| 粒状贝氏体组织的疲劳性能 |
| 周鹿宾;张杰;康沫狂 |
| 副教授;西安市西北工业大学材料科学与工程系;西北工业大学;西北工业大学 |
|
| FATIGUE BEHAVIOUR OF GRANULAR BAINITE STRUCTURE |
| ZHOU Lubin;ZHANG Jie;KANG Mokuang Northwest Polytechnic University; Xi'anAssociate Professor; Department of Materials Science and Engineering; Northwest Polytechnic University; Xi' an |
引用本文:
周鹿宾;张杰;康沫狂. 粒状贝氏体组织的疲劳性能[J]. 金属学报, 1988, 24(4): 261-265.
,
,
.
FATIGUE BEHAVIOUR OF GRANULAR BAINITE STRUCTURE[J]. Acta Metall Sin, 1988, 24(4): 261-265.
1 Zhang X L, Hirt M A. Eng Fract Mech, 1983; 18: 965 2 Beerers C J. Met Sci, 1977; 11: 362 3 Orowan E. Proc Roy Soc, 1939; 171: 79 4 Dutta V B, Suresk S, Ritchie R O. Metall Trans, 1984; 15A: 1193 5 Fuchs H O. et al. Metal Fatigue in Engineering. New York: Wiley. 1980 6 Kramer I R. Metall Trans, 1974; 5: 1735 7 Smith R W, Hirschberg M H, Manson S S. NASA TN-D1574, 1963T |
|