Please wait a minute...
金属学报  2011, Vol. 47 Issue (1): 109-114    DOI: 10.3724/SP.J.1037.2010.00370
  论文 本期目录 | 过刊浏览 |
Na1.4Co2O4基热电材料的溶胶-凝胶法制备及表征
厉英, 马北越, 王臻明, 姜茂发
东北大学材料与冶金学院, 沈阳 110819
PREPARATION OF Na1.4Co2O4 BASED THERMOELECTRIC MATERIALS BY SOL-GEL METHOD AND CHARACTERIZATION
LI Ying, MA Beiyue, WANG Zhenming, JIANG Maofa
School of Materials and Metallurgy, Northeastern University, Shenyang 110819
引用本文:

厉英 马北越 王臻明 姜茂发. Na1.4Co2O4基热电材料的溶胶-凝胶法制备及表征[J]. 金属学报, 2011, 47(1): 109-114.
, , . PREPARATION OF Na1.4Co2O4 BASED THERMOELECTRIC MATERIALS BY SOL-GEL METHOD AND CHARACTERIZATION[J]. Acta Metall Sin, 2011, 47(1): 109-114.

全文: PDF(1112 KB)  
摘要: 采用溶胶-凝胶法制备了掺杂Sr, Li和Cu的Na1.4Co2O4基热电材料, 采用XRD分析了Na1.4Co2O4基热电材料的相组成.通过DTA-TG曲线确定材料的预烧结和终烧结温度分别为450和850 ℃. 研究了掺杂量对Na1.4Co2O4基材料电阻率、Seebeck系数和功率因子等热电性能的影响. 结果表明, 掺杂Li可降低Na1.4Co2O4的电阻率, 掺杂 Sr和Cu使材料的电阻率增加; 掺杂Li和Cu可大幅度提高Na1.4Co2O4的Seebeck系数和功率因子; 掺杂Sr的改善效果不显著, 掺杂Li的效果最好; 当Li掺杂量为0.40, Na1.4Co2O4基热电材料的功率因子在15℃时达到最大值 7444.73 μW?m-1?K-2.
关键词 : 热电材料,  钴酸盐,  热电性能,  掺杂,  溶胶-凝胶法    
Abstract:Sr, Li and Cu-doped Na1.4Co2O4 based thermoelectric materials were prepared by sol-gel process. The phase constitution of Na1.4Co2O4 based thermoelectric materials was analyzed by XRD. According to DTA-TG curves, the pre-sintering and sintering temperatures of the materials were obtained to be 450 ℃ and 850 ℃, respectively. The influences of doping amount on the electrical resistivity, Seebeck coefficient and power factor of Na1.4Co2O4 based materials were investigated. The results showed that doping Li could decrease the electrical resistivity of Na1.4Co2O4, doping Sr and Cu could increase the electrical resistivity. Doping Li and Cu could improve the Seebeck coefficient and power factor of Na1.4Co2O4. The improving effect on Na1.4Co2O4 by doping Sr is not remarkable but by doping Li is the best. When 0.40 Li was doped, the power factor of Na1.0Li0.4Co2O4 at 15 ℃ reaches maximum value of 7444.73 μW?m-1?K-2.
Key words: thermoelectric material    cobaltite    thermoelectric property    doping    sol-gel method
收稿日期: 2010-07-23     
基金资助:

国家自然科学基金项目51074038和50774018资助

作者简介: 厉英, 女, 1963年生, 博士, 副教授
[1] Ibrahim M M, Saleh S A, Ibrahim E M M, Hakeem A M A. J Alloys Compd, 2008; 452: 200

[2] Xiang P H, Kinemuchi Y, Kaga H, Watari K. J Alloys Compd, 2008; 454: 364

[3] Seetawan T, Amornkitbamrung V, Burinprakhon T, Maensiri S, Tongbai P, Kurosaki K, Muta H, Uno M, Yamanaka S. J Alloys Compd, 2008; 416: 291

[4] Cheng J G, Sui Y, Fu H J, Lu Z, Wei B, Qian Z N, Miao J P, Liu Z G, Huang X Q, Zhu R B, Wang X J, Su W H. J Alloys Compd, 2006; 407: 299

[5] Li Y, Xu G Y, Jiang M F. J Mater Sci Technol, 2006; 22: 526

[6] Li N, Jiang Y, Li G H,Wang C, Shi J F, Yu D B. J Alloys Compd, 2009; 467: 444

[7] Terassaki I, Sasago Y, Uchinokura K. Phys Rev, 1997; 56B: 12685

[8] Shi Y W, Qiao G J, Jin Z H. Rare Met Mater Eng, 2005; 34: 12

(石尧文, 乔冠军, 金志浩. 稀有金属材料与工程, 2005; 34: 12)

[9] Itoh T, Kawata T, Kitajima T, Terasaki I. Proc 17th Int Conf on Thermoelectrics, NJ: IEEE, 1998: 595

