Please wait a minute...
金属学报  2026, Vol. 62 Issue (7): 1257-1272    DOI: 10.11900/0412.1961.2024.00225
  研究论文 本期目录 | 过刊浏览 |
Mn / N比对22%Cr节Ni型双相不锈钢多道次焊接热影响区组织和力学性能的影响
郭孟雨, 杨银辉(), 高梓豪, 曹建春, 吴诗裕, 陈晓雨
昆明理工大学 材料科学与工程学院 昆明 650093
Effect of Mn / N Ratio on the Microstructure and Mechanical Properties of Multi-Pass Welding HAZ of 22%Cr Low Nickel Type Duplex Stainless Steel
GUO Mengyu, YANG Yinhui(), GAO Zihao, CAO Jianchun, WU Shiyu, CHEN Xiaoyu
School of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093, China
引用本文:

郭孟雨, 杨银辉, 高梓豪, 曹建春, 吴诗裕, 陈晓雨. Mn / N比对22%Cr节Ni型双相不锈钢多道次焊接热影响区组织和力学性能的影响[J]. 金属学报, 2026, 62(7): 1257-1272.
Mengyu GUO, Yinhui YANG, Zihao GAO, Jianchun CAO, Shiyu WU, Xiaoyu CHEN. Effect of Mn / N Ratio on the Microstructure and Mechanical Properties of Multi-Pass Welding HAZ of 22%Cr Low Nickel Type Duplex Stainless Steel[J]. Acta Metall Sin, 2026, 62(7): 1257-1272.

全文: PDF(8858 KB)   HTML
摘要: 

在焊接热循环过程中,Mn / N质量比对节Ni型双相不锈钢(DSS)的转变奥氏体形成、析出相形成和两相(δ和γ相)比例有较大影响,探究其对多道次焊接热影响区(HAZ)组织转变的影响有利于改善HAZ的综合力学性能。本工作基于2205 DSS对比研究了Mn / N比对DSS固溶态和多道次焊接热影响区(HAZ)组织演变和力学性能的影响。结果表明,高的N含量(Mn / N比为3.77)促进HAZ形成了高体积分数(58.7%)的部分转变奥氏体(PTA),其抗拉强度和延伸率分别为836 MPa和39.5%,具有高的强塑性。Mn / N比增至17.80时,HAZ中δ/γ相界上形成胞状Cr2N,魏氏体奥氏体(WA)数量增多导致相界附近铁素体位错墙的形成,使延伸率相对固溶态明显降低。高Mn / N比(65.91) DSS的HAZ中晶界转变奥氏体(GBA)数量先增后减,晶内奥氏体(IGA)和WA数量增多,抑制了Cr2N析出且强塑性降低。与2205 DSS (Mn / N比为3.06)相比,较低Mn / N比DSS焊接HAZ冲击断口以脆性断裂为主。当Mn / N比为3.77时,高N固溶和Cr2N析出对奥氏体相的共同强化增大了DSS中HAZ两相硬度差,且大尺寸(Cr, Mn)O夹杂也一定程度促进了裂纹萌生,使其冲击功降至24.2 J。高Mn / N比则会导致HAZ中形成较多的GBA和WA分割细化铁素体,形成细小IGA而阻碍裂纹扩展,且少量细小σ相的析出提高了铁素体硬度,降低两相硬度差,冲击功增加至134.8 J。

关键词 : 多道次焊接,  焊接热影响区,  Mn / N比,  冲击韧性,  抗拉强度    
Abstract:

Variations in the Mn / N ratio greatly affect the formation of reformed austenite and precipitation and two-phase ratio in duplex stainless steel (DSS) during the welding thermal cycle. Therefore, investigating the influence of the Mn / N ratio on the multipass welding heat-affected zone (HAZ) microstructure is beneficial for enhancing the comprehensive mechanical properties of the HAZ of low-nickel-type DSS thick plates. This study comparatively investigated the effect of Mn / N ratio on the microstructure evolution and mechanical properties of DSS in the solution-treated and multi-pass welded HAZ, with 2205 DSS as a reference. The higher nitrogen content (Mn / N ratio = 3.77) resulted in substantial partial transformed austenite formation with a high volume fraction of 58.7%, yielding a tensile strength of 836 MPa and an elongation of 39.5%, indicating its high strength and plasticity. As the Mn / N ratio increases to 17.80, an increase in the Widmanstätten austenite (WA) amount caused cellular Cr2N formation at the δ/γ phase interfaces and dislocation walls in ferrite for HAZ, considerably decreasing elongation compared to the solid solution state. For DSS with a high Mn / N ratio of 65.91, the grain boundary austenite (GBA) amount initially increased and then decreased, while the intragranular austenite (IGA) and WA amounts increased in HAZ, inhibiting Cr2N precipitation and reducing ductility and strength. Compared with the 2205 DSS (Mn / N ratio = 3.06), the fracture surfaces of DSS with lower Mn / N ratios exhibited brittle fracture. The