Ni_3Si体系的螺旋燃烧 |
严新炎;张树格;孙国雄 |
南京东南大学;南京轻工部电光源材料研究所;南京东南大学 |
|
SPIN COMBUSTION IN (3Ni+Si) SYSTEM |
YAN Xinyan(Southeast University; Nanjing 210018) ZHANG Shuge(Research Institute of Electric Light Source Materials; Nanjing; 210015); SUN Guoxiong(Southeast University); Nanjing 210018)(Manuscript received 94-04-04) |
引用本文:
严新炎;张树格;孙国雄. Ni_3Si体系的螺旋燃烧[J]. 金属学报, 1995, 31(13): 15-20.
,
,
.
SPIN COMBUSTION IN (3Ni+Si) SYSTEM[J]. Acta Metall Sin, 1995, 31(13): 15-20.
1MerzhanovAG.In:MunirZA,HoltJBeds.,CombustionandPlasmaSynthesisofHighTemperatureMaterials.NewYork:VCHPublInc,1990:1-532MunirZA,Ansclmi-TamburiniU,MaterSciRep,1989:3:2773BorovinskayaIP.PureApplChem,1992;7:644StruninaAG,DvoryankinAV.DoklAkadNaukSSSR,1981;260(5):1185-11885YiHC,MooreJJ.JMaterSci,1990;25:1159—11686FilonenkoAK,VershennikovVI.FizGoreniyaUzkyva,1975;11(3):353-3627IvlevaTP,MerzhanovAC.ShkadmskiiKG.FizGoreniyaVzryva,1980;16(2):3-108MaksinovYuM.PakAT,LavenchukGB,NaiborodenkoYuS.MerzhanovAG.FizGoreniyaVaryva.,1979;15(4):156-159 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|