| 喷射成形Al-22Si-5Fe合金的热变形行为及组织稳定性 |
| 蔡元华1), 梁瑞光2), 苏占培2), 张济山1) |
1) 北京科技大学新金属材料国家重点实验室, 北京 100083
2) 山东省济宁市任城区农业机械管理局, 济宁 272000 |
|
| HOT DEFORMATION BEHAVIOR AND MICROSTRUCTURAL STABILITY OF SPRAY FORMED Al-22Si-5Fe ALLOY |
| CAI Yuanhua1), LIANG Ruiguang2), SU Zhanpei2), ZHANG Jishan1) |
1) State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083
2) Agricultural Machine Management Bureau of Rencheng District, Jining 272000 |
引用本文:
蔡元华 梁瑞光 苏占培 张济山 . 喷射成形Al-22Si-5Fe合金的热变形行为及组织稳定性[J]. 金属学报, 2010, 46(7): 814-820.
,
,
,
.
HOT DEFORMATION BEHAVIOR AND MICROSTRUCTURAL STABILITY OF SPRAY FORMED Al-22Si-5Fe ALLOY[J]. Acta Metall Sin, 2010, 46(7): 814-820.
| [1] Amano N, Odani Y, Takeda Y, Akechi K. Met Powder Rep, 1989; 44: 186
[2] Hayashi T, Takeda Y, Akechi K, Fujiwara T. Met Powder Rep, 1991; 46: 23
[3] Andrews J B, Seneviratne M V C. AFS Trans, 1984; 92: 209
[4] Hennessey C W, Caley W F, Kipouros G J, Bishop D P. Int J Powder Metall, 2005; 41: 50
[5] Hunt W H. Int J Powder Metall, 2000; 36: 51
[6] Ye H Z. J Mater Eng Perform, 2003; 12: 288
[7] Crepeau P N. AFS Trans, 1995; 103: 361
[8] Dwivedi D K, Sharma A, Rajan T V. Mater Manuf Processes, 2005; 20: 777
[9] Chen C, Liu Z X, Ren B, Wang M X, Weng Y G, Liu Z Y. Trans Nonferrous Met Soc China, 2007; 17: 301
[10] Chang J Y, Moon I, Choi C S. J Mater Sci, 1998; 33: 5015
[11] Huang H J, Cai Y H, Cui H, Huang J F, He J P, Zhang J S. Mater Sci Eng, 2009; A502: 118
[12] Hou L G, Cui H, Cai Y H, Zhang J S. Mater Sci Eng, 2009; A527: 85
[13] Srivastava A K, Srivastava V C, Gloter A, Ojha S N. Acta Mater, 2006; 54: 1741
[14] Shi H F, Yuan X G, Diao X G, Huang H J. Trans Nonferrous Met Soc China, 2007; 17: 710
(时海芳, 袁晓光, 刁晓刚, 黄宏军. 中国有色金属学报, 2007; 17: 710)
[15] Zener C, Hollomon J H. J Appl Phys, 1944; 15: 22
[16] Shi H, McLaren A J, Sellars C M, Shahani R, Bolingbroke R. Mater Sci Technol, 1997; 13: 210
[17] Predel B. In: Madelung O ed., Phase Equilibria, Crystallographic and Thermodynamic Data of Binary Alloys. Berlin: Springer–Verlay, 1994; 5: 1
[18] James F S, Alexander W. Thermodynamic and Kinetic DataMaterials Science and Engineering Handbook. Boca Raton: CRC Press LLC, 2001: 1
[19] Knipling K E, Dunand D C, Seidman D N. Z Metall, 2006; 97: 246 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|