| Al-2.2Li-2.5Cu-0.2Mg合金组织与性能的关系 |
| 张匀;赵洪恩;姚大平;高国忠;陈继志;胡壮麒 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| RELATIONSHIP BETWEEN MICROSTRUCTURE AND PROPERTIES IN Al-2.2Li-2.5Cu-0.2Mg ALLOY |
| ZHANG Yun;ZHAO Hong'en;YAO Daping;GAO Guozhong;CHEN Jizhi;HU Zhuangqi Institute of Metal Research; Academia Sinica; Shenyang |
引用本文:
张匀;赵洪恩;姚大平;高国忠;陈继志;胡壮麒. Al-2.2Li-2.5Cu-0.2Mg合金组织与性能的关系[J]. 金属学报, 1989, 25(3): 5-11.
,
,
,
,
,
.
RELATIONSHIP BETWEEN MICROSTRUCTURE AND PROPERTIES IN Al-2.2Li-2.5Cu-0.2Mg ALLOY[J]. Acta Metall Sin, 1989, 25(3): 5-11.
1 宫木美光,日野光雄.金属,1984;54(1) :11 2 Gregson P J, Flower H M. Acta Metall, 1985; 33 (3) : 527 3 Grimes R, Cornish A J, Miller W S, Reynolds M A. Met Mater, 1985: 1: 357 4 Kar R J, Bohlen J W, Chanani G R. In: Starke E A Jr., Sanders T H Jr. eds., Aluminum-Lithium Alloys Ⅱ, TMS-AIME, 1984: 255 5 White J, Miller W S, Palmer I G, Davis R, Saini T S. In: Baker C, Gregson P J, Harris S J, Peel C J eds., Aluminium-Lithium Alloys Ⅲ, London: The Institute of Metals, 1986: 530 6 Starke E A Jr, Sanders T H Jr., Palmer I G. J Met, 1981; 33 (8) : 24 7 Feng W X, Lin F S, Starke E A Jr. In: Starke E A Jr., Sanders T H Jr. eds., Aluminum-Lithium Alloys Ⅱ, TMS-AIME, 1984: 235 8 Bischler P J E, Martin J W. In: Baker C, Gregson P J, Harris S J, Peel C J eds., Aluminium-Lithium Alloys Ⅲ, London: The Institute of Metals, 1986: 539 9 Ahmad M, Ericsson T. In: Baker C, Gregson P J, Harris S J, Peel C J eds., Aluminium-Lithium Alloys Ⅲ, London: The Institute of Metals, 1986: 509 10 Miller W S, White J, Lloyd D J. J Phys (Paris), 1987; 48 (9) : C3--139 11 Damerval C, Raviart J L, Lapasset G. J Phys (Paris), 1987; 48 (9) : C3--661 12 Thomas G, Bell W L, Otte H M. Phys Status Solidi, 1965; 12: 353 13 Tosten M H, Vasudevan A K, Howell P R. Metall Trans, 1988; 19A: 51 14 Rioja R J, Ludwiczak E A. In; Baker C, Gregson P J, Harris S J, Peel C J eds., Aluminium-Lithium Alloys Ⅲ, London: The Institute of Metals, 1986: 471 15 Silcock J M. J Inst Met, 1959--60; 88: 357 16 Mondolfo L F. Aluminum Alloys: Structure and Properties, London: Butterworth, 1976 17 Vasudevan A K, Fricke W G Jr., Malcolm R C, Bucci R J, Przystupa M A, Barlat F. Metall Trans, 1988; 19A: 731 18 Palmer I G, Lewis R E, Crooks D D, Starke E A Jr., Crooks R E. In: Starke E A Jr., Sanders T H Jr. eds., Aluminum-Lithium Alloys Ⅱ. TMS-AIME, 1984: 9 |
|