| 熔融NaF-AlF_3体系活度的测定 |
| 谢刚;宋宁 |
| 昆明工学院 |
|
| DETERMINATION OF ACTIVITIES IN MELTED NaF-AlF_3 SYSTEM |
| XIE Gang; SONG Ning(Kunming Institute of Technology) |
引用本文:
谢刚;宋宁. 熔融NaF-AlF_3体系活度的测定[J]. 金属学报, 1994, 30(17): 199-203.
,
.
DETERMINATION OF ACTIVITIES IN MELTED NaF-AlF_3 SYSTEM[J]. Acta Metall Sin, 1994, 30(17): 199-203.
| 1GrjotheimK,MalinovskyM,KrohnC,MatiasovskyK,ThonstadJ..邱竹贤,沈时英,郑宏译.铝电解原理,北京:冶金工业出版社,1982:1752FeinleibM,PorterB,JElectrochemSoc,1956;4:2313TingleWH,PetitJ,FrankWB.Aluminum,1981,57:2864DewingEW.MetallTrans,1970;1:16915DewingEW.MetallTrans,1970;1:22116YoshidaK,DewingEW.MetallTrans,1972;3:6837傅崇锐.冶金溶液热力学原理与计算.北京:冶金工业出版社,1979:138 谢刚,沈时英.东北工学院学报,1989;2:1379DewingEW.MetallTrans,1972;3:49510StertenA,HambergK.MaelandI.ActaChemScand,1982;A36:32911BrisleyRJ,FrayDJ.MetallTral1s,1983;14B:435 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|