combined strengthening effect of the high-nitrogen solid solution and Cr2N precipitation on the austenite phase increased the hardness difference between the two phases in the HAZ of the DSS with Mn / N ratio of 3.77. In addition, the formation of some large (Cr, Mn)O inclusions promoted crack initiation to some extent, lowering the impact energy to 24.2 J. High Mn / N ratio led to more GBA and WA segmented ferrite refinement, as well as the formation of small amounts of IGA, which hindered crack propagation. Moreover, the precipitation of a small amount of the σ phase increased the hardness of ferrite, reduced the hardness difference between the two phases, and increased the impact energy to 134.8 J.

Key words: multi-pass welding    welding HAZ    Mn / N ratio    impact toughness    tensile strength
收稿日期: 2024-07-04     
ZTFLH:  TG142  
基金资助:国家自然科学基金项目(51861019)
通讯作者: 杨银辉,yyhyanr@sina.com,主要从事不锈钢材料设计、热变形、焊接性及强韧化等研究
Corresponding author: YANG Yinhui, professor, Tel: 13518726308, E-mail: yyhyanr@sina.com
作者简介: 郭孟雨,女,2000年生,硕士生
Steel No.Mass fraction / %Mn / N ratio
CSiMnSPCrNiMoCuNFe
DSS10.0130.160.520.0090.00622.395.512.640.140.17Bal.3.06 (2205 steel)
DSS20.0040.201.960.0040.00722.061.322.720.110.52Bal.3.77
DSS30.0110.118.010.0090.00722.521.372.690.140.47Bal.17.80
DSS40.0110.1114.510.0060.00522.491.342.700.140.22Bal.65.91
表1  双相不锈钢试样的化学成分及Mn / N比
图1  DSS1~DSS4试样的多道焊接热循环曲线
图2  拉伸试样尺寸
图3  DSS1~DSS4试样固溶态和多道次焊接热影响区(HAZ)显微组织的OM像
图4  DSS1~DSS4试样固溶态与多道次焊接HAZ奥氏体体积分数的变化及各奥氏体相占比
图5  DSS1和DSS2试样经多道次焊接热循环后HAZ组织的STEM像和选区电子衍射(SAED)花样
图6  DSS3试样经多道次焊接热循环后HAZ显微组织的STEM像和SAED花样
图7  DSS4试样经多道次焊接热循环后HAZ的STEM像、SAED花样及EDS分析
图8  DSS1~DSS4试样固溶处理与多道次焊接HAZ的拉伸曲线
图9  DSS1~DSS4试样固溶处理和多道次焊接HAZ的拉伸力学性能
图10  DSS1~DSS4试样多道次焊接HAZ拉伸断口的SEM像
图11  DSS1~DSS4试样固溶处理和多道次焊接HAZ的冲击功及硬度分布
图12  DSS1~DSS4试样多道次焊接HAZ冲击断口的SEM像
图13  DSS1~DSS4试样多道次焊接HAZ冲击断口夹杂物形貌、粒径统计和EDS分析结果
图14  DSS1~DSS4试样多道次焊接HAZ中转变奥氏体演变示意图
图15  DSS1~DSS4试样多道次焊接HAZ的冲击断裂机理演变示意图
[1] Guo L Q, Zhao X M, Li M, et al. Annealing effects on the microstructure and magnetic domain structures of duplex stainless steel studied by in situ technique [J]. Appl. Surf. Sci., 2012, 259: 213
doi: 10.1016/j.apsusc.2012.07.021
[2] Ramkumar K D, Mishra D, Raj B G, et al. Effect of optimal weld parameters in the microstructure and mechanical properties of autogeneous gas tungsten arc weldments of super-duplex stainless steel UNS S32750 [J]. Mater. Des., 2015, 66: 356
doi: 10.1016/j.matdes.2014.10.084
[3] Yang R Z, Zhai R Z, Ren S F, et al. Evolution and healing mechanism of 1Cr22Mn16N high nitrogen austenitic stainless steel interface microstructure during plastic deformation bonding [J]. Acta Metall. Sin., 2024, 60: 915
doi: 10.11900/0412.1961.2023.00015
[3] 杨瑞泽, 翟汝宗, 任少飞 等. 1Cr22Mn16N高氮奥氏体不锈钢塑性变形连接中界面组织演化及愈合机制 [J]. 金属学报, 2024, 60: 915
doi: 10.11900/0412.1961.2023.00015
[4] Luo H, Dong C F, Xiao K, et al. Characterization of passive film on 2205 duplex stainless steel in sodium thiosulphate solution [J]. Appl. Surf. Sci., 2011, 258: 631
doi: 10.1016/j.apsusc.2011.06.077
[5] Su S, Han P, Yang S W, et al. Crystallographic understanding of the effect of Ni content on the hardenability of high-strength low-alloy steel [J]. Acta Metall. Sin., 2024, 60: 789
