Eu掺杂ZnO结构光电性质的第一性原理及实验研究
李泓霖1),张仲1),吕英波2),黄金昭1),刘如喜1)
1) 济南大学物理科学与技术学院, 济南 250022
2) 山东大学威海分校空间科学与物理学院, 威海 264209
FIRST-PRINCIPLES AND EXPERIMENTAL STUDY ON THE ELECTRONIC AND OPTICAL PROPERTIES OF Eu DOPED ZnO STRUCTURE
LI Honglin1), ZHANG Zhong1), LU Yingbo2), HUANG Jinzhao1), LIU Ruxi1)
1) School of Physics and Technology, University of Jinan, Jinan 250022
2) School of Space Science and Physics, Shandong University at Weihai, Weihai 264209
全文: PDF(1082 KB)  
摘要: 

采用基于密度泛函理论的第一性原理平面波超软赝势方法, 计算了稀土Eu掺杂ZnO结构的能带结构、态密度以及光学性质,并与未掺杂体系进行了对比分析. 结果表明, Eu掺杂的ZnO结构引入了由Eu贡献的导电载流子,体系的电导率增强, Fermi能级上升进入导带并表现n型导电性. 光学性质上, 掺杂结构在低能区域的吸收系数要比纯净ZnO高. 在随后的实验部分, 通过烧结法制备了Eu掺杂的ZnO粉体, 并利用SEM, XRD和光致发光光谱(PL)表征了掺杂前后ZnO结构的变化. 结果表明, Eu的掺入使得ZnO的晶格常数变大, 结晶程度变弱.

关键词 ZnOEu掺杂第一性原理    
Abstract

Pure and Eu doped ZnO were calculated by first-principles full potential linearized augmented plane wave ultra-soft pseudo-potential method to investigate band structures, density of states (DOS) and optical properties of the structures. The results show that the conduction bands generate conductive carriers introduced by impurity atom of Eu. The electrical conductivity of the system is improved and the Fermi levels shift upward into the conduction band and show n-type conductivity. The absorption coefficient of Eu doped ZnO are higher than that of pure ZnO in low energy region. In the experiment part, pure and Eu doped ZnO powder were prepared through sintering method and the corresponding properties of the samples were investigated by XRD, SEM and photoluminescence (PL) spectra, which show that the lattice constants of ZnO become larger and crystallization turn worse after doping.

Key wordsZnO    Eu    doping    first-principles
收稿日期: 2012-11-07     
基金资助:

国家青年科学基金项目11104114和山东省科技发展计划项目2009GG2003028资助

通讯作者: 张仲     E-mail: ss-zhangz@ujn.edu.cn
作者简介: 李泓霖, 男, 1990年生, 硕士生

引用本文:

李泓霖,张仲,吕英波,黄金昭,刘如喜. Eu掺杂ZnO结构光电性质的第一性原理及实验研究[J]. 金属学报, 2013, 29(4): 506-512.
LI Honglin, ZHANG Zhong, LU Yingbo, HUANG Jinzhao, LIU Ruxi. FIRST-PRINCIPLES AND EXPERIMENTAL STUDY ON THE ELECTRONIC AND OPTICAL PROPERTIES OF Eu DOPED ZnO STRUCTURE. Acta Metall Sin, 2013, 29(4): 506-512.

链接本文:

https://www.ams.org.cn/CN/10.3724/SP.J.1037.2012.00667      或      https://www.ams.org.cn/CN/Y2013/V29/I4/506

[1] Huang S Y, Xu S, Chai J W, Cheng Q J, Long J D, Ostrikov K.  Mater Lett, 2009; 63: 972


 


[2] Zhou H M, Yi D Q, Yu Z M, Xiao L R, Li J, Wang B.  Acta Metall Sin, 2006; 42: 505

 


(周宏明, 易丹青, 余志明, 肖来荣, 李荐, 王斌. 金属学报, 2006; 42: 505)

 


[3] Lu Y F, Ye Z Z, Zhu L P, Zeng Y J, Huang J Y, Zhao B H.  J Mater Sci Technol, 2013; 29: 154

 


[4] Huang G S, Wu X L, Cheng Y C, Shen J C, Huang A P, Chu P K.  Appl Phys, 2007; 86A: 463

 


[5] Pei G Q, Xia C T, Wu B, Wang T.  Comput Mater Sci, 2008; 43: 489

 


[6] Kaur G, Dwivedi Y, Rai S B.  J Fluoresc, 2011; 21: 423

 


[7] Peng Z J, Yang Y Y, Wang C B, Fu Z Q.  Acta Metall Sin, 2008; 10: 1265

 


(彭志坚, 杨义勇, 王成彪, 付志强. 金属学报, 2008; 10: 1265)

 


[8] Abdullah M, Panatarani C, Kim T O, Okuyam K.  J Alloys Compd, 2004; 377: 298

 


[9] Ronfard-Haret J C, Valat P, Wintgens V, Kossanyi J.  J Lumin, 2000; 91: 71

 


[10] Lang J H, Li X, Yang J H, Yang L L, Zhang Y J, Yan Y S, Han Q, Wei M B, Gao M, Liu X Y, Wang R.

