| Ü690合金在高温水中的应力腐蚀裂纹扩展行为 |
| 但体纯1, 吕战鹏 2, 王俭秋1,韩恩厚1,庄子哲雄2,柯伟1 |
1. 中国科学院金属研究所腐蚀与防护国家重点实验室, 沈阳 110016
2. 日本东北大学断裂与可靠性研究中心, 仙台 980--8579 |
|
| CRACK GROWTH BEHAVIOR FOR STRESS CORROSION CRACKING OF 690 ALLOY IN HIGH TEMPERATURE WATER |
| DAN Tichun 1, LÜ Zhanpeng 2, WANG Jianqiu 1, HAN Enhou 1, SHOJI Testuo 2, KE Wei 1 |
1. Environmental Corrosion Center, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
2. Fracture and Reliability Research Institute, Tohoku University, Sendai 980–8579, Japan |
引用本文:
但体纯 吕战鹏 王俭秋 韩恩厚 庄子哲雄 柯伟. Ü690合金在高温水中的应力腐蚀裂纹扩展行为[J]. 金属学报, 2010, 46(10): 1267-1274.
,
,
,
,
,
.
CRACK GROWTH BEHAVIOR FOR STRESS CORROSION CRACKING OF 690 ALLOY IN HIGH TEMPERATURE WATER[J]. Acta Metall Sin, 2010, 46(10): 1267-1274.
| [1] Speidel M O, Magdowski R. 6th International Symposium on Environmental Degradation of Materials in Nuclear Power Systems-Water Reactors,edited by Gold R E, Simonen E P.(1993): 361-371.[2] Moshier W C, Brown C M. Corrosion, 2000, Vol. 56(No. 3): 307-320.[3] Yamazaki S, Lu Z P, Ito Y, Takeda Y, Shoji T. Corros Sci, 2008, Vol. 50(2008): 835-846.[4] Rebak R B, Szklarska-Smialowska Z. Corros Sci, 1996, Vol. 38, No. 6(1996): 971-988.[5] Page R A, Mcminn A. Metall Trans A, 1986, Vol. 17A, No. 5(1986): 877-887.[6] Andresen P L, Hickling J, Ahluwalia A, Wilson J. Corrosion, 2008, Vol. 64(2008): 707-720.[7] Vaillant F, Mitheux J D, Bouvier O, Vancon D, Zacharie G, Brechet Y, Louchet F. 9th International Symposium on Environmental Degradation of Materials in Nuclear Power Systems-Water Reactors,edited by Ford F P, Bruemmer S M, Was G S.(1999): 251-260[8] Sui G, Titchmarsh J M, Heys G B, Congleton J. Corros Sci, 1997, Vol. 39(No. 3): 565-587.[9] Scenini F, Newman R C, Cottis R A, Jacko R J. 12th International Symposium on Environmental Degradation of Materials in Nuclear Power Systems-Water Reactors,edited by Allen T R, King P J, Nelson L.(2005): 891-901[10] Young B A, Gao X, Srivatsan T S, King P J. Materials and Design. 2007. Vol. 28: 373-379.[11] Lu Z, Shoji T, Takeda Y, Kai A, Ito Y. Corrosion. 2007. Vol. 63(No. 11): 1020-1032.[12] Lu Z P, Shoji T, Takeda Y, Ito Y, Yamazaki S. Corros Sci, 2008, Vol. 50: 698-712.[13] Lu Z P, Shoji T, Takeda Y, Ito Y, Kai A, Tsuchiya N. Corros Sci. 2008. Vol. 50: 625-638.[14] Lu Z P, Shoji T, Takeda Y, Ito Y, Kai A, Yamazaki S. Corros Sci, 2008, Vol. 50: 561-575.[15] Dan T C. PhD Thesis,Institute of Metal Research, Chinese Academy of Sciences, 2010. (但体纯. 中国科学院金属研究所博士论文,2010)[16] Shen Y, Shewmon P G. Metall Trans A, 1991, Vol. 22A, No. 8(1991): 1857-1864.[17] Arioka K, Yamada T, Terachi T, Miyamoto T. Corrosion, 2008, 64(9): 691-706.[18] Lu Z P, Shoji T, Dan T C, Qiu Y B, Yonezawa T. To be published on Corros Sci, 2010.[19] Moshier W C, Brown C M. Corrosion. 2000. 56(3): 307-320.[20] Shoji T, Lu Z P, Das N K, Murakami H, Takeda Y, Ismail T. Proceedings of PVP 2009: 2009 ASME Pressure Vessels and Piping Division Conference,edited by ASME.(2009): 1-20[21] Marchetti L, Perrin S, Raquet O, Pijolat M. Materials Science Forum. 2008. Vols. 595-598: 529-537. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|