| Fe液中Ba-O,Ba-S,Ba-P平衡的研究 |
| 王建生;韩其勇;魏寿昆;宋波 |
| 北京科技大学;北京科技大学理化系;教授;北京(100083);北京科技大学;北京科技大学 |
|
| EQUILIBRIUM OF Ba-O, Ba-S and Ba-P IN MOLTEN Fe |
| WANG Jiansheng;HAN Qiyong;WEI Shoukun;SONG Bo University of Science and Technology Beijing |
引用本文:
王建生;韩其勇;魏寿昆;宋波. Fe液中Ba-O,Ba-S,Ba-P平衡的研究[J]. 金属学报, 1993, 29(2): 64-69.
,
,
,
.
EQUILIBRIUM OF Ba-O, Ba-S and Ba-P IN MOLTEN Fe[J]. Acta Metall Sin, 1993, 29(2): 64-69.
1 严铄,徐思盛,王毓麟.钢铁,1981;16(4) :28 2#12 996501,1983 3#12 981424,1983 4 知水,杨印东,李万象.特殊钢,1984;(增刊):10 5 Hultgren R, Orr R L, Anderson P D, Kelley K K. Selected Values of Thermodynamic Properties of Metals and Alloys. New York: Wiley, 1963: 43 6 Schins H E J, Van Wijk R W M, Dorpema B. Z Metallk, 1971; 62: 330 7 张晓东,韩其勇,陈冬.金属学报,1990;26:B457 8 Turkdogan E T. Physical Chemistry of High Temperature Technology. New York: Academic, 1980: 6 9 Sigworth G K, Elliott J F. Met Sci, 1974; 8: 298 10 Han Qiyong, Zhang Xiaodong, Chen Dong, Wang Pengfei. Metall Trans, 1988; 19B: 617 11 王鹏飞,韩其勇.金属学报,1988;24:B7 12 韩其勇,周德壁.第6届冶金过程物理化学学术会议论文集,1986,重庆,1986:166 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|