doi: 10.11900/0412.1961.2022.00297
[5] 苏 帅, 韩 鹏, 杨善武 等. Ni含量对高强度低合金钢淬透性影响的晶体学认识 [J]. 金属学报, 2024, 60: 789
[6] Su Y S, Yang Y H, Cao J C, et al. Research on hot working behavior of low-nickel duplex stainless steel 2101 [J]. Acta Metall. Sin., 2018, 54: 485
[6] 苏煜森, 杨银辉, 曹建春 等. 节Ni型2101双相不锈钢的高温热加工行为研究 [J]. 金属学报, 2018, 54: 485
doi: 10.11900/0412.1961.2017.00151
[7] Garzón C M, Ramirez A J. Growth kinetics of secondary austenite in the welding microstructure of a UNS S32304 duplex stainless steel [J]. Acta Mater., 2006, 54: 3321
doi: 10.1016/j.actamat.2006.03.018
[8] Le J J, Liu L, Liu F, et al. Interdiffusion kinetics of the intermetallic coatings on AZ91D magnesium alloy formed in molten salts at lower temperatures [J]. J. Alloys Compd., 2014, 610: 173
doi: 10.1016/j.jallcom.2014.04.209
[9] Ramirez A J, Lippold J C, Brandi S D. The relationship between chromium nitride and secondary austenite precipitation in duplex stainless steels [J]. Metall. Mater. Trans., 2003, 34A: 1575
[10] Tan H, Wang Z Y, Jiang Y M, et al. Influence of welding thermal cycles on microstructure and pitting corrosion resistance of 2304 duplex stainless steels [J]. Corros. Sci., 2012, 55: 368
doi: 10.1016/j.corsci.2011.10.039
[11] Hertzman S, Brolund B, Ferreira P J. An experimental and theoretical study of heat-affected zone austenite reformation in three duplex stainless steels [J]. Metall. Mater. Trans., 1997, 28A: 277
[12] Wessman S, Selleby M. Evaluation of austenite reformation in duplex stainless steel weld metal using computational thermodynamics [J]. Weld. World, 2014, 58: 217
doi: 10.1007/s40194-013-0104-9
[13] Sun Y T, Wu X Y, Wu X, et al. Influence of multi-pass welding on the microstructure evolution and corrosion resistance of a super duplex stainless steel [J]. Int. J. Electrochem. Sci., 2016, 11: 9666
doi: 10.20964/2016.11.28
[14] Zhang Z Q, Jing H Y, Xu L Y, et al. Investigation on microstructure and impact toughness of different zones in duplex stainless steel welding joint [J]. J. Mater. Eng. Perform., 2017, 26: 134
doi: 10.1007/s11665-016-2441-5
[15] Zhang Z Q, Jing H Y, Xu L Y, et al. Influence of microstructure and elemental partitioning on pitting corrosion resistance of duplex stainless steel welding joints [J]. Appl. Surf. Sci., 2017, 394: 297
doi: 10.1016/j.apsusc.2016.10.047
[16] Ramirez A J, Brandi S D, Lippold J C. Secondary austenite and chromium nitride precipitation in simulated heat affected zones of duplex stainless steels [J]. Sci. Technol. Weld. Join., 2004, 9: 301
doi: 10.1179/136217104225021715
[17] Varbai B, Adonyi Y, Baumer R, et al. Weldability of duplex stainless steels—Thermal cycle and nitrogen effects [J]. Weld J., 2019, 98: 78
[18] Wang Y, Wang Y F, Wang Z H. Enhancing yield strength of high nitrogen austenitic stainless steel [J]. J. Constr. Steel Res., 2021, 187: 106927
doi: 10.1016/j.jcsr.2021.106927
[19] Hosseini V A, Wessman S, Hurtig K, et al. Nitrogen loss and effects on microstructure in multipass TIG welding of a super duplex stainless steel [J]. Mater. Des., 2016, 98: 88
doi: 10.1016/j.matdes.2016.03.011
[20] Han Z C, Wang S G, Hu J H, et al. Effect of welding process parameters on structure and property of 2205 duplex stainless steel weld joint [J]. J. Mater. Eng., 2008, (8): 48
