| 梯度硬质合金梯度层形成的计算机模拟及验证 |
| 张伟彬1,沙春生1,杜勇1,温光华2,谢文2,王社权2 |
1.中南大学粉末冶金国家重点实验室, 长沙 410083
2.株洲钻石切削刀具股份有限公司, 株洲 412007 |
|
| COMPUTER SIMULATIONS AND VERIFICATION OF GRADIENT ZONE FORMATION IN CEMENTED CARBIDES |
| ZHANG Weibin1, SHA Chunsheng1, DU Yong1, WEN Guanghua2, XIE Wen2, WANG Shequan2 |
1.State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083
2.Zhuzhou Cemented Carbide Cutting Tools Limited Company, Zhuzhou 412007 |
引用本文:
张伟彬 沙春生 杜勇 温光华 谢文 王社权. 梯度硬质合金梯度层形成的计算机模拟及验证[J]. 金属学报, 2011, 47(10): 1307-1314.
,
,
,
,
,
.
COMPUTER SIMULATIONS AND VERIFICATION OF GRADIENT ZONE FORMATION IN CEMENTED CARBIDES[J]. Acta Metall Sin, 2011, 47(10): 1307-1314.
| [1] Zhang W Z, Liu Y, He Y H, Wang H B. Rare Met Cem Carbides, 2005; 33(2): 28(张武装, 刘 咏, 贺跃辉, 王海兵. 稀有金属及硬质合金, 2005; 33(2): 28)[2] Konyashin I Y. Mater Sci Eng, 1997; A230: 213[3] Konyashin I Y. Surf Coat Technol, 1995; 71: 277[4] Knotek O, Loffler F, Kramer G. Int J Ref Hard Mater, 1996; 14: 195[5] Narasimhan K, Boppana S P, Bhat D G. Wear, 1995; 188: 123[6] Frykholm R, Ekroth M, Jansson B, Andrén H O, Ågren J. Acta Mater, 2003; 51: 1115[7] Schwarzkopf M, Exner H E, Fischmeister H F. Mater Sci Eng, 1998; A105–106: 225[8] Chen L M, Lengauer W, Ettmayer P, Dreyer K, Daub H W, Kassel D. Int J Ref Hard Mater, 2000; 18: 307[9] Frykholm R, Andrén H O. Mater Chem Phys, 2001; 67: 203[10] Andr´en H O. Mater Chem Phy, 2001; 67: 209[11] Rosso M, Kassel D. Int J Ref Hard Mater, 1999; 17: 187[12] Dreyer K, Kassel D. Int Plansee Seminar, 2001; 2: 768[13] Suzuki H, Koji H, Yasuro T. Trans Jpn Inst Met, 1981; 22: 758[14] Gustafson P, Östlund Å. Int J Ref Hard Mater, 1993–1994; 12: 129[15] Ekroth M, Frykholm R, Lindholm M, Andrén H O, Ågren J. Acta Mater, 2000; 48: 2177[16] Frykholm R, Ekroth M, Jansson B, Andrén H O, Ågren J. Int J Ref Hard Mater, 2001; 19: 527[17] Ekroth M, Frisk K, Jansson B, Dumitrescu F S. Metall Mater Trans, 2000; 31B: 615[18] Frisk K, Dumitrescu F S, Ekroth M, Jansson B, Kruse O, Sundman B. J Phase Equilib, 2001; 22: 645[19] Gustafson P. Mater Sci Technol, 1986; 2: 635[20] Andrén J O, Helander T, H¨oglund L H, Shi P F, Sundman B. Calphad, 2002; 26: 273[21] Andrén H O. Mater Chem Phys, 2001; 67: 209 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|