| GH738高温合金热变形过程显微组织控制与预测 I.组织演化模型的构建 |
| 姚志浩,董建新,张麦仓 |
| 北京科技大学材料科学与工程学院, 北京 100083 |
|
| MICROSTRUCTURE CONTROL AND PREDICTION OF GH738 SUPERALLOY DURING HOT DEFORMATION
I. Construction of Microstructure Evolution Model |
| YAO Zhihao, DONG Jianxin, ZHANG Maicang |
| School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
姚志浩 董建新 张麦仓. GH738高温合金热变形过程显微组织控制与预测 I.组织演化模型的构建[J]. 金属学报, 2011, 47(12): 1581-1590.
,
,
.
MICROSTRUCTURE CONTROL AND PREDICTION OF GH738 SUPERALLOY DURING HOT DEFORMATION
I. Construction of Microstructure Evolution Model[J]. Acta Metall Sin, 2011, 47(12): 1581-1590.
| [1] Yao Z H, Dong J X, Zhang M C, Zheng L. Rare Met Mater Eng, 2010; 39: 1565(姚志浩, 董建新, 张麦仓, 郑磊. 稀有金属材料与工程, 2010; 39: 1565)[2] Chang K M, Liu X B. Mater Sci Eng, 2001; A308: 1[3] Semiatin S L, Fagin P N, Glavicic M G. Scr Mater, 2004; 50: 625[4] Liu X B, Kang B, Chang K M. Mater Sci Eng, 2003; A340: 8[5] Yao Z H, Dong J X, Zhang M C, Yu Q Y, Zheng L. Trans Mater Heat Treat, 2011; 32: 44(姚志浩, 董建新, 张麦仓, 于秋颖, 郑磊. 材料热处理学报, 2011; 32: 44)[6] Donachie M J, Pinkowish A A, Danesi W P, Radavich J F, Couts W H. Metall Trans, 1970; 1: 2623[7] Guimaraes A A, Jonas J J. Metall Trans, 1981; A12: 1655[8] Livesey D W, Sellars C M. Mater Sci Technol, 1985; 1: 136[9] Li M Q, Yao X Y, Luo J, Lin Y Y, Su S B, Wang H R. Acta Metall Sin, 2007; 43: 937(李淼泉, 姚晓燕, 罗皎, 林莺莺, 苏少博, 王海荣. 金属学报, 2007; 43: 937)[10] Salehi A R, Serajzadeh S, Yazdipour N.Mater Chem Phys, 2007; 101: 153[11] Gao H, Barber G C, Chen Q A, Lu Y Q. J Mater Process Technol, 2003; 142: 52[12] Ganapathysubramanian S, Zabaras N. Int J Solid Struct, 2004; 41: 2011[13] Wang B X, Liu X H, Wang G D. Mater Sci Eng, 2005; A393: 102[14] Sui F L, Xu L X, Chen L Q, Liu X H. J Mater Process Technol, 2011; 211: 433[15] Zhao M L, Sun W R, Yang S L, Qi F, Guo S R, Hu Z Q. Acta Metall Sin, 2009; 45: 79(赵美兰, 孙文儒, 杨树林, 祁峰, 郭守仁, 胡壮麒. 金属学报, 2009; 45: 79)[16] Sellars C M, McTegart W J. Acta Metall, 1966; 14: 1136[17] McQueen H J, Ryan N D. Mater Sci Eng, 2002; A322: 43[18] Sommitsch C, Mitter W. Acta Metall, 2006; 54: 357[19] Gottstein G, Frommert M, Goerdeler M, Schafer N. Mater Sci Eng, 2004; A387–389: 604[20] Solhjoo S. Mater Des, 2010; 31: 1360[21] Poliak E I, Jonas J J. ISIJ Int, 2003; 43: 692[22] Li G, Maccagno T M, Bai D Q. ISIJ Int, 1996; 36: 1479[23] Bai D Q, Yue S, Jonas J J. ISIJ Int, 1996; 36: 1084[24] Shen B Z, Fang N W, Shen H F, Liu B C. Mater Sci Technol, 2005; 13: 516(沈丙振, 方能炜, 沈厚发, 柳百成. 材料科学与工艺, 2005; 13: 516)[25] Li G, Maccagno T M, Bai D Q. ISIJ Int, 1996; 36: 1479[26] Sellars C M, Whiteman J A. Met Sci, 1979; 13: 187[27] Anelli E. ISIJ Int, 1992; 32: 440 |
|