[20] 韩志诚, 王少刚, 胡经洪 等. 焊接工艺对2205双相不锈钢接头组织与性能的影响 [J]. 材料工程, 2008, (8): 48
[21] Yang J, Dong H G, Xia Y Q, et al. Carbide precipitates and mechanical properties of medium Mn steel joint with metal inert gas welding [J]. J. Mater. Sci. Technol., 2021, 75: 48
doi: 10.1016/j.jmst.2020.10.029
[22] Wang H H, Meng L, Luo Q, et al. Superior cryogenic toughness of high-Mn austenitic steel by welding thermal cycles: The role of grain boundary evolution [J]. Mater. Sci. Eng., 2020, A788: 139573
[23] García-García V, Mejía I, Reyes-Calderón F. Experimental and FEM study of Ti-containing TWIP steel weldability [J]. J. Mater. Process. Technol., 2018, 261: 107
doi: 10.1016/j.jmatprotec.2018.05.028
[24] Han K, Yoo J, Lee B, et al. Hot ductility and hot cracking susceptibility of Ti-modified austenitic high Mn steel weld HAZ [J]. Mater. Chem. Phys., 2016, 184: 118
doi: 10.1016/j.matchemphys.2016.09.032
[25] Yoo J, Kim B, Park Y, et al. Microstructural evolution and solidification cracking susceptibility of Fe-18Mn-0.6C-xAl steel welds [J]. J. Mater. Sci., 2015, 50: 279
doi: 10.1007/s10853-014-8586-4
[26] Wang J, Uggowitzer P J, Magdowski R, et al. Nickel-free duplex stainless steels [J]. Scr. Mater., 1998, 40: 123
doi: 10.1016/S1359-6462(98)00396-0
[27] Taiwade R V, Patil A P, Ghugal R D, et al. Effect of welding passes on heat affected zone and tensile properties of AISI 304 stainless steel and chrome-manganese austenitic stainless steel [J]. ISIJ Int., 2013, 53: 102
doi: 10.2355/isijinternational.53.102
[28] Lavenstein S, Gu Y J, Madisetti D, et al. The heterogeneity of persistent slip band nucleation and evolution in metals at the micrometer scale [J]. Science, 2020, 370: eabb2690
doi: 10.1126/science.abb2690
[29] Xie X F, Jiang W C, Liu R M, et al. Evolution of phase ratio and its effect on residual stress for 2205 duplex stainless steel multipass welded joints by thermo-metallurgical-mechanical model [J]. Int. J. Press. Vessels Pip., 2024, 211: 105283
doi: 10.1016/j.ijpvp.2024.105283
[30] Chu J H, Nian Y, Zhang L Q, et al. Formation, evolution and remove behavior of manganese-containing inclusions in medium/high manganese steels [J]. J. Mater. Res. Technol., 2023, 22: 1505
doi: 10.1016/j.jmrt.2022.12.023
[31] Pandey C, Mahapatra M M, Kumar P, et al. Microstructure and mechanical property relationship for different heat treatment and hydrogen level in multi-pass welded P91 steel joint [J]. J. Manuf. Process., 2017, 28: 220
doi: 10.1016/j.jmapro.2017.06.009
[32] Chen T H, Yang J R. Microstructural characterization of simulated heat affected zone in a nitrogen-containing 2205 duplex stainless steel [J]. Mater. Sci. Eng., 2002, A338: 166
[33] Kellai A, Lounis A, Kahla S, et al. Effect of root pass filler metal on microstructure and mechanical properties in the multi-pass welding of duplex stainless steels [J]. Int. J. Adv. Manuf. Technol., 2018, 95: 3215
doi: 10.1007/s00170-017-1412-9
[34] Eghlimi A, Shamanian M, Raeissi K. Effect of current type on microstructure and corrosion resistance of super duplex stainless steel claddings produced by the gas tungsten arc welding process [J]. Surf. Coat. Technol., 2014, 244: 45
