相变硬化激光热处理的数值解及组织性能的预测 |
朱祖昌;李培耀;俞少罗 |
上海工程技术大学;工程技术大学测试中心 |
|
NUMERICAL SOLUTION AND PREDICTION OF MICROSTRUCTURES AND PROPERTIES FOR PHASE TRANSFORMATION HARDENING WITH LASER TREATMENT |
ZHU Zuchang;LI Peiyao; YU Shaoluo(Shanghai University of Engineering Scicnce;Shanghai 200335)(Manuscript received 1995-04-26; in revised form 1995-09-05) |
引用本文:
朱祖昌;李培耀;俞少罗. 相变硬化激光热处理的数值解及组织性能的预测[J]. 金属学报, 1996, 32(1): 105-112.
,
,
.
NUMERICAL SOLUTION AND PREDICTION OF MICROSTRUCTURES AND PROPERTIES FOR PHASE TRANSFORMATION HARDENING WITH LASER TREATMENT[J]. Acta Metall Sin, 1996, 32(1): 105-112.
1KouS,SunDK,LeYP.MetallTrans,1983;14A:6432AshbyMF,EasterlingKE.ActaMetall,1984,32:19353ShercliffHR,AshbyMF.MetallTrans.1991:22A:24594ClineHE,AnthonyTR.JApplphys,1977;48:38955KouS,LeY.MetallTrans,1983;14A:22456赵海鸥,冯燕武,唐传芳,朱沅浦.金属学报,1987;23:B1907杨洗陈.中国激光,1990;17:2298朱祖昌,方伟,梅或,管彩萍,俞少罗.上海工程技术大学学报,1994;8(4):379朱祖昌,王维荣,俞少罗.中国激光,1994;21(10):84610BrooksCR.HeatTreatmentofFerrousAlloys.NewYork:McGraw-Hill,1979:4411ZhuZuchang,LiXiuqian,YuShaoluo.ChineseJournalofLasers1994;B3(4):36312ZhuZuchang,WangWeixiang,LiXiuqian,YuShaoluo.ChineseJournalofLasers.1994,B3(1):91$ |
|