| 大晶粒Fe_3Al基合金的超塑性 |
| 单爱党;林栋梁;陈明伟;郦定强 |
| 上海交通大学 |
|
| SUPERPLASTICITY IN Fe_3Al ALLOY WITH LARGE GRAINS |
| SHAN Aidang;LIN Dongliang; CHEN Mingwei; LI Dingqiang(Shanghai Jiaotong Universitty; Shanghai 200030)(Manuscript received. 94-05-12) |
引用本文:
单爱党;林栋梁;陈明伟;郦定强. 大晶粒Fe_3Al基合金的超塑性[J]. 金属学报, 1995, 31(13): 35-39.
,
,
,
.
SUPERPLASTICITY IN Fe_3Al ALLOY WITH LARGE GRAINS[J]. Acta Metall Sin, 1995, 31(13): 35-39.
| 1McKameyCG,DeVanJH,TortorelliPF,SikkaVK.JMaterRes,1991;16:17792LiuCT,LeeEH,McKameyCG.ScrMetall,1989;23:8753LiuCT,McKameyCG,LeeEH,ScrMetallMater,1990;24:3854SikkaVK.ProceedingofStructuralIntermetallicsTMSSymposium.19935StoloffNS.ActaMetall,1964:12:4736MendirattaMG,LipsittHA.MetallTrans,1987;18A:2837DiehmRS,MikkolaD.E,In:LiuCTetal.eds.HighTemperatureOrderedIntermetallicAlloys,Vol.8l,Pittsburgh:MaterialsResearchSociety,1987;3298NiehTG,MayoMJ,KobayashM,WadsworthJ.Superplasiicity,inMetals,CeramicandIntermetallics,Pittsburgh:MaterialsResearchSociety.196:1899OchiaiS,KobayashM,MichimnraK,MayoMJ,KobayashM,WadsworthJ.SuperplasticityinMetals,CeramicandIntermetallics,Pittsburgh,MaterialsResearchSociety,196:20110BackofenWA,TurnerIR.AveryDH.TransASM,1964;57:98011GriffithP,HammondC.ActaMetall,1972;20:93512GhoshAK.AyresRA,MetallTrans,1976;7A:1589d |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|