doi: 10.1016/j.surfcoat.2014.01.047
[35] Haghdadi N, Breen A J, Chen H, et al. New insights into the character of austenite-ferrite boundaries in an additively manufactured duplex stainless steel [J]. Scr. Mater., 2024, 245: 116049
doi: 10.1016/j.scriptamat.2024.116049
[36] Jang Y H, Kim S S, Lee J H. Effect of different Mn contents on tensile and corrosion behavior of CD4MCU cast duplex stainless steels [J]. Mater. Sci. Eng., 2005, A369: 302
[37] Ferreira V H M M, Coury F G, De Araujo Santana D, et al. Novel high nitrogen austenitic stainless steels: From high-throughput screening to experimental validation and properties relationship [J]. J. Mater. Res. Technol., 2024, 30: 640
doi: 10.1016/j.jmrt.2024.03.090
[38] Yang Y H, Pan X Y. Effect of Mn / N ratio on microstructure and mechanical behavior of simulated welding heat affected zone in 22% Cr lean duplex stainless steel [J]. Mater. Sci. Eng., 2022, A835: 142676
[39] Krawczynska A T, Brynk T, Gierlotka S, et al. Mechanical properties of nanostructured 316LVM stainless steel annealed under pressure [J]. Mech. Mater., 2013, 767: 25
[40] Kartik B, Veerababu R, Sundararaman M, et al. Satyanarayana. Effect of high temperature ageing on microstructure and mechanical properties of a nickel-free high nitrogen austenitic stainless steel [J]. Mater. Sci. Eng., 2015, A642: 288
[41] Lee T H, Kim S J, Takaki S. Time-temperature-precipitation characteristics of high-nitrogen austenitic Fe-18Cr-18Mn-2Mo-0.9N steel [J]. Metall. Mater. Trans., 2006, 37A: 3445
[42] Zhou J Q, Han X P. Effects of ultrafine grains on fracture toughness of nanocrystalline materials [J]. J. Eng. Mech., 2014, 31: 229
[42] 周剑秋, 韩雪平. 超细晶粒对纳晶材料断裂韧性的影响 [J]. 工程力学, 2014, 31: 229
[43] Zhang W Y, Jiang W C, Li H J, et al. Effect of tensile overload on fatigue crack behavior of 2205 duplex stainless steel: Experiment and finite element simulation [J]. Int. J. Fatigue., 2019, 128: 105199
doi: 10.1016/j.ijfatigue.2019.105199
[44] Cui C, Weng Z J, Gu K X, et al. The strengthening role of post-welded cryogenic treatment on the performance and microstructure of 304 austenitic stainless steel weldments [J]. J. Mater. Res. Technol., 2024, 29: 5576
doi: 10.1016/j.jmrt.2024.02.220
[45] Mohammed R, Reddy G, Rao K. Microstructure and pitting corrosion of shielded metal arc welded high nitrogen stainless steel [J]. Def. Technol., 2015, 11: 237
doi: 10.1016/j.dt.2015.04.002
[46] Whitcroft C S, Martin J W. The influence of chromium content on the precipitation of γ' (ordered NI3Ti) in some austenitic steels [J]. Mater. Charact., 1997, 39: 91
doi: 10.1016/S1044-5803(97)00127-7
[47] Chen J H, Cao R. Micromechanism of cleavage fracture of weld metals [J]. Acta Metall. Sin., 2017, 53: 1427
doi: 10.11900/0412.1961.2017.00145
[47] 陈剑虹, 曹 睿. 焊缝金属解理断裂微观机理 [J]. 金属学报, 2017, 53: 1427
doi: 10.11900/0412.1961.2017.00145
[48] Zhang Z Q, Jing H Y, Xu L Y, et al. Investigation on microstructure evolution and properties of duplex stainless steel joint multi-pass welded by using different methods [J]. Mater. Des., 2016, 109: 670
doi: 10.1016/j.matdes.2016.07.110
[1] 江慧敏, 魏梦洁, 胡小强, 蔡欣, 李殿中, 党恩. 回火温度对超深井承压件F22M钢微观组织与力学性能的影响[J]. 金属学报, 2026, 62(4): 587-598.
