γ辐照对CuZnAl形状记忆合金影响的研究 |
张桂林;徐峰;刘文宏;俞方华;王景成;邵自昌 |
中国科学院上海原子核研究所;中国科学院上海原子核研究所;中国科学院上海原子核研究所;中国科学院上海原子核研究所;上海钢铁研究所;上海钢铁研究所 |
|
EFFECT OF γ-IRRADIATION ON CuZnAl SHAPE MEMORY ALLOY |
ZHANG Guilin;XU Feng;LIU Wenhong;YU Fanghua;WANG Jingcheng;SHAO Zichang Shanghai Institute of Nuclear Research; Academia Sinica; Shanghai Iron and Steel Research Institute |
引用本文:
张桂林;徐峰;刘文宏;俞方华;王景成;邵自昌. γ辐照对CuZnAl形状记忆合金影响的研究[J]. 金属学报, 1992, 28(3): 42-44.
,
,
,
,
,
.
EFFECT OF γ-IRRADIATION ON CuZnAl SHAPE MEMORY ALLOY[J]. Acta Metall Sin, 1992, 28(3): 42-44.
1 Thomas G, Mori H, Fujita H, Sinclair R. Scr Metall 1982; 16: 589 2 Billington D S, Crawford J H. Radiation Damage in Solids. New Jersey: Princeton, 1961: 26 3 Miura K, Flore N F, Allen C W. J Nucl Mater, 1973/1974; 49: 108 4 Chadderton L T. Radiation Damage in Crystals. New York: John Wiley & Sons, 1965: 16 5 Dzhafaroy T D. Phys Status Solidi, 1989; b 11: 155 6 Bojarski Z, Morawiec H, Panek T J. Phys Status Solidi, 1984; a 83: K9 |
|