| 裂纹尖端局部形变带的TEM观察 |
| 姚可夫;唐迺泳;陈南平 |
| 清华大学;博士后;清华大学;清华大学 |
|
| TEM OBSERVATION ON LOCAL DEFORMATION BAND AHEAD OF CRACK TIP |
| YAO Kefu University of Science and Technology Beijing; TANG Naiyong; CHEN Nanping Tsinghua University; Beijing |
引用本文:
姚可夫;唐迺泳;陈南平. 裂纹尖端局部形变带的TEM观察[J]. 金属学报, 1991, 27(6): 1-8.
,
,
.
TEM OBSERVATION ON LOCAL DEFORMATION BAND AHEAD OF CRACK TIP[J]. Acta Metall Sin, 1991, 27(6): 1-8.
1 Asaro R J. Adv Appl Mech, 1983; 26: 1 2 Tvergaard V, Needlman A, Lo K K. J Mech Phys Solids, 1981; 29: 115 3 李国琛,力学学报,1988;20:305 4 Embury J D, Korbel A, Raghunathan V S, Rys J. Acta Metall, 1984; 32: 1883 5 姚可夫.清华大学博士学位论文,1989 6 姚可夫,唐迺泳,陈南平.金属学报,1989;25:A213 7 Gardner R N, Wilsdorf H G F. Metall Trans, 1980; 11A: 659 8 Majumdat B S, Butns S J. Acta Metall, 1981; 29: 579 9 Lin I-H, Thomson R. Acta Metall, 1986; 34: 187 10 姚可夫,唐迺泳,陈南平.第五届全国断裂学术会议文集,桂林,1988:1564 11 Ohr S M, Mater Sci Eng, 1985; 72: 1 12 Pichl W, Schoeck G. Ser Metall, 1990; 24: 13 |
|