[10] Mrotzek A, M¨uller E, Plewa J. Proc 22nd Int Conf on Thermoelectrics, NJ: IEEE, 2003: 219

[11] Ito M, Nagira T, Furumoto D, Oda Y, Hara S. Sci Technol Adv Mater, 2004; 5: 125

[12] Motohashi T, Naujalis E, Veda R, Isawa K, Karppinen M, Yamauchi H. Appl Phys Lett, 2001; 79: 1480

[13] Wu D, Wang N L, Li G, Luo J L , Zheng P, Chen X H, Wang C H, Luo X G, Jin R, Mandrus D. J Phys Chem Solids, 2006; 67: 635

[14] Pei J, Chen G, Li X, Li Y X, Zhou N. Mater Lett, 2009; 63: 1459

[15] Yakabe H, Fujita K, Nakamura K, Kikuchi K. Proc 17th Int Conf on Thermoelectrics, NJ: IEEE, 1999: 551 

[16] Cui Z Q, Liu B X. Metallography and Heat Treatment Principle. Harbin: Harbin Institute of Technology Press, 2001: 19

(崔忠圻, 刘北兴. 金属学与热处理原理. 哈尔滨: 哈尔滨工业大学出版社, 2001: 19)

[17] Zhong G X. Semiconductor Refrigeration and Its Application. Beijing: Science Press, 1989: 13, 190

(钟广学. 半导体制冷器件及其应用. 北京: 科学出版社, 1989: 13, 190)

[18] Park K, Jang K U, Kwon H C, Kim J G, Cho W S. J Alloys Compd, 2006; 419: 213

[19] Wang Y, Sui Y, Cheng J G, Wang X J, Miao J P, Liu Z G, Qian Z N, Su W H. J Alloys Compd, 2008; 448: 1

[20] Nagira T, Ito M, Katsuyama S, Majima K, Nagai H. J Alloys Compd, 2003; 348: 263
[1] 王福容, 张永梅, 柏国宁, 郭庆伟, 赵宇宏. Al掺杂Mg/Mg2Sn合金界面的第一性原理计算[J]. 金属学报, 2023, 59(6): 812-820.
[2] 李斗, 徐长江, 李旭光, 李双明, 钟宏. La掺杂P型CeyFe3CoSb12 热电材料及涂层的热电性能[J]. 金属学报, 2023, 59(2): 237-247.
[3] 刘志愿, 王永贵, 赵成玉, 杨婷, 夏爱林. p型方钴矿热电材料纳米-介观尺度微结构调控[J]. 金属学报, 2022, 58(8): 979-991.
[4] 赵立东, 王思宁, 肖钰. 热电材料的载流子迁移率优化[J]. 金属学报, 2021, 57(9): 1171-1183.
[5] 毛斐, 吕皓, 唐法威, 郭凯, 刘东, 宋晓艳. Mn和In添加对SmCo7结构稳定性及磁矩影响的第一性原理计算[J]. 金属学报, 2021, 57(7): 948-958.
[6] 杨莎莎,杨峰,陈明辉,牛云松,朱圣龙,王福会. N掺杂对磁控溅射Ta涂层微观结构与耐磨损性能的影响[J]. 金属学报, 2019, 55(3): 308-316.
[7] 张世政,徐要辉,汪庭语,李锐星,才鸿年. In3+掺杂CeO2的固溶度及其储氧能力*[J]. 金属学报, 2016, 52(5): 607-613.
[8] 单麟婷, 巴德纯, 曹青, 侯雪艳, 李建昌. Ce-Cu共掺杂对SnO2薄膜光电特性的影响*[J]. 金属学报, 2014, 50(1): 95-102.
[9] 孙洪元,李双明,冯松科,傅恒志. Co-Sb合金定向凝固组织与相选择[J]. 金属学报, 2013, 49(6): 682-688.
[10] 李泓霖,张仲,吕英波,黄金昭,刘如喜. Eu掺杂ZnO结构光电性质的第一性原理及实验研究[J]. 金属学报, 2013, 29(4): 506-512.
[11] 周立颖,王福合. 点缺陷对γ-TiAl (100)表面O原子吸附和扩散影响的第一性原理研究[J]. 金属学报, 2013, 49(11): 1387-1391.
[12] 厉英,丁玉石,崔绍刚,王常珍. 掺杂Sc的CaZrO3的制备及电学性能[J]. 金属学报, 2012, 48(5): 575-578.
[13] 范永中 张淑娟 涂金伟 孙霞 刘芳 李明升. Si和Y掺杂对(Ti, Al)N涂层结构和性能的影响[J]. 金属学报, 2012, 48(1): 99-106.
[14] 高茜 孙本哲 祁阳 齐连仲. 溶胶--凝胶法制备的Zn1-xCoxO晶体粉末的结构和磁性行为[J]. 金属学报, 2011, 47(3): 337-343.
[15] 向鑫 陈长安 刘柯钊 罗丽珠 刘婷婷 王小英. C掺杂对Al中He行为的影响[J]. 金属学报, 2010, 46(3): 318-323.