[2] 宋逸思, 廖瑜, 李传维, 陈益华, 顾剑锋. 逆转变奥氏体对0Cr16Ni5Mo1超级马氏体不锈钢低温冲击韧性的影响[J]. 金属学报, 2025, 61(5): 687-698.
[3] 王冲, 王磊, 段然, 田强, 黄烁, 赵光普. 固溶后处理对GH4706合金时效析出相演化及力学性能的影响[J]. 金属学报, 2025, 61(11): 1638-1652.
[4] 朱东明, 何江里, 史根豪, 王青峰. 热输入对Q500qE钢模拟CGHAZ微观组织和冲击韧性的影响[J]. 金属学报, 2022, 58(12): 1581-1588.
[5] 蒋中华, 杜军毅, 王培, 郑建能, 李殿中, 李依依. M-A岛高温回火转变产物对核电SA508-3钢冲击韧性影响机制[J]. 金属学报, 2021, 57(7): 891-902.
[6] 张林, 郭晓, 高建文, 邓安元, 王恩刚. 电磁搅拌对TiB2颗粒增强钢组织和力学性能的影响[J]. 金属学报, 2020, 56(9): 1239-1246.
[7] 冯汉臣,闵学刚,魏大圣,周立初,崔世云,方峰. 低温回火对超大形变冷拔珠光体钢丝显微组织和力学性能的影响[J]. 金属学报, 2019, 55(5): 585-592.
[8] 马宏驰, 杜翠薇, 刘智勇, 李永, 李晓刚. E690高强低合金钢焊接热影响区典型组织在含SO2海洋环境中的应力腐蚀行为对比研究[J]. 金属学报, 2019, 55(4): 469-479.
[9] 万响亮, 胡锋, 成林, 黄刚, 张国宏, 吴开明. 两步贝氏体转变对中碳微纳结构钢韧性的影响[J]. 金属学报, 2019, 55(12): 1503-1511.
[10] 邵毅, 李彦默, 刘晨曦, 严泽生, 刘永长. 低碳铁素体不锈钢高频直缝电阻焊管退火工艺优化[J]. 金属学报, 2019, 55(11): 1367-1378.
[11] 季培蓓, 周立初, 周雪峰, 方峰, 蒋建清. 冷拉拔珠光体钢丝的力学性能各向异性研究[J]. 金属学报, 2018, 54(4): 494-500.
[12] 文明月, 董文超, 庞辉勇, 陆善平. 一种Fe-Cr-Ni-Mo高强钢焊接热影响区的显微组织与冲击韧性研究[J]. 金属学报, 2018, 54(4): 501-511.
[13] 杜瑜宾, 胡小锋, 姜海昌, 闫德胜, 戎利建. 回火时间对Fe-Cr-Ni-Mo高强钢碳化物演变及力学性能的影响[J]. 金属学报, 2018, 54(1): 11-20.
[14] 舒志强,袁鹏斌,欧阳志英,龚丹梅,白雪明. 回火温度对26CrMo钻杆钢显微组织和力学性能的影响[J]. 金属学报, 2017, 53(6): 669-676.
[15] 刘奋军, 傅莉, 陈海燕. 铝合金薄板高转速搅拌摩擦焊接头组织与力学性能[J]. 金属学报, 2017, 53(12): 1651-1658.