| Cu基形状记忆合金干滑动磨损研究 |
| 王红卫;吴望子;王凤庭;杨大智 |
| 大连理工大学;博士研究生;沈阳工业学院;大连理工大学;大连理工大学 |
|
| DRY SLIDING WEAR OF Cu-BASED SHAPE MEMORY ALLOY |
| WANG Hongwei Dalian University of Technology; WU Wangzi Shenyang Institute of Industry; WANG Fengting; YANG Dazhi Dalian University of Technology |
引用本文:
王红卫;吴望子;王凤庭;杨大智. Cu基形状记忆合金干滑动磨损研究[J]. 金属学报, 1991, 27(6): 50-55.
,
,
,
.
DRY SLIDING WEAR OF Cu-BASED SHAPE MEMORY ALLOY[J]. Acta Metall Sin, 1991, 27(6): 50-55.
1 金嘉陵,王宏亮.金属学报,1988;24:A66 2 Buckley D H. NASA SP 277, 1971: 194 3 Gerkema J, Miedema A R. Surf Sci, 1983; 124: 351 4 Chen L H, Rigney D A. Wear, 1985; 105: 47 5 Chen L H. Transfer During Sliding Wear of Selected Metal Systems, PhD Dissertation. The Ohio State University, 1984: 198 6 Chen L H, Rigney D A. Wear, 1990; 136: 223 7 Suh N P. Wear, 1977; 44:1 8 Lim S C, Ashby M F. Acta Metall, 1987; 36:1 9 Archard J F. J Appl Phys, 1953; 24: 981 |
|