| Al原子在非晶合金Fe_(78)Si_9B_(13)中的扩散 |
| 姜洪刚;丁炳哲;王景唐 |
| 中国科学院金属研究所;快速凝固与非平衡合金国家重点实验室;中国科学院金属研究所;快速凝固与非平衡合金国家重点实验室;中国科学院金属研究所;快速凝固与非平衡合金国家重点实验室 |
|
| DIFFUSIVITY OF AI IN AMORPHOUS ALLOY Fe_(78)Si_9B_(13) |
| JIANG Honggang;DING Bingzhe;WANG Jingtang Institute of Metal Research; Academia Sinica; Shenyang |
引用本文:
姜洪刚;丁炳哲;王景唐. Al原子在非晶合金Fe_(78)Si_9B_(13)中的扩散[J]. 金属学报, 1992, 28(1): 77-80.
,
,
.
DIFFUSIVITY OF AI IN AMORPHOUS ALLOY Fe_(78)Si_9B_(13)[J]. Acta Metall Sin, 1992, 28(1): 77-80.
| 1 Johnson W L. Mater Sci Eng, 1988; 97: 1--13
2 Schultz, L. Mater Sci Eng, 1988; 97: 15
3 Luborsky F E. J Appl Phys, 1983; 54: 5732
4 Sharma S K, Banerjee S, Kuldeep, Jain A K. J Mater Res, 1989; 4: 603
5 Kijek M, Ahmadzadeh M, Cantor B, Cahn R W. Scr Metall, 1980; 14: 1337
6 De Schepper L, Knuyt G, Stals L M. J Phys Chem Solids, 1983: 44: 171--174
7 Hirvonen J, Raisanen J. J Appl Phys, 1982; 53: 3314
8 Mibe U, Methfessel S. In: Steeb S, Warlimont H eds., Rapidly Quenched Metals, Vol. 5, Proc 5th Int conf on Rapidly Quenched Metals, Germany, September 3-7, 1984, North-Holland, 1985: 775
9 Limoge Y. Acta Metall Mater, 1990; 38: 1733 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|