Please wait a minute...
金属学报  2011, Vol. 47 Issue (1): 115-122    DOI: 10.3724/SP.J.1037.2010.00351
  论文 本期目录 | 过刊浏览 |
工艺参数对爆炸喷涂WC-Co涂层性能均匀性的影响
王铁钢1), 宋丙红2), 华伟刚1), 宫骏1), 孙超1)
1) 中国科学院金属研究所金属腐蚀与防护国家重点实验室, 沈阳 110016
2) 中航工业哈尔滨东安发动机(集团)有限公司, 哈尔滨 150066
INFLUENCE OF PROCESS PARAMETERS ON THE PERFORMANCE UNIFORMITY OF DETONATION GUN SPRAYED WC-Co COATINGS
WANG Tiegang1),  SONG Binghong2),  HUA Weigang1), GONG Jun1), SUN Chao1)
1) State Key Laboratory of Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
2) AVIC Harbin Dong'an Engine (Group) Co., Ltd., Harbin 150066
引用本文:

王铁钢 宋丙红 华伟刚 宫骏 孙超. 工艺参数对爆炸喷涂WC-Co涂层性能均匀性的影响[J]. 金属学报, 2011, 47(1): 115-122.
, , , , . INFLUENCE OF PROCESS PARAMETERS ON THE PERFORMANCE UNIFORMITY OF DETONATION GUN SPRAYED WC-Co COATINGS[J]. Acta Metall Sin, 2011, 47(1): 115-122.

全文: PDF(1488 KB)  
摘要: 采用正交实验, 分别研究了氧燃率、喷涂距离对爆炸喷涂WC-Co涂层性能的影响. 通过工艺优化, 获得了结构均匀致密、硬度高、弹性模量大、耐磨性能好的WC-Co涂层. 利用 XRD和SEM分析涂层的物相组成、观察其微观结构, 经截面与表面力学性能和磨损性能对比, 优化后的涂层表现出近似各向同性特征. 分析指出涂层均匀的微观结构及低孔隙率是导致其近似各向同性特征的主要原因.
关键词 : 爆炸喷涂,  WC-Co涂层,  孔隙率,  显微硬度,  弹性模量,  微尺度磨粒磨损    
Abstract:Based on the orthogonal experiment, the effects of oxygen-fuel ratio and spraying distance on physical and mechanical properties of D-gun sprayed WC-Co coatings were investigated. An ideal coating with the uniform dense microstructures, high hardness and elastic modulus, and excellent wear resistance was obtained by technology optimization. The phase identifications and microstructure observation of the optimized WC-Co coating were conducted by XRD and SEM, respectively. The coating showed near-isotropic behaviors, which has been verified by the comparisons of mechanical and wear properties between cross section and surface. The mechanisms how the spraying parameters affected near--isotropic characters of the D-gun sprayed WC-Co coating were analyzed and discussed.
Key words: detonation gun spraying    WC-Co coating    porosity    microhardness    elastic modulus    micro-scale abrasive wear
收稿日期: 2010-07-14     
ZTFLH: 

TG174.44

 
作者简介: 王铁钢, 男, 1978年生, 助理研究员, 博士
[1] Lima R S, Karthikeyan J, Kay C M, Lindemann J, Berndt C C. Thin Solid Films, 2002; 416: 129

[2] Picas J A, Xiong Y, Punset M, Ajdelsztajn L, Forn A, Schoenung J M. Int J Refract Met Hard Mater, 2009; 27: 344

[3] Kucuk A, Lima R S, Berndt C C. J Am Ceram Soc, 2001; 84: 685

[4] Kulkarni A, Vaidya A, Goland A, Sampath S, Herman H. Mater Sci Eng, 2003; A359: 100

[5] Nakamura T, Qian G, Berndt C C. J AmCeramSoc, 2000; 83: 578

[6] Friis M, Persson C, Wigren J. Surf Coat Technol, 2001; 141: 115

[7] Gahlin R, Larsson M, Hedenqvist P, Jacobson S, Hogmark S. Surf Coat Technol, 1997; 90: 107

[8] Archard J F. J Appl Phys, 1953; 24: 981

[9] Kassman A, Jacobson S, Erickson L, Hedenqvist P, Olsson M. Surf Coat Technol, 1991; 50: 75

[10] Bemporad E, Sebastiani M, Felicis D D, Carassiti F, Valle R, Casadei F. Thin Solid Films, 2006; 515: 186

[11] Trezona R I, Hutchings I M. Wear, 1999; 233–235: 209

[12] Shipway P H, Hutchings I M. Surf Coat Technol, 1995; 71: 1

[13] Gee M G, Gant A, Hutchings I M, Bethke R, Schiffman K, Acker K V, Poulat S, Gachon Y, Stebut J V. Wear, 2003; 255: 1

[14] Kusano Y, Acker K V, Hutchings I M. Surf Coat Technol, 2004; 183: 312

[15] Du H, Hua W G, Liu J G, Gong J, Sun C, Wen L S. Mater Sci Eng, 2005; A408: 202

