| Fe-C-Mo合金中温转变后期的研究 |
| 徐启昆;王东亚 |
| 重庆大学冶金及材料工程系;重庆大学 |
|
| INVESTIGATION ON LATER STAGE OF INTERMEDIATE TRANSFORMATION IN Fe-C-Mo ALLOYS |
| XU Qikun;WANG Dongya Chongqing University Department of Metallurgy and Materials Engineering;Chongqing University; Sichuan |
引用本文:
徐启昆;王东亚. Fe-C-Mo合金中温转变后期的研究[J]. 金属学报, 1988, 24(4): 242-247.
,
.
INVESTIGATION ON LATER STAGE OF INTERMEDIATE TRANSFORMATION IN Fe-C-Mo ALLOYS[J]. Acta Metall Sin, 1988, 24(4): 242-247.
1 Davenport E S, Bain E C, Kearny N J. Trans AIME. 1930; 90: 1117 2 徐启昆,何幼凡.金属热处理学报,1986;7(2) :91 3 徐启昆.重庆大学学报,1986;(3) :98 4 徐启昆,王东亚.材料科学进展,贝氏体相变专辑,1988;1(3) :41 5 A Letter from Reynolds W T Jr. 1986 6 Christian J W. The Theory of Transformations in Metals and Alloys, Part 1, Pergamon Press, 1981: 542 7 Kennon N F. Metall Trans, 1978; 9A: 57 8 Shiflet G J, Aaronson H I, The Incomplete Transformation (Stesis) Phenomenon in Fe-C-Mo Alloys, An unpublished Research in Carnegie-Mellon University, PA. 1982 9 Berry F G. Davenport A T, Honeycombe R W K. The Mech of Phase Tran sf in Crystalline Solids, London: The Inst of Metals, 1969: 288 10 Berry F G, Honeycombe R W K. Metall Trans, 1970; 1: 3279 11 Xu Qikun (徐启昆), Wang Jun (王俊), Wang Dongya (王东亚). Proc 11th Int Cong on Electron Microscopy, Kyoto: JSEM, 1986: 1267 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|