| 冷加工和热处理对Nb及Nb合金弹性性能的影响 |
| 黄特伟 |
| 冶金工业部钢铁研究总院 |
|
| INFLUENCE OF COLD-WORKING AND HEAT-TREATING ON ELASTIC PROPERTIES OF Nb AND Nb-BASE ALLOYS |
| HUANG Tewei Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing |
引用本文:
黄特伟. 冷加工和热处理对Nb及Nb合金弹性性能的影响[J]. 金属学报, 1992, 28(1): 11-15.
.
INFLUENCE OF COLD-WORKING AND HEAT-TREATING ON ELASTIC PROPERTIES OF Nb AND Nb-BASE ALLOYS[J]. Acta Metall Sin, 1992, 28(1): 11-15.