| 激光合成纳米晶Si粉及粉体性能表征 |
| 李亚利;梁勇;肖克沈;郑丰;胡壮麒 |
| 中国科学院金属研究所快速凝固非平衡合金国家重点实验室 |
|
| LASER SYNTHESIS AND CHARACTERIZATION OF NANO-CRYSTALLINE Si POWDER |
| LI Yali; LIANG Yong; XIAO Keshen; ZHENG Feng; HU Zhuangqi(State Key Lab of RSA ; Institute of Metal Research; Chinese A cademy of Sciences; Shenyang 110015)(Manuscript received 94-02-28) |
引用本文:
李亚利;梁勇;肖克沈;郑丰;胡壮麒. 激光合成纳米晶Si粉及粉体性能表征[J]. 金属学报, 1995, 31(13): 21-25.
,
,
,
,
.
LASER SYNTHESIS AND CHARACTERIZATION OF NANO-CRYSTALLINE Si POWDER[J]. Acta Metall Sin, 1995, 31(13): 21-25.
| 1CannonWR,DanforthSC,HaggertyJS,MarraRA.JAmCeramSoc,1982;65:3242RitterJE,NairSV,GennariPA,DunlayWA,HaggertyJS,GarveyGJ.AdvCeramMater,1988;3:4153LightfootA、KerHL,HaggertyJS.CeramEngSciProc,1990;11(7—8):8424SheldonBW,HaggertyJS.JAmCeramSoc,1991;74:14175FlintJH.HaggertyJS.In:MessingGLed.CeramicTrans,Westerville.OH.1988:2446梁勇,郑丰.佟百运.材料科学进展.1987:2(2):457HaggertyJS.AD,A14439,1984:49< |
|