 


 Appl Surf Sci, 2011; 257: 9574

 


[11] Atsushi I, Satoshi F, Hisao Y.  Opt Mater, 2011; 33: 1116

 


[12] Chen P L, Ma X Y, Yang D R.  J Alloys Compd, 2007; 431: 317

 


[13] Zhang L L, Ling Y W, Zhang L, Shi P.  Rare Met Mater Eng, 2008; 37: 370

 


(张琳丽, 凌亚文, 张玲, 史彭. 稀有金属材料与工程, 2008; 37: 370)

 


[14] Xin X S, Zhou B B, Lu S C, Su W H.  Acta Phys Sin, 2005; 54: 1859

 


(辛显双, 周百斌, 吕树臣, 苏文辉. 物理学报, 2005; 54: 1859)

 


[15] Bagnall D M, Chen Y F, Zhu Z, Yao T, Shen M Y, Goto T.  Appl Phys Lett, 1998; 73: 1038

 


[16] Deng S H, Duan M Y, Xu M, He L.  Physica, 2011; 406B: 2314

 


[17] Hong G Y.  Rare Earth Luminescent Materials-Basic and Applied. Beijing: Science Press, 2011: 50

 


(洪广言. 稀土发光材料-基础与应用. 北京: 科学出版社, 2011: 50)

 


[18] Zhang F C, Zhang Z Y, Zhang W H.  Acta Opt Sin, 2009; 29: 1025

 


[19] Burstein E.  Phys Rev, 1954; 93: 632

 


[20] Shen X C.  Semiconductor Optical Properties. Beijing: Science Press, 1992: 24

 


(沈学础. 半导体光学性质. 北京: 科学出版社, 1992: 24)

 


[21] Yang L L, Zhao Q X, Willander M, Ivanov I G.  J Appl Phys, 2009; 105: 053503

 


[22] Wang Y G, Lau S P, Lee H W, Yu S F, Tay B K, Zhang X H, Hng H H.  J Appl Phys, 2003; 94: 354

 


[23] Wu C L, Qiao X L, Luo L L, Li H J.  Mater Res Bull, 2008; 43: 1883

 


[24] Alvi N H, Ali S M U, Hussain S, Nur O, Willander M.  Scr Mater, 2011; 64: 697

 


[25] Yang J H, Wang R, Yang L L, Lang J U, Wei M B.  J Alloys Compd, 2011; 509: 3606

 


[26] Lu J G, Fujita S, Kawaharamura T, Nishinaka H, Kamada Y, Ohshima T, Ye Z Z, Zeng Y J, Zhang Y Z, Zhu L

 


P, He H P, Zhao B H.  J Appl Phys, 2007; 101: 083705

 


[27] Chaitanya D P, Thomas A, Ruairi H, Stefano S.  J Magn Magn Mater, 2007; 316: e185

 


[28] Zhao J L, Li X M, Bian J M, Yu W D, Zhang C Y.  J Cryst Growth, 2005; 208: 495
[1] 高翔, 张桂凯, 向鑫, 罗丽珠, 汪小琳. 合金元素对V(110)表面O吸附影响的第一性原理研究[J]. 金属学报, 2020, 56(6): 919-928.
[2] 白静, 石少锋, 王锦龙, 王帅, 赵骧. Ni-Mn-Ga-Ti铁磁形状记忆合金的相稳定性和磁性能的第一性原理计算[J]. 金属学报, 2019, 55(3): 369-375.
[3] 杨莎莎,杨峰,陈明辉,牛云松,朱圣龙,王福会. N掺杂对磁控溅射Ta涂层微观结构与耐磨损性能的影响[J]. 金属学报, 2019, 55(3): 308-316.
[4] 董彩虹, 刘永利, 祁阳. 厚度对Bi薄膜表面特性和电学性质的影响[J]. 金属学报, 2018, 54(6): 935-942.
[5] 周刚, 叶荔华, 王皞, 徐东生, 孟长功, 杨锐. 六角结构金属中基面/柱面取向转变的孪晶路径及合金化效应的第一性原理研究[J]. 金属学报, 2018, 54(4): 603-612.
[6] 崔荣华, 王歆钰, 董正超, 仲崇贵. Mg1-xZnx合金的弹性和热力学性质的第一性原理研究[J]. 金属学报, 2017, 53(9): 1133-1139.
[7] 陶辉锦,周珊,刘宇,尹健,许昊. D019-Ti3Al中点缺陷浓度与相互作用的第一性原理研究[J]. 金属学报, 2017, 53(6): 751-759.
[8] 白静,李泽,万震,赵骧. Ni-Mn-Ga-Cu铁磁形状记忆合金的晶体结构、相稳定性和磁性能的第一性原理研究[J]. 金属学报, 2017, 53(1): 83-89.
[9] 张世政,徐要辉,汪庭语,李锐星,才鸿年. In3+掺杂CeO2的固溶度及其储氧能力*[J]. 金属学报, 2016, 52(5): 607-613.
[10] 盛立远,郭建亭,赖琛,奚廷斐. Zr添加对NiAl/Cr(Mo)基共晶合金微观组织和力学性能的影响*[J]. 金属学报, 2015, 51(7): 828-834.
[11] 李国建, 王振, 王强, 王慧敏, 杜娇娇, 马永会, 赫冀成. 强磁场作用时间对氧化法制备的Co掺杂ZnO薄膜微观结构和光学性能的影响[J]. 金属学报, 2014, 50(12): 1538-1542.
[12] 单麟婷, 巴德纯, 曹青, 侯雪艳, 李建昌. Ce-Cu共掺杂对SnO2薄膜光电特性的影响*[J]. 金属学报, 2014, 50(1): 95-102.
[13] 王晓红,谢文静,郝臣,张鹏飞,傅小奇,司乃潮. 木素磺酸钙模板法液相合成花簇状ZnO及其光催化性能[J]. 金属学报, 2013, 49(9): 1098-1104.
[14] 刘中秋,李宝宽,姜茂发,张立,徐国栋. 连铸结晶器内氩气/钢液两相非稳态湍流特性的大涡模拟研究[J]. 金属学报, 2013, 49(5): 513-522.
[15] 张旭东,王绍青. Al3Sc和Al3Zr金属间化合物热力学性质的第一性原理计算[J]. 金属学报, 2013, 29(4): 501-505.