| 外加电位对奥氏体不锈钢应力腐蚀与腐蚀疲劳交互作用的影响 |
| 冯淘;陈良奭;柯伟 |
| 中国科学院金属腐蚀与防护研究所腐蚀科学开放实验室;中国科学院金属腐蚀与防护研究所;研究员;中国科学院金属腐蚀与防护研究所腐蚀科学开放实验室 |
|
| EFFECT OF POTENTIAL ON INTERACTION BETWEEN STRESS CORROSION CRACKING AND CORROSION FATIGUE OF AUSTENITIC STAINLESS STEEL IN BOILING 42% MgCl_2 SOLUTION |
| FENG Tao;CHEN Liangshi;KE Wei Corrosion Science Laboratory; Academia Sinica; Shenyang |
引用本文:
冯淘;陈良奭;柯伟. 外加电位对奥氏体不锈钢应力腐蚀与腐蚀疲劳交互作用的影响[J]. 金属学报, 1990, 26(6): 94-99.
,
,
.
EFFECT OF POTENTIAL ON INTERACTION BETWEEN STRESS CORROSION CRACKING AND CORROSION FATIGUE OF AUSTENITIC STAINLESS STEEL IN BOILING 42% MgCl_2 SOLUTION[J]. Acta Metall Sin, 1990, 26(6): 94-99.
1 Eremias B, Maricev V A. Werks Korros, 1979; 30: 551 2 Staehle R W. In: Miller K J, Smith R F eds., Mechanical Behaviour of Materials, Vol. 1, Proc the 3rd Int Conf, held in Cambridge, England, 20--24 August 1978, Oxford: Pergamon, 1979: 93 3 Gattgher J P, Wei R P. Proc the Int Conf on Corrosion Fatigue: Chemistry, Mechanics and Microstructure, 14--18 June, 1971, Sponsored by National Assn. of Corrosion Engineers, etc. Houston, NACE, 1972: 409 4 Wei R P. In: Gu Haicheng, He Jiawen eds., Proc of an Int Syposium on Microstructure and Mechanical Behaviour of Materials, held in Xi'an. China, 21--24 October, 1985: 507B |
|