Launch Vehicle Technology,Beijing 100076
2. State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, |
引用本文:
李海庆,宫骏,孙超. NiCrAlY/Al--Al2O3/Ti2AlNb高温抗氧化和力学性能研究[J]. 金属学报, 2012, 48(5): 579-586.
[1] Leyens C, Peters M. Titanium and Titanium Alloys. Weinheim: Wiley--VCH, 2003; 52
[2] Kumpfert J. Adv Eng Mater, 2001; 3: 851
[3] Ralison A, Dettenwanger F, Schutze M. Mater High Temp, 2003; 20: 607
[4] Christoph L. Oxid Met, 1999; 52: 475
[5] Ralison A, Dettenwanger F, Schutze M. Mater Corros, 2000; 51: 317
[6] Dudziak T, Du H L, Datta P K, Wilson A, Ross I M, Moser M, Braun R. Corros Sci, 2009; 51: 1189
[7] Leyens C, Braun R, Frohlich M, Hovsepian P E. JOM, 2006; 58: 17
[8] Cvijovic I, Jovanovic M T, Perusko D. Corros Sci, 2008; 50: 1919
[9] Xiong Y M, Zhu S L, Wang F H. Surf Coat Technol, 2005; 197: 322
[10] Braun R, Leyens C. Mater High Temp, 2005; 22: 437
[11] Braun R, Frohlich M, Leyens C, Renusch D. Oxid Met, 2009; 71: 295
[12] Tang Z L, Wang F H, Wu W T. Surf Coat Technol, 1998; 110: 57
[13] Zhang K, Wang Q M, Sun C, Wang F H. Corros Sci, 2007; 49: 3598
[14] Goward G W. Surf Coat Technol, 1998; 108: 73
[15] Sivakumar R, Mordike B L. Surf Coat Technol, 1989; 37: 139
[16] Wang Q M, Zhang K, Gong J, Cui Y Y, Sun C, Wen L S. Acta Mater, 2007; 55: 1427
[17] Muller J, Schierling M, Zimmermann E, Neuschutz D. Surf Coat Technol, 1999; 120--121: 16
[18] Wang Q M, Wu Y N, Ke P L, Sun C, Huang R F, Wen L S. Acta Metall Sin, 2004; 40: 83
(王启民, 吴颖娜, 柯培玲, 孙超, 黄荣芳, 闻立时. 金属学报, 2004; 40: 83)
[19] Li H Q, Wang Q M, Jiang S M, Gong J, Sun C. Corros Sci, 2010; 52: 1668
[20] Knotek O, Lugscheider E, Loffler F, Beele W. Surf Coat Technol, 1994; 68--69: 22
[21] Yao Y, Li W Z, Wang Q M, Gong J, Sun C, Li J B. Acta Metall Sin, 2008; 44: 876
(姚勇, 李伟洲, 王启民, 宫骏, 孙 超, 李家宝. 金属学报, 2008; 44: 876) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|