[16] Lima R S, Marple B R. Acta Mater, 2004; 52: 1163

[17] Mcpherson R. Thin Solid Films, 1981; 83: 297

[18] Yang J F, Ohji T, Kanzaki S, Diaz A, Hampshire S. J Am Ceram Soc, 2002; 85: 1512

[19] Bolelli G, Cannillo V, Lusvarghi L, Manfredini T, Siligardi C, Bartuli C, LoretoA, Valente T. J Eur CeramSoc, 2005; 25: 1835

[20] Camerucci M A, Urretavizcaya G, Cavalieri A L. J Eur Ceram Soc, 2001; 21: 1195

[21] Mellali M, Fauchais P, Grimaud A. Surf Coat Technol, 1996; 81: 275

[22] Ban Z G, Shaw L L. Acta Mater, 2001; 49: 2933

[23] Fervel V, Normand B, Liao H, Coddet C, Beche E, Berjoan R. Surf Coat Technol, 1999; 111: 255

[24] Semenov S Y, Cetegen B M. Mater Sci Eng, 2002; A335: 67

[25] Wang T G, Zhao S S, Hua W G, Gong J, Sun C. Surf Coat Technol, 2009; 203: 1637

[26] Cartier M, McDonnell L, Cashell E M. Surf Coat Technol, 1991; 48: 241

[27] Matejicek J, Sampath S, Brand P C, Prask H J. Acta Mater, 1999; 47: 607

[28] Allen A J, Ilavsky J, Long G G, Wallace J S, Berndt C C, Herman H. Acta Mater, 2001; 49: 1661

[29] Kroupa F, Dubsky J. Scr Mater, 1999; 40: 1249

[30] Jin G, Xu B S, Wang H D, Li Q F,Wei S C. Mater Lett, 2007; 61: 2454
[1] 梁琛, 王小娟, 王海鹏. 快速凝固Ti-Al-Nb合金B2相形成机制与显微力学性能[J]. 金属学报, 2022, 58(9): 1169-1178.
[2] 王明康, 苑峻豪, 刘宇峰, 王清, 董闯, 张中伟. Ti对Zr-Nb二元合金β结构稳定性和力学性能的影响[J]. 金属学报, 2021, 57(1): 95-102.
[3] 刘震鹏, 闫志巧, 陈峰, 王顺成, 龙莹, 吴益雄. 金刚石工具用Cu-10Sn-xNi合金的制备和性能表征[J]. 金属学报, 2020, 56(5): 760-768.
[4] 李源才, 江五贵, 周宇. 纳米孔洞对单晶/多晶Ni复合体拉伸性能的影响[J]. 金属学报, 2020, 56(5): 776-784.
[5] 邓聪坤,江鸿翔,赵九洲,何杰,赵雷. Ag-Ni偏晶合金凝固过程研究[J]. 金属学报, 2020, 56(2): 212-220.
[6] 刘海霞, 陈金豪, 陈杰, 刘光磊. NaCl溶液腐蚀后304不锈钢的射流空蚀特征[J]. 金属学报, 2020, 56(10): 1377-1385.
[7] 翟斌, 周凯, 吕鹏, 王海鹏. 自由落体条件下Ti-6Al-4V合金微液滴的快速凝固研究[J]. 金属学报, 2018, 54(5): 824-830.
[8] 陈占兴,丁宏升,刘石球,陈瑞润,郭景杰,傅恒志. 直流电流对Ti-48Al-2Cr-2Nb合金组织和性能的影响[J]. 金属学报, 2017, 53(5): 583-591.
[9] 丁杰, 张志明, 王俭秋, 韩恩厚, 唐伟宝, 张茂龙, 孙志远. 三代核电接管安全端异种金属焊接接头的显微表征[J]. 金属学报, 2015, 51(4): 425-439.
[10] 齐东丽, 雷浩, 范迪, 裴志亮, 宫骏, 孙超. Mo含量对CrMoN复合涂层的组织结构和性能的影响[J]. 金属学报, 2015, 51(3): 371-377.
[11] 濮晟, 谢光, 郑伟, 王栋, 卢玉章, 楼琅洪, 冯强. W和Re对固溶态镍基单晶高温合金变形和再结晶的影响*[J]. 金属学报, 2015, 51(2): 239-248.
[12] 薛飞, 米涛, 王美玲, 丁贤飞, 李相辉, 冯强. Ni对Co-Al-W基合金时效组织演变和γ′相溶解行为的影响*[J]. 金属学报, 2014, 50(7): 845-853.
[13] 秦飞, 项敏, 武伟. 纳米压痕法确定TSV-Cu的应力-应变关系*[J]. 金属学报, 2014, 50(6): 722-726.
[14] 叶兴龙, 刘枫, 金海军. 压缩变形纳米多孔金电化学驱动性能研究*[J]. 金属学报, 2014, 50(2): 252-258.
[15] 李群,王清,李晓娜,高晓霞,董闯. 三元β-Ti-Mo-Zr(Sn)合金析出相对弹性模量和力学性能的影响[J]. 金属学报, 2013, 49(9): 1143-1147.